Influence of annealing duration on the erosive wear behavior of polyphenylenesulphide composites

被引:10
|
作者
Yilmaz, Taner [1 ,2 ]
机构
[1] Kocaeli Univ, Civil Aviat Coll, TR-41285 Izmit, Turkey
[2] Kocaeli Univ, Grad Sch Nat & Appl Sci, TR-41380 Izmit, Turkey
关键词
SOLID PARTICLE EROSION; TRANSCRYSTALLINE INTERPHASE; MECHANICAL-PROPERTIES; FIBER; PERFORMANCE; CRYSTALLIZATION; POLYETHERIMIDE; MORPHOLOGY; PARAMETERS; EPOXY;
D O I
10.1007/s10853-009-4204-2
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The influence of annealing duration on the erosive wear behavior of short glass fiber (40% w/w) and CaCO3 mineral particulate (25% w/w)-short glass fiber (40% w/w) (total: 65% w/w) reinforced PPS composites has been characterized under various experimental conditions by differential scanning calorimetry (DSC) and erosion measurements. The erosive wear of the composites have been evaluated at different impingement angles (30, 45, 60, and 90A degrees) and at four different annealing periods (30, 60, 90, and 120 min). Increase in the total crystallization causes an improvement in the erosive wear properties of the samples. Annealing time controls the morphology by influencing the degree of crystallinity in the matrix and in the fiber-matrix interface. This formation restricts fiber-matrix debonding. There is no linear proportionality between annealing time and relative degree of crystallization. The results indicate that PPS composites show maximum in wear versus impact angle relation at 60A degrees confirming their semi-ductile failure behavior. The morphologies of eroded surface are examined by the scanning electron microscope.
引用
收藏
页码:2381 / 2389
页数:9
相关论文
共 50 条
  • [1] Influence of annealing duration on the erosive wear behavior of polyphenylenesulphide composites
    Taner Yilmaz
    Journal of Materials Science, 2010, 45 : 2381 - 2389
  • [2] Erosive wear behaviour of polyphenylenesulphide (PPS) composites
    Sinmazcelik, Tamer
    Taskiran, Isa
    MATERIALS & DESIGN, 2007, 28 (09): : 2471 - 2477
  • [3] Erosive wear behavior of sprayed metal matrix composites: An overview
    Pasha, Mudasar
    Kaleemulla, Mohammed
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART J-JOURNAL OF ENGINEERING TRIBOLOGY, 2013, 227 (10) : 1063 - 1075
  • [4] Investigation on the erosive wear behavior of SiC-modified epoxy composites
    Xia, YF
    Huang, ZH
    Pan, W
    Qi, LH
    Miao, HZ
    RARE METAL MATERIALS AND ENGINEERING, 2005, 34 : 536 - 539
  • [5] EROSIVE WEAR OF FIBROUS PEEK COMPOSITES
    LHYMN, C
    LHYMN, YO
    ADVANCED MATERIALS : THE BIG PAYOFF, 1989, 21 : 720 - 729
  • [6] Influence of angle of incidence, temperature and SiC content on erosive wear behavior of ZrB2-SiC composites
    Gupta, Yashpal
    Venkateswaran, T.
    Kumar, B. Venkata Manoj
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2020, 17 (02) : 459 - 467
  • [7] Erosive wear and wear mechanism of in situ TiCP/Fe composites
    Liu, ZJ
    Ning, ZL
    Li, FZ
    Yao, XR
    Ren, SZ
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2005, 21 (05) : 719 - 723
  • [8] Erosive Wear and Wear Mechanism of in situ TiCP/Fe Composites
    Zhaojing LIU
    Journal of Materials Science & Technology, 2005, (05) : 113 - 117
  • [9] Erosive wear of advanced composites based on WC
    Hussainova, Irina
    Antonov, Maksim
    Zikin, Arkadi
    TRIBOLOGY INTERNATIONAL, 2012, 46 (01) : 254 - 260
  • [10] Erosive wear behaviour in duophase SiAlON composites
    Liu, DM
    Lin, JT
    Lee, RRR
    CERAMICS INTERNATIONAL, 1998, 24 (03) : 217 - 221