The molten Fe80P13C7 alloys can achieve a large undercooling up to 320 K by fluxing technique. With the help of fluxing technique, the molten Fe80P13C7 alloys can be solidified at different undercooling (ΔT) through isothermal undercooling experiment. It is indicated that the microstructure of the solidified Fe80P13C7 alloy specimens is refined significantly with the increasing undercooling and the grain size is about 20 μm, 10 μm, 200 nm and 70 nm for ΔT=50 K, 150 K, 250 K and 320 K, respectively. The solidification morphologies of the solidified Fe80P13C7 alloy specimens under different undercooling are quite different. When ΔT=50 K, it presents a traditional solidification microstructure under a undercooling condition, composed of the primary dendrite and anomalous eutectic within the dendrites. When ΔT=150 K, a cell-like solidification morphology can be found, which can be proposed to be formed based on the nucleation and growth of spinodal decomposition mechanism. When ΔT=250 K, there is a strong direction of the solidification under an optical micrograph, two zones can be divided, and the microstructure of each zone presents a network which results from a liquid spinodal decomposition. When ΔT=320 K, the microstructure presents a random network completely. Microhardness test shows that the hardness of the solidified specimens increases with the undercooling.
引用
收藏
页码:1626 / 1630
页数:4
相关论文
共 50 条
  • [1] Solidified morphology and mechanism of bulk nanocrystalline Fe80P13C7 alloy at isothermal undercooling
    Wang Tuo
    Li Qiang
    SCIENCE CHINA-TECHNOLOGICAL SCIENCES, 2014, 57 (08) : 1626 - 1630
  • [2] Solidified morphology and mechanism of bulk nanocrystalline Fe80P13C7 alloy at isothermal undercooling
    WANG Tuo
    LI Qiang
    Science China(Technological Sciences), 2014, (08) : 1626 - 1630
  • [3] Formation of bulk magnetic ternary Fe80P13C7 glassy alloy
    Li, Qiang
    Li, Jinfeng
    Gong, Pan
    Yao, Kefu
    Gao, Jingen
    Li, Hongxiang
    INTERMETALLICS, 2012, 26 : 62 - 65
  • [4] MAGNETIC DOMAINS OF AN AMORPHOUS FE80P13C7 ALLOY
    TAKAHASHI, M
    SUZUKI, T
    MIYAZAKI, T
    JAPANESE JOURNAL OF APPLIED PHYSICS, 1977, 16 (03) : 521 - 522
  • [5] CRYSTALLIZATION OF FE80P13C7 AMORPHOUS ALLOY POWDER
    SATO, T
    ICHIYAMA, T
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1990, 9 (06) : 652 - 654
  • [6] Enhancement of plasticity by cryogenic thermal cycling on Fe80P13C7 bulk amorphous alloy
    Guan, Huimin
    Li, Mingcan
    MATERIALS LETTERS, 2021, 300
  • [7] Compaction of bulk ferromagnetic Fe80P13C7 amorphous alloys
    Chan, FW
    Ma, NG
    Kui, HW
    JOURNAL OF MATERIALS RESEARCH, 2001, 16 (10) : 2767 - 2769
  • [8] MAGNETIC-ANISOTROPY OF AN AMORPHOUS FE80P13C7 ALLOY
    TAKAHASHI, M
    ONO, F
    TAKAKURA, K
    JAPANESE JOURNAL OF APPLIED PHYSICS, 1976, 15 (01) : 183 - 184
  • [9] MAGNETIC-ANISOTROPY IN AN AMORPHOUS FE80P13C7 ALLOY
    TAKAHASHI, M
    MIYAZAKI, T
    JAPANESE JOURNAL OF APPLIED PHYSICS, 1979, 18 (04) : 743 - 752
  • [10] STUDY OF CRYSTALLOGRAPHICAL STRUCTURE FOR AN AMORPHOUS FE80P13C7 ALLOY
    TAKAHASHI, M
    SUZUKI, T
    JAPANESE JOURNAL OF APPLIED PHYSICS, 1976, 15 (08) : 1555 - 1556