Manufacturing process and microstructure of copper-coated aluminum wires

被引:5
|
作者
Chen, Xiao-hua [1 ,2 ]
Tang, Xin [3 ]
Wang, Zi-dong [3 ]
Hui, Xi-dong [1 ]
Li, Mo [2 ]
Wang, Yong-wei [4 ]
机构
[1] Univ Sci & Technol Beijing, State Key Lab Adv Met & Mat, Beijing 100083, Peoples R China
[2] Georgia Inst Technol, Sch Mat Sci & Engn, Atlanta, GA 30312 USA
[3] Univ Sci & Technol Beijing, Sch Mat Sci & Engn, Beijing 100083, Peoples R China
[4] Univ Sci & Technol, Sch Mech Engn, Beijing 100083, Peoples R China
基金
高等学校博士学科点专项科研基金;
关键词
bimetallic; composites; copper; aluminum; hot dip coating; interfaces; EXTRUSION PROCESS; STEEL; CONDUCTORS; FIELD;
D O I
10.1007/s12613-015-1060-8
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Copper-coated aluminum wires exhibit good electrical conductivity, high thermal conductivity, low contact resistance of copper and low density, and provide economic advantages over aluminum. However, there are some problems in the manufacturing processes of hot-dip copper-coated aluminum wires, such as the difficulties in controlling coating process. In this work, the hot-dip copper-coating method of aluminum wires was investigated for producing copper-coated aluminum wire composites. The interface microstructure between the aluminum wire and the copper coating layer was analyzed by scanning electron microscopy (SEM) and energy-dispersive X-ray spectrometry (EDS). Five different fluxing agents were tested. Experimental results show that appropriate conditions for the hot-dip process are determined as the liquid copper temperature of 1085A degrees C and the treatment time less than 1 s. A success in hot-dip copper-coated aluminum wires is achieved by hot-dipping a low-melting-point metal into a high-melting-point metal liquid, which is significant for the further development and application of copper-coated aluminum wire composites.
引用
收藏
页码:190 / 196
页数:7
相关论文
共 50 条
  • [1] Manufacturing process and microstructure of copper-coated aluminum wires
    Xiao-hua Chen
    Xin Tang
    Zi-dong Wang
    Xi-dong Hui
    Mo Li
    Yong-wei Wang
    International Journal of Minerals, Metallurgy, and Materials, 2015, 22 : 190 - 196
  • [2] Manufacturing process and microstructure of copper-coated aluminum wires
    Xiao-hua Chen
    Xin Tang
    Zi-dong Wang
    Xi-dong Hui
    Mo Li
    Yong-wei Wang
    International Journal of Minerals Metallurgy and Materials, 2015, 22 (02) : 190 - 196
  • [3] STUDIES OF DUPLEX (COPPER-COATED) WIRES FOR USE IN INTRAUTERINE-DEVICES
    SIKOV, MR
    DIVINE, JR
    HACKETT, PL
    CONTRACEPTION, 1976, 13 (01) : 55 - 63
  • [4] Wettability and spreading kinetics of molten aluminum on copper-coated ceramics
    C. A. León
    G. Mendoza-Suarez
    R A. L. Drew
    Journal of Materials Science, 2006, 41 : 5081 - 5087
  • [5] Fabrication of aluminum foam stabilized by copper-coated carbon fibers
    Cao, Zhuo-Kun
    Li, Bing
    Yao, Guang-Chun
    Wang, Yong
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 486 (1-2): : 350 - 356
  • [6] Electrodeposition of Aluminum onto Copper-Coated Printed Circuit Boards
    Xu, Min
    Yue, Guikuan
    Bizzotto, Dan
    Asselin, Edouard
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2017, 164 (12) : D729 - D736
  • [7] Wettability and spreading kinetics of molten aluminum on copper-coated ceramics
    Leon, C. A.
    Mendoza-Suarez, G.
    Drew, R. A. L.
    JOURNAL OF MATERIALS SCIENCE, 2006, 41 (16) : 5081 - 5087
  • [8] THE DRAWING PROCESS OF THE WIRES OF COPPER AND ALUMINUM: EVOLUTION OF THE MICROSTRUCTURE AND (MECHANICAL/ELECTRICAL) PROPERTIES
    Zidani, M.
    Hadid, M. D.
    Messaoudi, S.
    Dendouga, F.
    Bessais, L.
    Baira, F.
    Bayarassou, M.
    Helbert, A. L.
    Mathon, M. H.
    Baudin, T.
    METAL 2014: 23RD INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS, 2014, : 442 - 446
  • [9] Structure feature characterization of aluminum foam reinforced by copper-coated carbon fibers
    Du J.
    Wang B.
    Cao Z.
    Yao G.
    Liang L.
    Cailiao Daobao/Materials Review, 2016, 30 (03): : 82 - 85and115
  • [10] Absorption loss at high temperatures in aluminum- and copper-coated optical fibers
    V. V. Voloshin
    I. L. Vorob’ev
    G. A. Ivanov
    V. A. Isaev
    A. O. Kolosovskii
    B. Lenardich
    S. M. Popov
    Yu. K. Chamorovskii
    Journal of Communications Technology and Electronics, 2011, 56 : 90 - 96