Deformation Behavior of Polyurethane Adhesive in the Single-Lap Joint Based on the Microbeam X-ray Scattering Method

被引:6
|
作者
Obayashi, Kakeru [3 ]
Kamitani, Kazutaka [4 ]
Chu, Chien-Wei [4 ]
Kawatoko, Ryosuke [3 ]
Cheng, Chao-Hung [3 ]
Takahara, Atsushi [3 ,5 ]
Kojio, Ken [1 ,2 ]
机构
[1] Kyushu Univ, Inst Mat Chem & Engn, Int Inst Carbon Neutral Energy Res WPI I2CNER, Grad Sch Engn,Res Ctr Negat Emiss Technol, Fukuoka, 8190395, Japan
[2] Kyushu Univ, Ctr Polymer Interface & Mol Adhes Sci, Fukuoka, 8190395, Japan
[3] Kyushu Univ, Grad Sch Engineerin g, Fukuoka, 8190395, Japan
[4] Kyushu Univ, Inst Mat Chem & Engn, Fukuoka, 8190395, Japan
[5] Kyushu Univ, Res Ctr Negat Emiss Technol, Fukuoka, 8190395, Japan
关键词
polyurethane; adhesive; microphase-separated structure; small-angle X-ray scattering (SAXS); wide-angle X-ray scattering (WAXS); SIMPLE SHEAR DEFORMATION; SEGMENTED POLYURETHANE; THERMOPLASTIC POLYURETHANES; MECHANICAL-PROPERTIES; AGGREGATION STRUCTURE; IN-SITU; STRAIN; DIFFRACTION; POLYPROPYLENE; ELASTOMERS;
D O I
10.1021/acsapm.2c00436
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Single-lap joint (SLJ) specimens were prepared using two stainless steel substrates as adherends and polyurethanes (PU) as an adhesive and then employed for adhesion testing. To investigate the internal structure of the PU adhesive during the shear deformation process, the in situ synchrotron radiation microbeam small-angle and wide-angle X-ray scattering (SAXS and WAXS) measurements were carried out. A lab-made portable tensile tester was developed for the SAXS/WAXS measurement during lap shear deformation. The structure of adhesive bulk was also investigated during the simple uniaxial deformation for the comparison. An isotropic scattering ring-which was formed from the periodic structure of hard segment domains of the PU adhesive-was clearly observed in the SAXS pattern at the initial state. This isotropic ring changed to an ellipsoid shape whose minor and major axes were tilted from the stretching direction. The spacing of the hard segment domains of PU adhesives increased, and the tilt angle of the stress direction was merged with the stretching direction with an increase in the applied deformation. The orientation direction of the hard segment domains and molecular chain of the soft segment changed with a similar trend. Furthermore, the degree of change in these values was larger at the edge of the adhesive of the SLJ specimens, indicating the existence of spatial distribution of direction and the value of stress in the adhesive during lap shear deformation. These findings are expected to be quite useful for practical design of adhesives.
引用
收藏
页码:5387 / 5394
页数:8
相关论文
共 50 条
  • [1] FEA of Stress behavior in the Single-lap Adhesive Joint
    He, Xiaocong
    ADVANCED MATERIALS AND COMPUTER SCIENCE, PTS 1-3, 2011, 474-476 : 807 - 810
  • [2] Impact of joint variables on shear and fatigue behavior of composite-metal single-lap adhesive joint
    Kumar, Vivek
    Sharma, Saurabh
    Singh, Akhilendra
    ENGINEERING FAILURE ANALYSIS, 2025, 168
  • [3] Static compression testing CFRP single-lap composited joints using X-ray μCT
    Zhang, Hongzhuang
    Li, Changyou
    Dai, Weibing
    Liu, Yuzhuo
    Tian, Sen
    Huang, Wenchao
    Jia, Dawei
    He, David
    Zhang, Yimin
    COMPOSITE STRUCTURES, 2020, 234
  • [4] Exploring the impact of graphene nanoplatelets on adhesive mechanical strength: A comprehensive investigation into single-lap joint elastoplastic behavior via cohesive zone method
    Abdalla, Amer Murtada Amer
    Elmoghazy, Yasser Hamed
    Sarkon, Garshasp Keyvan
    Gazioglu, Aysegul
    Sabry, Omar Khaled
    Sawelih, Abdulrahman Awad
    Al Sharif, Anas
    Wehbi, Hicham
    Abd, Asem Yahya Ali
    Sahmani, Saeid
    Safaei, Babak
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2025, 138
  • [5] Experimental Study on the Effect of Bonding Area Dimensions on the Mechanical Behavior of Composite Single-Lap Joint with Epoxy and Polyurethane Adhesives
    Abbasi, Mohammad
    Ciardiello, Raffaele
    Goglio, Luca
    APPLIED SCIENCES-BASEL, 2023, 13 (13):
  • [6] X-ray based defect testing method for a lap joint with unequal thickness steel plates
    Chi D.
    Ma Z.
    Cheng Y.
    Wang Z.
    Hanjie Xuebao/Transactions of the China Welding Institution, 2019, 40 (11): : 45 - 48
  • [7] Effect of carbon filler–modified epoxy adhesive on failure behavior of bonded single-lap joint: an experimental study combined with digital image correlation method
    Özkan Öz
    Fatih Huzeyfe Öztürk
    Welding in the World, 2022, 66 : 2143 - 2156
  • [8] INVERSION ANALYSIS FOR INTERFACIAL STRESS OF COMPOSITE SINGLE-LAP JOINT BASED ON FULL-FIELD DEFORMATION AND FEM
    Bai, R. X.
    Bao, S. H.
    Lei, Z. K.
    Yan, C.
    ICCM 21: 21ST INTERNATIONAL CONFERENCE ON COMPOSITE MATERIALS (ICCM-21), 2017,
  • [9] Progressive failure analysis of bolted single-lap composite joint based on extended finite element method
    Wang, Zhenqing
    Zhou, Song
    Zhang, Jifeng
    Wu, Xiaodi
    Zhou, Limin
    MATERIALS & DESIGN, 2012, 37 : 582 - 588
  • [10] Effect of carbon filler-modified epoxy adhesive on failure behavior of bonded single-lap joint: an experimental study combined with digital image correlation method
    Oz, Ozkan
    Ozturk, Fatih Huzeyfe
    WELDING IN THE WORLD, 2022, 66 (10) : 2143 - 2156