Friction and wear mechanisms in MoS2/Sb2O3/Au nanocomposite coatings

被引:171
|
作者
Scharf, T. W. [1 ]
Kotula, P. G. [1 ]
Prasad, S. V. [1 ]
机构
[1] Sandia Natl Labs, Ctr Mat Sci & Engn, Albuquerque, NM 87185 USA
关键词
Coatings; Thin films; Nanocomposites; Wear; Friction; SOLID LUBRICANT COATINGS; DEPOSITED MOS2 FILMS; ABSORPTION FINE-STRUCTURE; TUNGSTEN DISULFIDE FILMS; THIN-FILMS; TRIBOLOGICAL PERFORMANCE; DUCTILE MATERIALS; BEHAVIOR; METAL; MICROSTRUCTURE;
D O I
10.1016/j.actamat.2010.03.040
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Fundamental phenomena governing the tribological mechanisms in sputter deposited amorphous MoS2/Sb2O3/Au nanocomposite coatings are reported. In dry environments the nanocomposite has the same low friction coefficient as pure MoS2 (similar to 0.007). However, unlike pure MoS2 coatings, which wear through in air (50% relative humidity), the composite coatings showed minimal wear, with wear factors of similar to 1.2-1.4 x 10(-7) mm(3) Nm(-1) in both dry nitrogen and air. The coatings exhibited non-Amontonian friction behavior, with the friction coefficient decreasing with increasing Hertzian contact stress. Cross-sectional transmission electron microscopy of wear surfaces revealed that frictional contact resulted in an amorphous to crystalline transformation in MoS2 with 2H-basal (0 0 0 2) planes aligned parallel to the direction of sliding. In air the wear surface and subsurface regions exhibited islands of Au. The mating transfer films were also comprised of (0 0 0 2)-oriented basal planes of MoS2, resulting in predominantly self-mated "basal on basal" interfacial sliding and, thus, low friction and wear. (C) 2010 Published by Elsevier Ltd. on behalf of Acta Materialia Inc.
引用
收藏
页码:4100 / 4109
页数:10
相关论文
共 50 条
  • [1] Temperature-Dependent Friction and Wear of MoS2/Sb2O3/Au Nanocomposites
    J. F. Curry
    T. F. Babuska
    M. T. Brumbach
    N. Argibay
    Tribology Letters, 2016, 64
  • [2] Temperature-Dependent Friction and Wear of MoS2/Sb2O3/Au Nanocomposites
    Curry, J. F.
    Babuska, T. F.
    Brumbach, M. T.
    Argibay, N.
    TRIBOLOGY LETTERS, 2016, 64 (01)
  • [3] An atom probe tomography investigation of Ti–MoS2 and MoS2–Sb2O3–Au films
    Harpal Singh
    Kalyan C. Mutyala
    Ryan D. Evans
    Gary L. Doll
    Journal of Materials Research, 2017, 32 : 1710 - 1717
  • [4] TRIBOLOGICAL PERFORMANCE OF MOS2 COMPACTS CONTAINING MOO3, SB2O3 OR MOO3 AND SB2O3
    CENTERS, PW
    WEAR, 1988, 122 (01) : 97 - 102
  • [5] The Anti-Oxidation Properties of MoS2/Sb2O3 Films
    Zhang, Yanshuai
    Zhou, Hui
    Wan, Zhihua
    Zheng, Jun
    Sang, Ruipeng
    Yang, Lamaocao
    MATERIALS PROCESSING TECHNOLOGY II, PTS 1-4, 2012, 538-541 : 136 - 140
  • [6] Microtribological performance of Au-MoS2 nanocomposite and Au/MoS2 bilayer coatings
    Stoyanov, Pantcho
    Gupta, Shivani
    Chromik, Richard R.
    Lince, Jeffrey R.
    TRIBOLOGY INTERNATIONAL, 2012, 52 : 144 - 152
  • [7] Environmental Effects on the Tribology and Microstructure of MoS2–Sb2O3–C Films
    Gregory J. Dudder
    Xueying Zhao
    Brandon Krick
    W. Gregory Sawyer
    Scott S. Perry
    Tribology Letters, 2011, 42 : 203 - 213
  • [8] Microstructure and lubrication mechanism of multilayered MoS2/Sb2O3 thin films
    J.J. Hu
    J.E. Bultman
    J.S. Zabinski
    Tribology Letters, 2006, 21 : 169 - 174
  • [9] Microstructure and lubrication mechanism of multilayered MoS2/Sb2O3 thin films
    Hu, J. J.
    Bultman, J. E.
    Zabinski, J. S.
    TRIBOLOGY LETTERS, 2006, 21 (02) : 169 - 174
  • [10] 掺杂Sb2O3/Au对MoS2溅射膜抗氧化性能的影响
    陈焘
    郭等柱
    万志华
    白芝芳
    真空与低温, 2000, (04) : 11 - 16