Effect of strain-paths on mechanical properties of hot rolled commercially pure titanium

被引:21
|
作者
Sahoo, S. K. [1 ]
Sabat, R. K. [2 ]
Bishoyi, B. D. [1 ]
Anjani, A. G. S. [1 ]
Suwas, S. [2 ]
机构
[1] NIT Rourkela, Dept Met & Mat Engn, Rourkela 769008, Odisha, India
[2] IISc Bangalore, Dept Mat Engn, Bangalore 560012, Karnataka, India
关键词
CP-titanium; Strain-paths; Stored energy; Microstructure; X-ray techniques; Deformation and fracture; TEXTURE; ANISOTROPY; MICROSTRUCTURE; EVOLUTION; SHEET;
D O I
10.1016/j.matlet.2016.05.162
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this paper, a fine distinction between the role of strain-paths on the evolution of mechanical properties has been reported. Commercially pure (CP) titanium plates were subjected to hot rolling of 90% reduction in thickness through different strain-paths such as unidirectional rolling (UDR), multistep cross-rolling (MSCR) and reverse-rolling (RR). It was observed that the sample rolled through RR had higher mechanical properties (both yield strength and ductility) followed by the samples rolled through MSCR and UDR respectively. It was further observed that the RR sample had higher stored energy followed by MSCR and UDR samples which eventually controls the evolution of microstructure and hence defines the mechanical properties. (C) 2016 Elsevier B.V. All rights reserved.
引用
收藏
页码:166 / 169
页数:4
相关论文
共 50 条
  • [1] Texture and microstructure evolution of commercially pure titanium during hot rolling: Role of strain-paths
    Sahoo, S. K.
    Sabat, R. K.
    Sahni, S.
    Suwas, S.
    MATERIALS & DESIGN, 2016, 91 : 58 - 71
  • [2] Mechanical Properties of Commercially Pure Titanium During Hot Compression
    Zhang, Yanshu
    Jin, Quanlin
    MANUFACTURING PROCESS TECHNOLOGY, PTS 1-5, 2011, 189-193 : 1799 - +
  • [3] Effect of annealing temperature on microstructure and mechanical properties of cold-rolled commercially pure titanium sheets
    Zhao, Shuai
    Wang, Yang
    Peng, Lin
    Zhang, Yuan-xiang
    Ran, Rong
    Yuan, Guo
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2022, 32 (08) : 2587 - 2597
  • [4] PREVENTION OF SURFACE WRINKLES IN COMMERCIALLY PURE TITANIUM HOT ROLLED SLABS
    HAYAKAWA, H
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1985, 71 : 1629 - 1629
  • [5] EFFECT OF LOW TEMPERATURES ON THE MECHANICAL PROPERTIES OF A COMMERCIALLY PURE TITANIUM
    GEIL, GW
    CARWILE, NL
    JOURNAL OF RESEARCH OF THE NATIONAL BUREAU OF STANDARDS, 1955, 54 (02): : 91 - 101
  • [6] Effect of Orientation and Temperature on the Mechanical Properties of Commercially Pure Titanium
    Battaini, M.
    Pereloma, E. V.
    Davies, C. H. J.
    THERMEC 2006 SUPPLEMENT: 5TH INTERNATIONAL CONFERENCE ON PROCESSING AND MANUFACTURING OF ADVANCED MATERIALS, 2007, 15-17 : 941 - 946
  • [7] Effect of grain size on mechanical properties of commercially pure titanium
    Salishchev G.A.
    Mironov S.Yu.
    Russian Physics Journal, 2001, 44 (6) : 596 - 601
  • [8] Orientation Effect on Mechanical Properties of Commercially Pure Titanium at Room Temperature
    M. Battaini
    E.V. Pereloma
    C.H.J. Davies
    Metallurgical and Materials Transactions A, 2007, 38 : 276 - 285
  • [9] Orientation effect on mechanical properties of commercially pure titanium at room temperature
    Battaini, M.
    Pereloma, E. V.
    Davies, C. H. J.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2007, 38A (02): : 276 - 285
  • [10] Mechanical properties and deformation mechanisms of a commercially pure titanium
    Nemat-Nasser, S
    Guo, WG
    Cheng, JY
    ACTA MATERIALIA, 1999, 47 (13) : 3705 - 3720