Elevated Temperature Creep and Tensile Performance of Extruded Mg-10Ce Alloy

被引:0
|
作者
Jordan Kozakevich
Joshua Stroh
Dimitry Sediako
David Weiss
Adam Loukus
Sven C. Vogel
机构
[1] University of British Columbia,High Performance Powertrain Materials Laboratory, School of Engineering
[2] Eck Industries,Material Science & Technology Division
[3] Loukus Technologies Inc.,undefined
[4] Los Alamos National Laboratory,undefined
关键词
automotive and transportation; creep and stress rupture; mechanical testing; rare earths;
D O I
暂无
中图分类号
学科分类号
摘要
Fitness-for-service testing on an extruded magnesium (Mg) alloy containing 10 wt.% cerium (Ce) has been conducted to understand how increased level of Ce affects the elevated temperature properties of Mg. Optical and scanning electron microscopy revealed a 39.4% area percentage of the Mg12Ce phase. The Mg12Ce intermetallic was formulated along the grain boundaries in semi-circular, asymmetrical and polyhedral morphologies. The Mg alloy was subjected to a room temperature (RT) and 200 °C tensile test and a 200 °C staircase creep test. At RT, the Mg-10Ce alloy exhibited an ultimate tensile strength (UTS), total elongation and toughness of 271 MPa, 0.95% and 1.6 MJ/m3, respectively. At 200 °C, the alloy exhibited a UTS, 0.2% yield strength, total elongation and toughness of 111 MPa, 103 MPa, 43 % and 39.8 MJ/m3, respectively. The alloy exhibits an increase in RT strength and 200°C toughness compared to conventional Mg alloys (i.e., AE44, WE43 etc.). The staircase creep experiment revealed steady-state creep rates of 1.88 x 10− 8, 3.40 × 10− 7  and 2.00 x 10− 6  s− 1 for applied loads of 22, 40 and 55 MPa, respectively. The stress exponent (4.88) calculated between 20 and 40 MPa indicated that power-law dislocation climb and activated cross-slip of the pyramidal planes (101¯1\documentclass[12pt]{minimal} \usepackage{amsmath} \usepackage{wasysym} \usepackage{amsfonts} \usepackage{amssymb} \usepackage{amsbsy} \usepackage{mathrsfs} \usepackage{upgreek} \setlength{\oddsidemargin}{-69pt} \begin{document}$$10\overline{1}1$$\end{document}) are the two dominant creep mechanisms, which are typical for high temperature and low-stress applications. The stress exponent (5.57) calculated between 40 and 55 MPa indicated that power-law breakdown dislocation climb and activated cross-slip of the basal planes (0002) were the two dominant creep mechanisms. A stress exponent value above 5 indicated that the alloy was moved into the transitional phase of creep between high-temperature/low-load creep and high-temperature/high-load creep. The alloy’s strong basal (0002) texture and high volume fraction Mg12Ce intermetallic contributed to its poor creep performance.
引用
收藏
页码:2758 / 2765
页数:7
相关论文
共 50 条
  • [1] Elevated Temperature Creep and Tensile Performance of Extruded Mg-10Ce Alloy
    Kozakevich, Jordan
    Stroh, Joshua
    Sediako, Dimitry
    Weiss, David
    Loukus, Adam
    Vogel, Sven C.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2023, 32 (06) : 2758 - 2765
  • [2] ELEVATED-TEMPERATURE TENSILE BEHAVIOR OF A RAPIDLY SOLIDIFIED AND REVERSE EXTRUDED Mg-Zn-Y-Ce-Zr ALLOY
    Carter, Jon T.
    Krajewski, Paul E.
    Shechtman, Daniel
    MAGNESIUM TECHNOLOGY 2010, 2010, : 227 - +
  • [3] Effect of heat treatment on elevated temperature tensile and creep properties of the extruded Mg-6Gd-4Y-Nd-0.7Zr alloy
    Yuan, Lin
    Shi, Wenchao
    Jiang, WenMao
    Zhao, Zhe
    Shan, Debin
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 658 : 339 - 347
  • [4] Elevated temperature tensile properties of an extruded aluminium alloy reinforced with SiCp
    Özdemir, A.
    Önel, K.
    International Journal of Materials Research, 2022, 97 (01) : 94 - 100
  • [5] Elevated temperature tensile properties of an extruded aluminium alloy reinforced with SiCp
    Özdemir, I
    Önel, K
    ZEITSCHRIFT FUR METALLKUNDE, 2006, 97 (01): : 94 - 100
  • [6] Elevated temperature tensile and creep rupture properties of INCONEL alloy 725
    Hibner, EL
    Sizek, HW
    Mannan, SK
    SUPERALLOYS 718, 625, 706 AND VARIOUS DERIVATIVES, 1996, : 491 - 501
  • [7] Tensile and compressive creep behavior of extruded Mg-10Gd-3Y-0.5Zr (wt.%) alloy
    Wang, H.
    Wang, Q. D.
    Boehlert, C. J.
    Yin, D. D.
    Yuan, J.
    MATERIALS CHARACTERIZATION, 2015, 99 : 25 - 37
  • [8] Tensile creep behavior and microstructure evolution of extruded Mg-10Gd-3Y-0.5Zr (wt%) alloy
    Wang, Huan
    Wang, Qudong
    Yin, Dongdi
    Yuan, Jie
    Ye, Bing
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 578 : 150 - 159
  • [9] Tensile creep anisotropy of a Mg-2Y alloy extruded sheet with a splitted texture
    Xiao, Zhenyu
    Huo, Qinghuan
    Zhang, Yuxiu
    Zhang, Zhirou
    Li, Zehao
    Hashimoto, Aki
    Yang, Xuyue
    JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 823
  • [10] High temperature tensile behaviors of extruded and rolled AZ31 Mg alloy
    Qiao J.
    Wang Y.
    Shi G.-D.
    Transactions of Nonferrous Metals Society of China (English Edition), 2010, 20 (SUPPL. 2): : s540 - s544