Effect of hydrogen on true leakage current characteristics of (Pb,La)(Zr,Ti)O3 thin-film capacitors with Pt- or Ir-based top electrodes

被引:0
|
作者
Soon-Gil Yoon
Dwi Wicaksana
Dong-Joo Kim
Seung-Hyun Kim
A. I. Kingon
机构
[1] North Carolina State University,Department of Materials Science and Engineering
[2] Chungnam National University,Department of Materials Engineering
[3] North Carolina State University,Department of Materials Science and Engineering
[4] Inostek Inc.,undefined
来源
关键词
D O I
暂无
中图分类号
学科分类号
摘要
The degradation behavior of polarization and leakage current characteristics of sol-gel-derived (Pb,La)(Zr,Ti)O3 (PLZT) thin films, with Pt, Ir, and IrO2 top electrodes, by annealing under a 4% H2/96% N2 atmosphere were investigated. The leakage current behaviors of Pt/PLZT/Pt and IrO2/PLZT/Pt capacitors annealed at 300 °C for 20 min in 4% H2 were well consistent with the space-charge-influenced injection model proposed. However, IrO2/PLZT/Pt capacitors recovered at 700 °C for 10 min in Ar ambient after hydrogen anneal were not consistent with the proposed model because a conducting phase of IrPb was formed between the top electrode and PLZT during the recovery anneal at 700 °C in Ar ambient and modified the Schottky barrier height. The true leakage current behavior of IrO2/PLZT/Pt capacitors recovered after hydrogen forming are similar to those of Ir/PLZT/Pt capacitors without the hydrogen-forming gas anneal. The P–E loops of Pt/PLZT/Pt and Ir/PLZT/Pt capacitors showed good recovery through recovery anneal after H2 treatment. However, IrO2/PLZT/Pt capacitors depended on the recovery anneal atmosphere (Ar or O2).
引用
收藏
页码:1185 / 1189
页数:4
相关论文
共 50 条
  • [1] Effect of hydrogen on true leakage current characteristics of (Pb,La)(Zr,Ti)O3 thin-film capacitors with Pt- or Ir-based top electrodes
    Yoon, SG
    Wicaksana, D
    Kim, DJ
    Kim, SH
    Kingon, AI
    JOURNAL OF MATERIALS RESEARCH, 2001, 16 (04) : 1185 - 1189
  • [2] Effect of hydrogen on (Pb,La)(Zr,Ti)O3 (PLZT) thin film capacitors with Pt or Ir-based top electrodes
    Yoon, SG
    Wicaksana, D
    Kim, DJ
    Kim, SH
    Kingon, AI
    PROCEEDINGS OF THE 2001 12TH IEEE INTERNATIONAL SYMPOSIUM ON APPLICATIONS OF FERROELECTRICS, VOLS I AND II, 2001, : 949 - 952
  • [3] Electrical properties of Pb(Zr, Ti)O3 thin film capacitors on Pt and Ir electrodes
    Nakamura, Takashi
    Nakao, Yuichi
    Kamisawa, Akira
    Takasu, Hidemi
    Japanese Journal of Applied Physics, Part 1: Regular Papers & Short Notes & Review Papers, 1995, 34 (9 B): : 5184 - 5187
  • [4] ELECTRICAL-PROPERTIES OF PB(ZR,TI)O-3 THIN-FILM CAPACITORS ON PT AND IR ELECTRODES
    NAKAMURA, T
    NAKAO, Y
    KAMISAWA, A
    TAKASU, H
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 1995, 34 (9B): : 5184 - 5187
  • [5] Asymmetry in the voltage shift in Pt/Pb(Zr,Ti)O3/Pt thin-film capacitors
    Lee, EG
    Kim, KS
    Lee, JK
    Jang, WY
    Lee, JG
    Kim, SJ
    JOURNAL OF THE KOREAN PHYSICAL SOCIETY, 2003, 42 (01) : 158 - 161
  • [6] Deformation in the hysteresis loop of Pt/Pb(Zr,Ti)O3/Pt thin-film capacitors
    Lee, EG
    Lee, JK
    Lee, JG
    Kim, JY
    Jang, HM
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1999, 18 (13) : 1033 - 1035
  • [7] Imprint characteristics of Pt/Pb(Zr,Ti)O3/Ir capacitors
    Kang-Woon Lee
    Won-Jong Lee
    Metals and Materials International, 2006, 12 : 85 - 93
  • [8] Recovery characteristics of hydrogen-damaged (Pb,La)(Zr,Ti)O3 capacitors with Pt and IrO2 top electrodes
    Yoon, SG
    Kingon, AI
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2001, 148 (07) : F137 - F139
  • [9] Stresses in Pt/Pb(Zr,Ti)O3/Pt thin-film stacks for integrated ferroelectric capacitors
    Spierings, G.A.C.M.
    Dormans, G.J.M.
    Moors, W.G.J.
    Ulenaers, M.J.E.
    Larsen, P.K.
    Journal of Applied Physics, 1995, 78 (03):
  • [10] The performance of Zr as barrier layer for Pt bottom electrodes in Pb(Zr,Ti)O3 thin film capacitors
    Mardare, CC
    Joanni, E
    Mardare, AI
    de Sá, CPM
    Tavares, PB
    THIN SOLID FILMS, 2005, 483 (1-2) : 21 - 26