Creep resistance of tin-based lead-free solder alloys

被引:0
|
作者
M. L. Huang
C. M. L. Wu
L. Wang
机构
[1] Dalian University of Technology,Department of Materials Science and Engineering
[2] City University of Hong Kong,Department of Physics and Materials Science
来源
关键词
Lead (Pb)-free solder; microstructure; creep; precipitation;
D O I
暂无
中图分类号
学科分类号
摘要
This paper reports on the microstructure-creep property relationship of three precipitation-strengthened tin (Sn)-based lead (Pb)-free solder alloys (Sn-0.7Cu, Sn-3.5Ag, and Sn-3.8Ag-0.7Cu) in bulk samples, together with Sn-37Pb as the alloy for comparison at temperatures of 303 K, 348 K, and 393 K. The creep resistance of these three Sn-based Pb-free solders increases, i.e., the steady-state creep rates decrease, with increasing volume fraction of precipitate phases for the Pb-free solder alloys. Their apparent stress exponents (na ∼ 7.3-17), which are all higher than that of pure Sn, attain higher values with increasing volume fraction of precipitate phases at constant temperature, and with decreasing temperature for the same solder alloy.
引用
下载
收藏
页码:1373 / 1377
页数:4
相关论文
共 50 条
  • [1] Creep resistance of tin-based lead-free solder alloys
    Huang, ML
    Wu, CML
    Wang, L
    JOURNAL OF ELECTRONIC MATERIALS, 2005, 34 (11) : 1373 - 1377
  • [2] A comparative study of room-temperature creep in lead-free tin-based solder alloys
    Mahmudi, R.
    Geranmayeh, A. R.
    INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2010, 101 (02) : 271 - 278
  • [3] Thermal analysis of selected tin-based lead-free solder alloys
    Palcut, M.
    Sopousek, J.
    Trnkova, L.
    Hodulova, E.
    Szewczykova, B.
    Ozvold, M.
    Turna, M.
    Janovec, J.
    KOVOVE MATERIALY-METALLIC MATERIALS, 2009, 47 (01): : 43 - 50
  • [4] Effect of Strain Rate and Temperature on the Tensile Properties of Tin-Based Lead-Free Solder Alloys
    Ning Bai
    Xu Chen
    Zhou Fang
    Journal of Electronic Materials, 2008, 37 : 1012 - 1019
  • [5] Effect of strain rate and temperature on the tensile properties of tin-based lead-free solder alloys
    Bai, Ning
    Chen, Xu
    Fang, Zhou
    JOURNAL OF ELECTRONIC MATERIALS, 2008, 37 (07) : 1012 - 1019
  • [6] Creep deformation characteristics of tin and tin-based electronic solder alloys
    M. D. Mathew
    H. Yang
    S. Movva
    K. L. Murty
    Metallurgical and Materials Transactions A, 2005, 36 : 99 - 105
  • [7] Creep deformation characteristics of tin and tin-based electronic solder alloys
    Mathew, MD
    Yang, H
    Movva, S
    Murty, KL
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2005, 36A (01): : 99 - 105
  • [8] COMPARISON OF CREEP LIFE ASSESSMENT BETWEEN TIN-BASED LEAD-FREE SOLDERS AND LEAD SOLDERS
    Monden, Kenji
    CHARACTERIZATION OF MINERALS, METALS, AND MATERIALS, 2012, : 479 - 486
  • [9] Investigation of Electrochemical Migration of Tin and Tin-Based Lead-Free Solder Alloys under Chloride-Containing Thin Electrolyte Layers
    Jiang, Shuyi
    Liao, Bokai
    Chen, Zhenyu
    Guo, Xingpeng
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2018, 13 (10): : 9942 - 9949
  • [10] Creep properties of Sn-Sb based lead-free solder alloys
    El-Daly, A. A.
    Swilem, Y.
    Hammad, A. E.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 471 (1-2) : 98 - 104