Corrosion behavior of niobium, tantalum and their alloys in boiling sulfuric acid solutions

被引:41
|
作者
Robin, A [1 ]
机构
[1] Polo Urbo Ind, Dept Engn Mat FAENQUIL, BR-12600000 Lorena, SP, Brazil
关键词
D O I
10.1016/S0263-4368(97)87506-3
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The corrosion resistance of niobium, tantalum and Nb-20, 40, 60 and 80 wt% Ta alloys in boiling 20, 40, 60 and 80 wt% H2SO4 solutions is studied using the mass-loss technique. The corrosion rates of all materials increase with acid concentration and diminish initially with time. After nearly 200 h, the corrosion rates stabilize due to superficial oxide formation. The corrosion resistance increases with tantalum content. A preferential dissolution of niobium from the Nb-Ta alloys is noted. Recrystallization heat treatments reduce slightly the corrosion rates. The anodized materials are more corrosion resistant than the untreated ones during the first 200 h, but behave similarly for longer exposure times. (C) 1997 Elsevier Science Ltd.
引用
收藏
页码:317 / 323
页数:7
相关论文
共 50 条