Crack Propagation Behavior of SNCM439 Steels in High-pressure Hydrogen Gas

被引:2
|
作者
Arashima, Hironobu [1 ]
Masada, Satoru [1 ]
Isobe, Shigehito [2 ]
Hashimoto, Naoyuki [2 ]
机构
[1] Japan Steel Works M&E Inc, 4 Chatsucho, Muroran, Hokkaido 0518505, Japan
[2] Hokkaido Univ, Kita Ku, N13,W8, Sapporo, Hokkaido 0608628, Japan
关键词
low-alloy steel; high-pressure hydrogen gas; hydrogen embrittlement; stress intensity factor; rising load test; crack initiation; INITIATION;
D O I
10.2355/isijinternational.ISIJINT-2022-017
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
To investigate the effect of high-pressure hydrogen gas on the fracture of high-strength low-alloy steels, rising load tests were conducted on JIS SNCM439 steel in high-pressure (20 MPa) hydrogen gas at room temperature (20-25 degrees C), and its hydrogen-induced crack initiation behavior was investigated. The load-crack opening displacement curve obtained for rising load tests in hydrogen began to deviate from that obtained in air at very low loads, indicating that the stress intensity factor at crack initiation was significantly smaller in hydrogen. Scanning electron microscopy observations of the fractured surfaces of the specimens unloaded during the middle of the rising load test confirmed that hydrogen-induced cracks had already occurred at a load lower than the deviation point. The stretch zone that appeared in the rising load test in air was not observed for the test in hydrogen, and the hydrogen-induced cracks were found to directly initiate from the tip of the fatigue pre-crack. The hydrogen-induced cracks were initiated at almost the same stress intensity factor value as that at which the stretch zone was observed in air, indicating that plastic slip and the resulting hydrogen ingress from the new surface were the causes of the hydrogen embrittlement. In addition, it was shown that the stress intensity factor for crack initiation in hydrogen increased and the effect of hydrogen decreased with the increase in loading rate, inferring that dislocation migration and hydrogen penetration into the steel are key factors for hydrogen embrittlement.
引用
收藏
页码:1540 / 1547
页数:8
相关论文
共 50 条
  • [1] Effects of inclusions on the fatigue life of SNCM439 steel in high-pressure hydrogen gas
    Arashima, Hironobu
    Yanagisawa, Yusuke
    Ikeda, Ryo
    Isobe, Shigehito
    Hashimoto, Naoyuki
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2022, 47 (59) : 25057 - 25065
  • [2] Phenomenological Aspect of Hydrogen Enviroment Embrittlement of SNCM439 Steels
    Arashima, Hironobu
    Masada, Satoru
    Itoh, Hideaki
    Ohnishi, Keizo
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2010, 96 (02): : 76 - 83
  • [3] Gigacycle fatigue behaviors of two SNCM439 steels with different tensile strengths
    Zheng Duan
    Xian-Feng Ma
    Hui-Ji Shi
    Ryosuke Murai
    Eiichi Yanagisawa
    Acta Mechanica Sinica, 2011, 27 : 778 - 784
  • [4] Gigacycle fatigue behaviors of two SNCM439 steels with different tensile strengths
    Duan, Zheng
    Ma, Xian-Feng
    Shi, Hui-Ji
    Murai, Ryosuke
    Yanagisawa, Eiichi
    ACTA MECHANICA SINICA, 2011, 27 (05) : 778 - 784
  • [5] Gigacycle fatigue behaviors of two SNCM439 steels with different tensile strengthes
    Ryosuke Murai
    Eiichi Yanagisawa
    Acta Mechanica Sinica, 2011, 27 (05) : 778 - 784
  • [6] Evaluation of fatigue strength in very-long life regime of SNCM439 steels
    Akiniwa, Yoshiaki
    Tanaka, Keisuke
    Nakatsu, Akira
    Nippon Kikai Gakkai Ronbunshu, A Hen/Transactions of the Japan Society of Mechanical Engineers, Part A, 2004, 70 (08): : 1036 - 1041
  • [7] Effect of Hydrogen on the Notch Tensile Strength of JIS SNCM439 Steel
    Arashima, Hironobu
    Masada, Satoru
    MATERIALS TRANSACTIONS, 2021, 62 (08) : 1133 - 1140
  • [8] Fatigue crack growth behavior and hydrogen penetration properties in austenitic stainless steels exposed to high-pressure hydrogen gas environments
    Mine, Yoji
    Narazaki, Chihiro
    Kanezaki, Toshihiko
    Matsuoka, Saburo
    Murakami, Yukitaka
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2007, 93 (03): : 247 - 256
  • [9] Investigation of hydrogen transport behavior of various low-alloy steels with high-pressure hydrogen gas
    Yamabe, Junichiro
    Awane, Tohru
    Matsuoka, Saburo
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2015, 40 (34) : 11075 - 11086
  • [10] Effect of high-pressure hydrogen gas on fracture of austenitic steels
    Marchi, C. San
    Balch, D. K.
    Somerday, B. P.
    Proceedings of the ASME Pressure Vessels and Piping Conference 2005, Vol 6, 2005, 6 : 483 - 491