Fabrication and characterization of boron-doped nanocrystalline diamond-coated MEMS probes

被引:0
|
作者
Robert Bogdanowicz
Michał Sobaszek
Mateusz Ficek
Daniel Kopiec
Magdalena Moczała
Karolina Orłowska
Mirosław Sawczak
Teodor Gotszalk
机构
[1] Gdańsk University of Technology,Department of Metrology and Optoelectronics, Faculty of Electronics, Telecommunications and Informatics
[2] Wrocław University of Technology,Faculty of Microsystem Electronics and Photonics
[3] Polish Academy of Sciences,undefined
[4] The Szewalski Institute of Fluid-Flow Machinery,undefined
来源
Applied Physics A | 2016年 / 122卷
关键词
Diamond Film; Contact Potential Difference; Chemical Vapour Deposition Diamond; Boron Doping; Nanocrystalline Diamond;
D O I
暂无
中图分类号
学科分类号
摘要
Fabrication processes of thin boron-doped nanocrystalline diamond (B-NCD) films on silicon-based micro- and nano-electromechanical structures have been investigated. B-NCD films were deposited using microwave plasma assisted chemical vapour deposition method. The variation in B-NCD morphology, structure and optical parameters was particularly investigated. The use of truncated cone-shaped substrate holder enabled to grow thin fully encapsulated nanocrystalline diamond film with a thickness of approx. 60 nm and RMS roughness of 17 nm. Raman spectra present the typical boron-doped nanocrystalline diamond line recorded at 1148 cm−1. Moreover, the change in mechanical parameters of silicon cantilevers over-coated with boron-doped diamond films was investigated with laser vibrometer. The increase of resonance to frequency of over-coated cantilever is attributed to the change in spring constant caused by B-NCD coating. Topography and electrical parameters of boron-doped diamond films were investigated by tapping mode AFM and electrical mode of AFM–Kelvin probe force microscopy (KPFM). The crystallite–grain size was recorded at 153 and 238 nm for boron-doped film and undoped, respectively. Based on the contact potential difference data from the KPFM measurements, the work function of diamond layers was estimated. For the undoped diamond films, average CPD of 650 mV and for boron-doped layer 155 mV were achieved. Based on CPD values, the values of work functions were calculated as 4.65 and 5.15 eV for doped and undoped diamond film, respectively. Boron doping increases the carrier density and the conductivity of the material and, consequently, the Fermi level.
引用
收藏
相关论文
共 50 条
  • [1] Fabrication and characterization of boron-doped nanocrystalline diamond-coated MEMS probes
    Bogdanowicz, Robert
    Sobaszek, Michal
    Ficek, Mateusz
    Kopiec, Daniel
    Moczala, Magdalena
    Orlowska, Karolina
    Sawczak, Miroslaw
    Gotszalk, Teodor
    APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING, 2016, 122 (04):
  • [2] Processing of nanoscale gaps for boron-doped nanocrystalline diamond based MEMS
    Iankov, Dimitre
    Zuerbig, Verena
    Pletschen, Wilfried
    Giese, Christian
    Iannucci, Robert
    Ambacher, Oliver
    Lebedev, Vadim
    28TH EUROPEAN CONFERENCE ON SOLID-STATE TRANSDUCERS (EUROSENSORS 2014), 2014, 87 : 903 - 906
  • [3] Quantum transport in boron-doped nanocrystalline diamond
    Mares, Jiri J.
    Hubik, Pavel
    Kristofik, Jozef
    Kindl, Dobroslav
    Nesladek, Milos
    CHEMICAL VAPOR DEPOSITION, 2008, 14 (7-8) : 161 - 172
  • [4] Superior Field Emissions from Boron-Doped Nanocrystalline Diamond Compared to Boron-Doped Microcrystalline Diamond
    Le Shim, Ee
    Lee, Min Ho
    Lu, Ming-Yen
    Kang, Chi Jung
    Lee, Kyu-Wang
    Choi, Young Jin
    JOURNAL OF NANOSCIENCE AND NANOTECHNOLOGY, 2012, 12 (12) : 8904 - 8907
  • [5] Boron-doped homoepitaxial diamond layers: Fabrication, characterization, and electronic applications
    Borst, TH
    Weis, O
    PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 1996, 154 (01): : 423 - 444
  • [6] Boron-doped homoepitaxial diamond layers: fabrication, characterization, and electronic applications
    Borst, T.H.
    Weis, O.
    Physica Status Solidi (A) Applied Research, 1996, 154 (01): : 423 - 444
  • [7] Fabrication and electrochemical characterization of boron-doped diamond microdisc array electrodes
    Tsunozaki, K
    Einaga, Y
    Rao, TN
    Fujishima, A
    CHEMISTRY LETTERS, 2002, (05) : 502 - 503
  • [8] Fabrication of boron-doped CVD diamond microelectrodes
    Cooper, JB
    Pang, S
    Albin, S
    Zheng, JL
    Johnson, RM
    ANALYTICAL CHEMISTRY, 1998, 70 (03) : 464 - 467
  • [9] CHARACTERIZATION OF BORON-DOPED DIAMOND FILM
    OKANO, K
    NARUKI, H
    AKIBA, Y
    KUROSU, T
    IIDA, M
    HIROSE, Y
    NAKAMURA, T
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 1989, 28 (06): : 1066 - 1071
  • [10] Electrochemical characterization of doped diamond-coated carbon fibers at different boron concentrations.
    Almeida, EC
    Diniz, AV
    Trava-Airoldi, VJ
    Ferreira, NG
    THIN SOLID FILMS, 2005, 485 (1-2) : 241 - 246