Enhanced high-voltage cycling stability of Ni-rich cathode materials via the self-assembly of Mn-rich shells

被引:53
|
作者
Dong, Xinyu [1 ,2 ]
Yao, Junyi [1 ,2 ]
Zhu, Wenchang [1 ,2 ]
Huang, Xue [1 ,2 ]
Kuai, Xiaoxiao [1 ,2 ]
Tang, Jing [3 ,5 ]
Li, Xiaolong [4 ]
Dai, Shuyan [1 ,2 ]
Shen, Liwei [1 ,2 ]
Yang, Ruizhi [1 ,2 ]
Gao, Lijun [1 ,2 ]
Zhao, Jianqing [1 ,2 ]
机构
[1] Soochow Univ, Soochow Inst Energy & Mat Innovat SIEMIS, Coll Energy, Suzhou 215006, Peoples R China
[2] Soochow Univ, Key Lab Adv Carbon Mat & Wearable Energy Technol, Suzhou 215006, Peoples R China
[3] East China Normal Univ, Shanghai Key Lab Green Chem & Chem Proc, Sch Chem & Mol Engn, Shanghai 20062, Peoples R China
[4] Chinese Acad Sci, Shanghai Adv Res Inst, Shanghai 201204, Peoples R China
[5] Univ Queensland, AIBN, Sch Chem Engn, Brisbane, Qld 4072, Australia
基金
中国国家自然科学基金;
关键词
LAYERED OXIDE CATHODES; LITHIUM-ION BATTERIES; CORE-SHELL; ELECTRODE MATERIALS; HIGH-ENERGY; LONG-LIFE; HIGH-CAPACITY; METAL OXIDE; SURFACE; INTERFACE;
D O I
10.1039/c9ta07147d
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Ni-rich layered LiNi1-x-yMnxCoyO2 (NMC, x + y < 0.5) oxides have been demonstrated to be promising cathode materials for high-energy lithium-ion batteries. However, when cycled at high voltages, NMC cathode materials with high Ni content usually show unsatisfactory capacity decay and voltage fading due to side reactions and electrochemical irreversibility during prolonged lithiation/delithiation cycles. Here, we report a Mn-rich Li0.65Mn0.59Ni0.12Co0.13O<delta> (LMNCO) material that consists of layered Li2MnO3 and spinel LiMn1.5Ni0.5O4-type components. LMNCO is a desirable shell material for improving the high-voltage cycling stability of Ni-rich LiNi0.8Mn0.1Co0.1O2 (NMC811) cathode materials. Core-shell-structured NMC811@x% LMNCO materials were fabricated with satisfactory structural conformality via sonofragmentation followed by solvent evaporation-induced self-assembly and post-annealing processes. The optimized NMC811@5% LMNCO cathode material can deliver an initial discharge capacity of 150.0 mA h g(-1) at 5C (1C = 200 mA g(-1)) in a voltage range of 2.7-4.6 V vs. Li+/Li with 83.4% retention for up to 500 cycles, significantly superior to that of the bare NMC811 material (75.6%). The Mn-rich shell also enables the effective stabilization of the Ni-rich cathode materials for long-term cycling at high voltages and 55 degrees C. In addition, this work offers a synthetic prototype for the fabrication of conformal core-shell-structures, which could be adopted for the surface modification of various functional materials to achieve enhanced performance in device applications.
引用
收藏
页码:20262 / 20273
页数:12
相关论文
共 50 条
  • [1] The Origin of High-Voltage Stability in Single-Crystal Layered Ni-Rich Cathode Materials
    Sun, Jianming
    Cao, Xin
    Yang, Huijun
    He, Ping
    Dato, Michael A.
    Cabana, Jordi
    Zhou, Haoshen
    ANGEWANDTE CHEMIE-INTERNATIONAL EDITION, 2022, 61 (40)
  • [2] Challenges and Modification Strategies of Ni-Rich Cathode Materials Operating at High-Voltage
    Liao, Caijian
    Li, Fangkun
    Liu, Jun
    NANOMATERIALS, 2022, 12 (11)
  • [3] Overall structural modification of a layered Ni-rich cathode for enhanced cycling stability and rate capability at high voltage
    Tang, Manjing
    Yang, Jun
    Chen, Nantao
    Zhu, Shengcai
    Wang, Xing
    Wang, Tian
    Zhang, Congcong
    Xia, Yongyao
    JOURNAL OF MATERIALS CHEMISTRY A, 2019, 7 (11) : 6080 - 6089
  • [4] Suppress moisture sensitivity of Ni-rich cathode materials by bioinspired self-assembly hydrophobic layer
    Huang, Yingde
    Li, Pei-Yao
    Wei, Han-Xin
    Luo, Yu-Hong
    Tang, Lin-Bo
    Chen, He-Zhang
    Zhang, Xia-hui
    Zheng, Jun-chao
    CHEMICAL ENGINEERING JOURNAL, 2023, 477
  • [5] Structural and interfacial stability of a coated Ni-rich layered oxide cathode at high-voltage operation
    Llanos, Princess Stephanie
    Ahaliabadeh, Zahra
    Miikkulainen, Ville
    Kong, Xiangze
    Obrezkov, Filipp
    Lahtinen, Jouko
    Yao, Lide
    Jiang, Hua
    Lassi, Ulla
    Kallio, Tanja
    MATERIALS TODAY ENERGY, 2025, 50
  • [6] Understanding the effects of surface modification on improving the high-voltage performance of Ni-rich cathode materials
    Liu, Siyang
    Su, Junming
    Zhang, Congcong
    Chen, Xiang
    Zhao, Jiayue
    Huang, Tao
    Wu, Jianhua
    Yu, Aishui
    MATERIALS TODAY ENERGY, 2018, 10 : 40 - 47
  • [7] Enhanced interfacial stability of Ni-rich cathode for Li-ion batteries towards excellent high-voltage performance
    Zhang, Dianwei
    Li, Yunjiao
    Xi, Xiaoming
    Wang, Shan
    Hao, Shuaipeng
    Lei, Tongxin
    Ren, Xugang
    Xiong, Yike
    Liu, Shuaiwei
    Zheng, Junchao
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 906
  • [8] Enhanced cycling stability and storage performance of Na0.67Ni0.33Mn0.67-xTixO1.9F0.1 cathode materials by Mn-rich shells and Ti doping
    Li, Xin
    Kong, Qingquan
    An, Xuguang
    Zhang, Jing
    Wang, Qingyuan
    Yao, Weitang
    JOURNAL OF COLLOID AND INTERFACE SCIENCE, 2023, 633 : 82 - 91
  • [9] Enhanced cycling stability and storage performance of Na0.67Ni0.33Mn0.67-xTixO1.9F0.1 cathode materials by Mn-rich shells and Ti doping
    Li, Xin
    Kong, Qingquan
    An, Xuguang
    Zhang, Jing
    Wang, Qingyuan
    Yao, Weitang
    JOURNAL OF COLLOID AND INTERFACE SCIENCE, 2023, 633 : 82 - 91
  • [10] Enhanced cycling stability and storage performance of Na0.67Ni0.33Mn0.67-xTixO1.9F0.1 cathode materials by Mn-rich shells and Ti doping
    Li X.
    Kong Q.
    An X.
    Zhang J.
    Wang Q.
    Yao W.
    Journal of Colloid and Interface Science, 2023, 633 : 82 - 91