Heat-affected zone crack healing in IN939 repaired joints using hot isostatic pressing

被引:7
|
作者
Xie, Jilin [1 ,2 ]
Ma, Yingche [1 ]
Xing, Weiwei [1 ]
Zhang, Long [1 ]
Ou, Meiqiong [1 ,2 ]
Liu, Kui [1 ]
机构
[1] Chinese Acad Sci, Inst Met Res, Shenyang, Liaoning, Peoples R China
[2] Univ Sci & Technol China, Sch Mat Sci & Engn, Hefei, Anhui, Peoples R China
关键词
IN; 939; superalloy; Microstructure; HAZ cracks; HIP; Crack healing; INCONEL 738LC SUPERALLOY; NICKEL-BASED SUPERALLOY; HAZ CRACKING; WELD; MICROSTRUCTURES; LIQUATION; ALLOYS;
D O I
10.1007/s40194-018-0579-5
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Simulation defects in IN 939 superalloy were repaired by gas tungsten arc welding (GTAW) using Nimonic C263 as filler metal. The microstructures and chemical compositions of fusion zone under the condition of as-welded and post-weld heat treatment (PWHT) were investigated by optical microscopy (OM), scanning electron microscopy (SEM), transmission electron microscopy (TEM), and electron probe X-ray microanalysis (EPMA). Moreover, the liquation cracking and strain age cracking in heat-affected zone (HAZ) were characterized as well. Post-weld hot isostatic pressing (HIP) was also applied to heal the HAZ cracks. The results show that elements segregation at as-welded joints could be significantly reduced by PWHT. HAZ cracks consisted of liquation cracking and strain age cracking. The liquation cracking was shorter than the strain age cracking. HIP is an effective way to heal the cracks in the repaired joints especially for liquation cracking. Though the strain age cracking can be healed by HIP. the healed trace concentrated with Al, Ti, B, and Zr elements can still be detected. Post-weld HIP is a necessary process to obtain crack-fire joints.
引用
收藏
页码:471 / 479
页数:9
相关论文
共 50 条
  • [1] Heat-affected zone crack healing in IN939 repaired joints using hot isostatic pressing
    Jilin Xie
    Yingche Ma
    Weiwei Xing
    Long Zhang
    Meiqiong Ou
    Kui Liu
    Welding in the World, 2018, 62 : 471 - 479
  • [2] Liquation cracking in the heat-affected zone of IN939 superalloy tungsten inert gas weldments
    Hassan Kazempour-Liasi
    Mohammad Tajally
    Hassan Abdollah-Pour
    International Journal of Minerals,Metallurgy and Materials, 2020, 27 (06) : 764 - 773
  • [3] Liquation cracking in the heat-affected zone of IN939 superalloy tungsten inert gas weldments
    Hassan Kazempour-Liasi
    Mohammad Tajally
    Hassan Abdollah-Pour
    International Journal of Minerals, Metallurgy and Materials, 2020, 27 : 764 - 773
  • [4] Liquation cracking in the heat-affected zone of IN939 superalloy tungsten inert gas weldments
    Kazempour-Liasi, Hassan
    Tajally, Mohammad
    Abdollah-Pour, Hassan
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2020, 27 (06) : 764 - 773
  • [5] The relationship of crack resistance and structure of a heat-affected zone of welded pipe joints
    Zueva, Svetlana N.
    Soya, Sergey V.
    Zadubrovskaya, Olga A.
    NAUKA I TEHNOLOGII TRUBOPROVODNOGO TRANSPORTA NEFTI I NEFTEPRODUKTOV-SCIENCE & TECHNOLOGIES-OIL AND OIL PRODUCTS PIPELINE TRANSPORTATION, 2018, 8 (02): : 154 - 160
  • [6] TOUGHNESS OF THE HEAT-AFFECTED ZONE IN WELDED-JOINTS
    DEGENKOLBE, J
    KAISER, HJ
    UWER, D
    STAHL UND EISEN, 1989, 109 (18): : 853 - 858
  • [7] TESTS FOR INVESTIGATING THE HOT EMBRITTLEMENT IN THE HEAT-AFFECTED ZONE OF WELDED-JOINTS OF AUSTENITIC STEELS
    DETERT, K
    KANBACH, H
    POHL, M
    SCHMIDTMANN, E
    ARCHIV FUR DAS EISENHUTTENWESEN, 1982, 53 (06): : 239 - 244
  • [8] Determining structural inhomogeneities in the heat-affected zone of welded joints
    Paetzold, Uwe
    Hou, Chun-Xiao
    Ruge, Juergen
    Schweissen und Schneiden/Welding and Cutting, 1989, (03):
  • [9] Crack arrest toughness of a heat-affected zone containing zones
    J Offshore Mech Arct Eng, Trans ASME, 4 (292-299):
  • [10] Effect of Preweld Heat Treatment on the Microstructure of Heat-Affected Zone (HAZ) and Weldability of Inconel 939 Superalloy
    Gonzalez Albarran, M. A.
    Martinez, D. I.
    Diaz, E.
    Diaz, J. C.
    Guzman, I.
    Saucedo, E.
    Guzman, A. Ma.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2014, 23 (04) : 1125 - 1130