Corrosion behaviour of aluminium nitride in liquid aluminium: Influence of the microstructure

被引:2
|
作者
Roulet, F
Tristant, P
Desmaison, J
Rezakhanlou, R
Ferrato, M
机构
[1] Univ Limoges, ESA CNRS 6015, Lab Mat Ceram & Traitements Surface, F-87060 Limoges, France
[2] EDF DER DEM, Ctr Rech Renardieres, F-77250 Moret Sur Loing, France
[3] Ceram & Composites Ctr Bazet, F-65460 Bazet, France
关键词
D O I
10.1016/S0955-2219(97)00069-1
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The intrinsic characteristics of sintered aluminium nitride (mechanical, thermal, chemical) facilitate their use in production of heater element protection tubes for molten aluminium industries. Two kinds of industrial materials are characterised from the mechanical and thermal point of view. Moreover the samples' microstructure is observed before and after corrosion tests in liquid aluminium alloy (dipped finger method). The two batches exhibit identical mechanical properties and the thermal conductivity decreases from 170 Wm(-1) K-1 at room temperature to 35 W m(-1) K-1 at 1000 degrees C. Conversely, the distribution of the secondary phase (YAG) depends on the material. Despite the microstructure differences revealed by scanning (SEM) and transmission (TEM) electron microscopy, no corrosion is observed after 2000 h tests in molten aluminium alloy. These results confirm that AlN could be a good candidate for this application. (C) 1997 Elsevier Science Limited.
引用
收藏
页码:1877 / 1883
页数:7
相关论文
共 50 条
  • [1] Corrosion behaviour of aluminium nitride in liquid aluminium: Influence of the microstructure
    Lab. Mat. Ceramiques Traitements S., ESA CNRS 6015, Université de Limoges, 123 av. Albert Thomas, F-87060 Limoges, France
    不详
    不详
    Journal of the European Ceramic Society, 17 (15-16): : 1877 - 1883
  • [2] The influence of mechanical grinding on the microstructure and corrosion behaviour of A356 aluminium alloys
    Goodall, M. D.
    Pawar, S.
    Curioni, M.
    Morsch, S.
    Unthank, M. G.
    Gibbon, S. R.
    Zhou, X.
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2022, 57 (02) : 97 - 104
  • [3] Microstructure and corrosion behaviour of aluminium fly ash composites
    Bieniás, J
    Walczak, M
    Surowska, B
    Sobczak, J
    JOURNAL OF OPTOELECTRONICS AND ADVANCED MATERIALS, 2003, 5 (02): : 493 - 502
  • [4] OBSERVATION OF MICROSTRUCTURE AND CORROSION BEHAVIOUR OF SOME ALUMINIUM BRONZES.
    Lorimer, G.W.
    Hasan, F.
    Iqbal, J.
    Ridley, N.
    British Corrosion Journal, 1986, 21 (04): : 244 - 248
  • [5] Influence of microstructure on wear behaviour of cast aluminium alloy
    Dwivedi, DK
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2003, 56 (03): : 215 - 220
  • [6] Influence of aluminium on the corrosion behaviour of binary magnesium-aluminium alloys in saline solutions
    Hoyer, P.
    Angrisani, G. L.
    Klose, C.
    Bach, Fr-W
    Hassel, T.
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2014, 65 (01): : 23 - 30
  • [7] Corrosion behaviour and related mechanism of lithium vapour on aluminium nitride ceramic
    Li, Bao-rang
    Wen, Bo
    Chen, Hao-zhi
    Zhang, Wei
    Meng, Xiao
    Jia, Ming-yong
    Chen, Fei
    CORROSION SCIENCE, 2021, 178
  • [9] Influence of microstructure and impurities on thermal conductivity of aluminium nitride ceramics
    Ruckmich, S
    ZEITSCHRIFT FUR METALLKUNDE, 2001, 92 (07): : 839 - 844
  • [10] Anodizing and corrosion behaviour of aluminium
    B. Doğru Mert
    B. Yazici
    T. Tüken
    G. Kardaş
    M. Erbil
    Protection of Metals and Physical Chemistry of Surfaces, 2011, 47 : 102 - 107