Stress corrosion cracking of X-70 pipeline steels by eletropulsing treatment in near-neutral pH solution

被引:0
|
作者
Bingyan Fang
Jianqiu Wang
Suhong Xiao
En-Hou Han
Ziyong Zhu
Wei Ke
机构
[1] Institute of Metal Research,Environmental Corrosion Center, Chinese Academy of Sciences
来源
关键词
Polymer; Grain Size; Electron Microscopy; Scanning Electron Microscopy; Tensile Strength;
D O I
暂无
中图分类号
学科分类号
摘要
Slow strain rate tests (SSRT) and environmental scanning electron microscopy (ESEM) were utilized to investigate stress corrosion cracking (SCC) behavior of electropulsed POSCO and Bao Steel X-70 pipeline steels specimens in XJ solution purged with 5% CO2 + 95% N2 at the strain rate of 2E-6/s. The results showed that the ultimate tensile strengths (UTS) were raised considerably for the electropulsed specimens. The UTS for electropulsed POSCO X-70 pipeline steel was enhanced much more compared to electropulsed Bao Steel X-70 pipeline steel. In addition, the relationship among UTS, the original grain size and high voltage in electropulsing treatment was revealed. SCC sensitivity increased with the decreasing electrochemical potential, especially at high cathodic potential.
引用
收藏
页码:6545 / 6552
页数:7
相关论文
共 50 条
  • [1] Stress corrosion cracking of X-70 pipeline steels by eletropulsing treatment in near-neutral pH solution
    Fang, BY
    Wang, JQ
    Xiao, SH
    Han, EH
    Zhu, ZY
    Ke, W
    JOURNAL OF MATERIALS SCIENCE, 2005, 40 (24) : 6545 - 6552
  • [2] Hydrogen in stress corrosion cracking of X-70 pipeline steels in near-neutral pH solutions
    Bingyan Fang
    En-Hou Han
    Jianqiu Wang
    Ziyong Zhu
    We Ke
    Journal of Materials Science, 2006, 41 : 1797 - 1803
  • [3] Hydrogen in stress corrosion cracking of X-70 pipeline steels in near-neutral pH solutions
    Fang, BY
    Han, EH
    Wang, JQ
    Zhu, ZY
    Ke, W
    JOURNAL OF MATERIALS SCIENCE, 2006, 41 (06) : 1797 - 1803
  • [4] Mechanical and environmental influences on stress corrosion cracking of an X-70 pipeline steel in dilute near-neutral pH solutions
    Fang, B.
    Han, E.-H.
    Wang, J.
    Ke, W.
    CORROSION, 2007, 63 (05) : 419 - 432
  • [5] Corrosion behavior of X-70 pipe steel in near-neutral pH solution
    Niu, L.
    Cheng, Y. F.
    APPLIED SURFACE SCIENCE, 2007, 253 (21) : 8626 - 8631
  • [6] Effect of Dissolved Oxygen on Stress Corrosion Cracking of X70 Pipeline Steel in Near-Neutral pH Solution
    Liu, Z. Y.
    Li, X. G.
    Du, C. W.
    Wang, L. X.
    Huang, Y. Z.
    CORROSION, 2010, 66 (01)
  • [7] Microstructural effect on near-neutral pH stress corrosion cracking resistance of pipeline steels
    Bulger, J. T.
    Lu, B. T.
    Luo, J. L.
    JOURNAL OF MATERIALS SCIENCE, 2006, 41 (15) : 5001 - 5005
  • [8] Microstructural effect on near-neutral pH stress corrosion cracking resistance of pipeline steels
    J. T. Bulger
    B. T. Lu
    J. L. Luo
    Journal of Materials Science, 2006, 41 : 5001 - 5005
  • [9] Effect of cyclic loading on cracking behaviour of X-70 pipeline steel in near-neutral pH solutions
    Guo, H
    Li, GF
    Cai, X
    Yang, RP
    Yang, W
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2005, 21 (04) : 459 - 464
  • [10] SCC behaviour of X-70 pipeline steel in near-neutral pH solutions
    Guo, H
    Li, GF
    Cai, X
    Zhou, JJ
    Yang, W
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2005, 21 (01) : 33 - 38