The effect of post-weld heat treatment affecting corrosion resistance and hydrogen embrittlement of HAZ part in FCAW

被引:22
|
作者
Moon, KM
Lee, MH
Kim, KJ
Kim, SJ
机构
[1] Nagoya Univ, Ctr Integrated Res Sci & Engn, Chikusa Ku, Nagoya, Aichi 4648603, Japan
[2] Korea Maritime Univ, Inst Corros & Corros Control, Pusan 606791, South Korea
来源
关键词
corrosion resistance; hydrogen embrittlement; post-weld heat treatment; slow strain rate test; quasi cleavage;
D O I
10.1016/S0257-8972(03)00060-4
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Evaluation of corrosion resistance of material surface was investigated with electrochemical factors, such as corrosion potential, corrosion current density with parameters of as-welded, post-weld heat treatment (PWHT) of 550, 600, 650 degreesC for a RE36 steel and mechanical properties such as elongation, hydrogen embrittlement and analysis of SEM fractography were also investigated with slow strain rate test (SSRT) method with applied constant cathodic potential in case of as-welded and PWHT of 550 degreesC. An optimum temperature for corrosion resistance improvement was apparently observed at 550 degreesC of PWHT and elongation was also increased with PWHT of 550 T than that of as-welded condition. Therefore, the susceptibility of hydrogen embrittlement was considered to be decreased with PWHT of 550 degreesC compared to that of as-welded condition and to be increased according to potential shifting in the low direction. (C) 2003 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:675 / 678
页数:4
相关论文
共 50 条
  • [1] The electrochemical study on mechanical and hydrogen embrittlement properties of HAZ part as a function of post-weld heat treatment in SMAW
    Kim, SJ
    Okido, M
    Moon, KM
    SURFACE & COATINGS TECHNOLOGY, 2003, 169 : 163 - 167
  • [2] Effect of Post-Weld Heat Treatment on the Corrosion Resistance of Super Austenitic Stainless Steel
    Kim, Yong-Seong
    Seo, Beom-Deok
    Choi, Kyu-Won
    Lee, Seung-Hyo
    Lee, Myeong-Hoon
    SCIENCE OF ADVANCED MATERIALS, 2022, 14 (07) : 1231 - 1241
  • [3] Effect of post-weld heat treatment on corrosion resistance of X90 pipeline steel joints
    Zhang, Defen
    Ran, Qingzheng
    Gong, Lijie
    Chen, Xiaowen
    Tang, Qiyuan
    Zeng, Dezhi
    INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2024, 115 (04) : 303 - 313
  • [4] Coupling effect of post-weld heat treatment and fatigue damage on the hydrogen embrittlement of X80 steel welded joints
    Gao, Zhiwei
    Wu, Shipin
    Xiang, Ting
    Gong, Baoming
    Deng, Caiyan
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 31 : 2646 - 2657
  • [5] EMBRITTLEMENT OF TYPE-316L AND TYPE-347 WELD OVERLAY BY POST-WELD HEAT-TREATMENT AND HYDROGEN
    TYSON, W
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1984, 15 (07): : 1475 - 1484
  • [6] Effect of post-weld heat treatment on the wear resistance of hardfacing martensitic steel deposits
    Gualco A.
    Svoboda H.G.
    Surian E.S.
    de Vedia L.A.
    Welding International, 2010, 24 (04) : 258 - 265
  • [7] Effect of Post-weld Heat Treatment on the Microstructure and Corrosion Resistance of Deposited Metal of a HighChromium Nickel-Based Alloy
    Xin-Jie Di
    Xiao-Qian Liu
    Cui-Xin Chen
    Bao-Sen Wang
    Xiao-Jiang Guo
    ActaMetallurgicaSinica(EnglishLetters), 2016, 29 (12) : 1136 - 1143
  • [8] Effect of Post-Weld Heat Treatment Temperatures on Microstructure, Intergranular Corrosion Resistance, and Mechanical Properties of 4130 Steel with Inconel 625 Weld Overlay
    Guo, Longlong
    Xiao, Fei
    Wang, Fan
    Wei, Zebing
    Zhang, Yong
    JOURNAL OF FAILURE ANALYSIS AND PREVENTION, 2021, 21 (05) : 1775 - 1783
  • [9] Effect of Post-Weld Heat Treatment Temperatures on Microstructure, Intergranular Corrosion Resistance, and Mechanical Properties of 4130 Steel with Inconel 625 Weld Overlay
    Longlong Guo
    Fei Xiao
    Fan Wang
    Zebing Wei
    Yong Zhang
    Journal of Failure Analysis and Prevention, 2021, 21 : 1775 - 1783
  • [10] Toughness recovery for weld HAZ by post weld heat treatment
    Okada, Hitoshi
    Matsuda, Fukuhisa
    Ikeuchi, Kenji
    Li, Zhonglin
    Yosetsu Gakkai Ronbunshu/Quarterly Journal of the Japan Welding Society, 1994, 12 (04): : 521 - 527