Sintering Behavior of Elemental Powders with FeB Addition in the Composition of Martensitic Stainless steel

被引:0
|
作者
Farid Akhtar
机构
[1] University of Science and Technology Beijing,Institute of Powder Metallurgy
[2] University of Engineering and Technology,Department of Metallurgical and Materials Engineering
关键词
FeB, 465 martensitic stainless steel, sintering, ultimate tensile strength (UTS);
D O I
暂无
中图分类号
学科分类号
摘要
The effect of sintering additive for the development of high-strength martensitic stainless steel from elemental powders was studied. The sintering parameters investigated were: sintering temperature, sintering time, and wt.% of FeB. In vacuum sintering, effective sintering took place between 1300 and 1350 °C with 1-1.5 wt.% FeB addition. The maximum sintered density and ultimate tensile strength (UTS) were achieved after sintering at 1350°C for 60 min with 1 wt.% FeB. Secondary pores were observed in samples containing more than 1.5 wt.% FeB sintered at 1350 °C for 60 min. More than 1.5 wt.% FeB content and temperature above 1350°C caused slumping of the specimens. Maximum UTS of 505 MPa was achieved with 1 wt.% FeB content. Above 0.5 wt.% FeB content, maximum increase in density was observed. Fracture morphologies of the sintered samples are reported.
引用
收藏
页码:726 / 729