Impact of curing time on ageing and degradation of phenol-urea-formaldehyde binder

被引:20
|
作者
Okhrimenko, D., V [1 ]
Thomsen, A. B. [2 ]
Ceccato, M. [1 ]
Johansson, D. B. [2 ]
Lybye, D. [2 ]
Bechgaard, K. [1 ]
Tougaard, S. [3 ]
Stipp, S. L. S. [1 ]
机构
[1] Univ Copenhagen, Dept Chem, Nanosci Ctr, DK-2100 Copenhagen OE, Denmark
[2] ROCKWOOL Int AS, Hovedgaden 584, DK-2640 Hedehusene, Denmark
[3] Univ Southern Denmark, Dept Phys Chem & Pharm, DK-5230 Odense M, Denmark
关键词
Coatings; Material stability; Mineral wool; Fibers; Resin; AMINO PROPYL TRIETHOXYSILANE; E-GLASS SURFACE; RESOL RESINS; C-13; NMR; HYDROLYTIC STABILITY; THERMAL-DEGRADATION; MASS-SPECTROMETRY; WOOD ADHESIVES; SPECTROSCOPY; SILANE;
D O I
10.1016/j.polymdegradstab.2018.04.001
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Phenol-urea-formaldehyde (PUF) resin is one of the most important thermosetting polymers. It is widely used in many industrial and construction applications as an organic coating and adhesive. For example, in production of mineral wool for insulation, PUF is used together with the coupling agent (3-aminopropylsilane, APS) and serves as a binder for attaching mineral fibers to each other and to create the necessary mechanical integrity and shape of the final product. However, during ageing under high humidity (95%) and temperature (70 degrees C), hydrolysis can degrade PUF, decreasing product quality. A better understanding of the chemical processes caused by hydrolysis would promote development of more stable PUF binders. We investigated the composition and stability changes during ageing of cured PUF powder binder and mineral wool fibers where PUF binds the fibers together. We aged the samples in hot water (80 degrees C) or in a controlled climate chamber (70 C; 91% RH) and analyzed them using X-ray photoelectron spectroscopy (XPS), element analysis and thermogravimetric (TG) analysis. We investigated the composition of species released from PUF during hydrolysis by electrospray ionization (ESI) of the aqueous solutions. The results show that the extent of PUF curing and the presence of APS as the coupling agent have an important impact on its stability. XPS revealed that poorly cured PUF contains a high fraction of NH-CH2-O-CH2-NH bonds which are easily hydrolyzed, while longer curing results mostly in more stable methylene bridges, NH-CH2-NH. We also observed evidence for urea NH CO bond decomposition by ESI analysis. Mineral wool fiber ageing studies showed that PUF rearranges on the fiber surface and detaches from it, together with the APS coupling agent. This improved understanding of the effects of ageing provides clues for designing a more robust binder, leading to increased quality and stability of mineral wool insulation. (C) 2018 Elsevier Ltd. All rights reserved.
引用
收藏
页码:86 / 94
页数:9
相关论文
共 50 条
  • [1] New accelerators of phenol-formaldehyde resins curing time and formulation of phenol-urea-formaldehyde co-condensed resins
    Zhao, CH
    Pizzi, A
    36th International Wood Composite Materials Symposium, Proceedings, 2002, : 139 - 139
  • [2] Investigation of the ageing effects on phenol-urea-formaldehyde binder and alkanol amine-acid anhydride binder coated mineral fibres
    Zafar, A.
    Schjodt-Thomsen, J.
    Sodhi, R.
    Goacher, R.
    de Kubber, D.
    POLYMER DEGRADATION AND STABILITY, 2013, 98 (01) : 339 - 347
  • [3] Influence of the synthesis conditions on the curing behavior of phenol-urea-formaldehyde resol resins
    He, GB
    Yan, N
    JOURNAL OF APPLIED POLYMER SCIENCE, 2005, 95 (06) : 1368 - 1375
  • [4] Chemical Structure and Curing Behavior of Phenol-Urea-Formaldehyde Cocondensed Resins of High Urea Content
    Fan, Dongbin
    Li, Jianzhang
    Chang, Jianmin
    Gou, Jinsheng
    Jiang, Jinxue
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2009, 23 (13-14) : 1787 - 1797
  • [5] Dissolution of Stone Wool Fibers with Phenol-urea-formaldehyde Binder in a Synthetic Lung Fluid
    Barly, Susanne H. Q.
    Okhrimenko, Denis V.
    Solvang, Mette
    Yue, Yuanzheng
    Stipp, Susan L. S.
    CHEMICAL RESEARCH IN TOXICOLOGY, 2019, 32 (12) : 2398 - 2410
  • [6] ANALYSIS OF CURING PROCESS AND THERMAL-PROPERTIES OF PHENOL-UREA-FORMALDEHYDE COCONDENSED RESINS
    TOMITA, B
    OHYAMA, M
    ITOH, A
    DOI, K
    HSE, CH
    MOKUZAI GAKKAISHI, 1994, 40 (02): : 170 - 175
  • [7] Phenol-urea-formaldehyde cocondensed resol resins: Their synthesis, curing kinetics, and network properties
    He, GB
    Riedl, B
    JOURNAL OF POLYMER SCIENCE PART B-POLYMER PHYSICS, 2003, 41 (16) : 1929 - 1938
  • [8] PHENOL-UREA-FORMALDEHYDE BINDER TOL-2 FOR HIGH-REACTIVITY CORESANDS.
    Voronin, Yu.F.
    Sinchugov, Yu.D.
    Koshelev, V.I.
    Parfenov, Yu.A.
    Kozlova, G.I.
    Soviet Castings Technology (English Translation of Liteinoe Proizvodstvo), 1987, (08): : 23 - 26
  • [9] Influence of Nanoclay on Phenol-Formaldehyde and Phenol-Urea-Formaldehyde Resins for Wood Adhesives
    Lei, H.
    Du, G.
    Pizzi, A.
    Celzard, A.
    Fang, Q.
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2010, 24 (8-10) : 1567 - 1576
  • [10] Encapsulation of bioinsecticide oil in phenol-urea-formaldehyde terpolymer
    Patil, Rahul D.
    Bendre, Ratnamala S.
    JOURNAL OF MACROMOLECULAR SCIENCE PART A-PURE AND APPLIED CHEMISTRY, 2022, 59 (05): : 366 - 378