Influence of Extrusion on the Microstructure and Mechanical Behavior of Mg-9Li-3Al-xSr Alloys

被引:0
|
作者
Yan Yang
Xiaodong Peng
Haiming Wen
Baolong Zheng
Yizhang Zhou
Weidong Xie
Enrique J. Lavernia
机构
[1] Chongqing University,College of Materials Science and Engineering
[2] University of California,Department of Chemical Engineering and Materials Science
关键词
Dislocation Density; Dynamic Recrystallization; Extrusion Direction; Extrusion Ratio; Extrude Alloy;
D O I
暂无
中图分类号
学科分类号
摘要
Mg-9Li-3Al-xSr (LA93-xSr, x = 0, 1.5, 2.5, and 3.5 wt pct) alloys were cast and extruded at 533 K (260 °C) with an extrusion ratio of 28. The microstructure and mechanical response are reported and discussed paying particular attention to the influence of extrusion and Sr content on phase composition, strength, and ductility. The results of the current study show that LA93-xSr alloys contain both α-Mg (hcp) and β-Li (bcc) matrix phases. Moreover, the addition of Sr refines the grain size in the as-cast alloys and leads to the formation of the intermetallic compound (Al4Sr). Our results show significant grain refinement during extrusion and almost no influence of Sr content on the grain size of the extruded alloys. The microstructure evolution during extrusion is governed by continuous dynamic recrystallization (CDRX) in the α-Mg phase, whereas discontinuous dynamic recrystallization (DDRX) occurs in the β-Li phase. The mechanical behavior of the extruded LA93-xSr alloy is discussed in terms of grain refinement and dislocation strengthening. The tensile strength of the extruded alloys first increases and then decreases, whereas the elongation decreases monotonically with increasing Sr; in contrast, hardness increases for all Sr compositions studied herein. Specifically, when Sr content is 2.5 wt pct, the extruded Mg-9Li-3Al-2.5Sr (LAJ932) alloy exhibits a favorable combination of strength and ductility with an ultimate tensile strength of 235 MPa, yield strength of 221 MPa, and an elongation of 19.4 pct.
引用
收藏
页码:1101 / 1113
页数:12
相关论文
共 50 条
  • [1] Influence of Extrusion on the Microstructure and Mechanical Behavior of Mg-9Li-3Al-xSr Alloys
    Yang, Yan
    Peng, Xiaodong
    Wen, Haiming
    Zheng, Baolong
    Zhou, Yizhang
    Xie, Weidong
    Lavernia, Enrique J.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2013, 44A (02): : 1101 - 1113
  • [2] Microstructure and solidification behavior of permanent-mould-cast Mg-9Li-3Al-xSr magnesium alloy
    Peng Xiaodong
    Yang Yan
    Wei Qunyi
    Xie Weidong
    Ning Xu
    ADVANCED STRUCTURAL MATERIALS, 2011, 686 : 247 - 252
  • [3] Microstructure and mechanical properties of Mg-9Li-3Al-xGd alloys
    Zhang, B.
    Peng, X. D.
    Ma, Y.
    Li, Y. M.
    Yu, Y. Q.
    Wei, G. B.
    MATERIALS SCIENCE AND TECHNOLOGY, 2015, 31 (09) : 1035 - 1041
  • [5] Influence of extrusion temperature on microstructure and mechanical behavior of duplex Mg-Li-Al-Sr alloy
    Yang, Yan
    Xiong, Xiaoming
    Su, Junfei
    Peng, Xiaodong
    Wen, Haiming
    Wei, Guobing
    Pan, Fusheng
    Lavernia, Enrique J.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 750 : 696 - 705
  • [6] Influence of RE on microstructure and mechanical properties of Mg-Li-Al alloys
    Liu, B.
    Zhang, M. L.
    Niu, Z. Y.
    2006 BIMW: 2006 BEIJING INTERNATIONAL MATERIALS WEEK, PTS 1-4: MAGNESIUM, 2007, 546-549 : 211 - +
  • [7] 挤压态Mg-9Li-3Al-xSr镁合金的微观组织与力学性能
    杨艳
    彭晓东
    李俊辰
    谢卫东
    魏国兵
    魏群义
    重庆大学学报, 2013, 36 (12) : 103 - 110
  • [8] Mechanical behavior of Mg-Li-Al alloys
    Rahulan, N.
    Gopalan, Sundararaman
    Kumaran, S.
    MATERIALS TODAY-PROCEEDINGS, 2018, 5 (09) : 17935 - 17943
  • [9] Influence of Sn on microstructure and mechanical properties of Mg-5Li-3Al-2Zn alloys
    Xiang, Q.
    Wu, R. Z.
    Zhang, M. L.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 477 (1-2) : 832 - 835
  • [10] Influence of Sn on microstructure and mechanical properties of Mg-5Li-3Al-2Zn alloys
    Xiang, Q.
    Wu, R.Z.
    Zhang, M.L.
    Journal of Alloys and Compounds, 2009, 477 (1-2): : 832 - 835