Dry sliding wear behaviour of metal toughened nanoceramics: A case study of aluminium-alumina nanocermets

被引:1
|
作者
Sharma, Nidhi [1 ]
Biswas, Krishanu [1 ]
Jha, Shikhar Krishn [1 ]
机构
[1] Indian Inst Technol Kanpur, Dept Mat Sci & Engn, Kanpur 208016, Uttar Pradesh, India
关键词
Nanocermets; Abrasive wear; Adhesive wear; Delamination; Optical profilometry; COMPOSITES; AL2O3; MICROSTRUCTURE; PERFORMANCE; MECHANISM; FRICTION;
D O I
10.1016/j.wear.2022.204389
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Sliding wear experiments were performed on the set of six Al-Al2O3 nanocermets, which were optimally designed with a tuned volumetric concentration of 20% Al and 80% Al2O3 to achieve a tailored cocooning of Al2O3 particles with thin Al film in the cermet structure. A combination of cryo-milling and room temperature ball milling was carried out to prepare Al-0.2-(Al2O3 )(0.8) powder mixtures and the nanocermets were prepared by spark plasma sintering (SPS). Pure Al, Al2O3 and nanocermet samples were subjected to a dry sliding wear test against a steel counter-body with the contact diameter of 1 mm to estimate their relative wear behaviour. The results suggest that the wear behaviour of nanocermets is comprised of both abrasive and adhesive losses. An increase in the milling duration of powder mixtures improved the wear resistance of the sintered nanocermets. Abrasion, adhesion, fracture, delamination and ploughing were found to be the major material removal mechanisms from the wear tracks. SEM was utilized to understand the morphological features of the wear tracks and wear debris, while XRD was used for the phase evaluation of the samples. HRTEM was used to observe the distribution of phases in the sintered nanocermet structure.
引用
收藏
页数:11
相关论文
共 50 条
  • [1] Dry sliding wear behaviour of aluminium/alumina/graphite hybrid metal matrix composites
    Radhika, N.
    Subramanian, R.
    Prasat, S. Venkat
    Anandavel, B.
    INDUSTRIAL LUBRICATION AND TRIBOLOGY, 2012, 64 (06) : 359 - 366
  • [2] Influence of alumina percentage on microstructure, mechanical and wear behaviour of 2014 aluminium-alumina metal matrix composites
    Bharath, V
    Auradi, V
    Nagaral, Madeva
    Boppana, Satish Babu
    JURNAL TRIBOLOGI, 2020, 25 : 29 - 44
  • [3] Dry sliding wear of zirconia-toughened alumina with different metal oxide additives
    Dey, Ashis Kumar
    Biswas, Koushik
    CERAMICS INTERNATIONAL, 2009, 35 (03) : 997 - 1002
  • [4] Comparison study on dry and wet sliding wear behaviour of aluminium/nano composites
    Jayapragash, A.
    Solamannan, G. G.
    Guganeswaran, I
    3RD INTERNATIONAL CONFERENCE ON ADVANCES IN MECHANICAL ENGINEERING (ICAME 2020), PTS 1-6, 2020, 912
  • [5] Dry Sliding Wear Behaviour of Basalt Short Fiber Reinforced Aluminium Metal Matrix Composites
    Vannan, S. Ezhil
    Vizhian, S. Paul
    DYNAMICS OF MACHINES AND MECHANISMS, INDUSTRIAL RESEARCH, 2014, 592-594 : 1285 - 1290
  • [6] Wear behaviour of graphitic aluminium composite sliding under dry conditions
    Mohan, S
    Pathak, JP
    Gupta, RC
    Srivastava, S
    ZEITSCHRIFT FUR METALLKUNDE, 2002, 93 (12): : 1245 - 1251
  • [7] Wear behaviour of graphitic aluminium composite sliding under dry conditions
    Mohan, S.
    Pathak, J.P.
    Gupta, R.C.
    Srivastava, S.
    International Journal of Materials Research, 2002, 93 (12) : 1245 - 1251
  • [8] THE DRY SLIDING WEAR OF CENOSPHERE-ALUMINIUM METAL MATRIX COMPOSITE
    Saravanan, V.
    Thyla, P. R.
    Balakrishnan, S. R.
    ADVANCED COMPOSITES LETTERS, 2014, 23 (03) : 49 - 58
  • [9] Dry sliding wear behaviour of an aluminium alloy-granite particle composite
    Singh, M
    Prasad, BK
    Mondal, DP
    Jha, AK
    TRIBOLOGY INTERNATIONAL, 2001, 34 (08) : 557 - 567
  • [10] DRY SLIDING WEAR BEHAVIOUR OF CARBON NANOTUBE/ALUMINA/EPOXY HYBRID NANOCOMPOSITES
    Ramkumar, R.
    Sabarinathan, C.
    Rajeswaran, M.
    Prathap, P.
    Ganesh, R. Sankar
    MATERIALI IN TEHNOLOGIJE, 2024, 58 (03):