摘要
Ni–20 wt.% Cu was oxidized in different oxygen pressures from 1×10−5 to 1 atm at 700–1100°C. The oxidation consisted of an initial transient period in which a composite scale of NiO and Cu oxides formed, and a subsequent quasi steady-state regime during which parabolic growth of NiO determined the overall oxidation rate. Based on the oxide composition and the oxygen- pressure dependence of the parabolic rate constant, it is concluded that outward transport of Ni via vacancies determines the growth rate of the oxide during the steady-state period, either in the grain boundaries or in the lattice. The influence of Cu dissolved in NiO on the oxidation rate and the oxygen-pressure dependence of the parabolic rate constants is discussed.
引用
收藏
页码:571 / 583
页数:12
相关论文
共 50 条
  • [1] High-temperature oxidation of Ni-20 wt.% Cu from 700 to 1100°C
    Haugsrud, R
    OXIDATION OF METALS, 2001, 55 (5-6): : 571 - 583
  • [2] High-temperature oxidation of Cu-30 wt.% Ni-15 wt.% Fe
    Haugsrud, R
    Norby, T
    Kofstad, P
    CORROSION SCIENCE, 2001, 43 (02) : 283 - 299
  • [3] High-temperature oxidation of Cu-10 wt% Ni and Cu-15 wt% Ni at 900-1050°C
    Haugsrud, R
    CORROSION SCIENCE, 2000, 42 (02) : 383 - 399
  • [4] Oxidation of Two Ternary Cu–Ni–20 wt.% Cr Alloys at 700–800°C in 1 atm O2
    Z. Q. Cao
    Y. Niu
    F. Gesmundo
    Oxidation of Metals, 2001, 56 : 287 - 297
  • [5] Oxidation of two ternary Cu-Ni-20 wt.% Cr alloys at 700-800°C in 1 atm O2
    Cao, ZQ
    Niu, Y
    Gesmundo, F
    OXIDATION OF METALS, 2001, 56 (3-4): : 287 - 297
  • [6] High temperature oxidation behaviour of Fe-15.7 wt.% Cr-8.5 wt.% Mn in oxygen without and with water vapour at 700 °C
    Chandra-ambhorn, S.
    Saranyachot, P.
    Thublaor, T.
    CORROSION SCIENCE, 2019, 148 : 39 - 47
  • [7] High-temperature compression behavior of W-10 wt.%Cu composite
    Lin, Dongguo
    Han, Jun Sae
    Kwon, Young Sam
    Ha, Sangyul
    Bollina, Ravi
    Park, Seong Jin
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2015, 53 : 87 - 91
  • [8] High-temperature oxidation behavior of Cu-20Ni-75Co alloy
    Cao, Zhongqiu
    Li, Fengchun
    Shen, Ying
    ADVANCED ENGINEERING MATERIALS III, PTS 1-3, 2013, 750-752 : 659 - 662
  • [9] High-temperature oxidation behaviour of refurbished (Ni,Pt)Al coating on Ni-based superalloy at 1100 °C
    Zhang, C. Y.
    Ma, Z.
    Dong, S. Z.
    Xu, M. M.
    Li, S.
    Zhang, C.
    Jiang, C. Y.
    Bao, Z. B.
    Zhu, S. L.
    Wang, F. H.
    CORROSION SCIENCE, 2021, 187
  • [10] High-temperature stability of Ni-3 wt.% SiCNP composite and the effect of milling time
    Yang, Chao
    Huang, Hefei
    Zhou, Xiaoling
    Li, Zhijun
    Zhou, Xingtai
    Xia, Tian
    Zhang, Deliang
    JOURNAL OF NUCLEAR MATERIALS, 2015, 467 : 635 - 643