Wood Plastic Composite Produced by Nonmetals from Pulverized Waste Printed Circuit Boards

被引:68
|
作者
Guo, Jie [1 ]
Tang, Yinen [1 ]
Xu, Zhenming [1 ]
机构
[1] Shanghai Jiao Tong Univ, Sch Environm Sci & Engn, Shanghai 200240, Peoples R China
基金
国家高技术研究发展计划(863计划);
关键词
RECOVERY;
D O I
10.1021/es902889b
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
Nonmetals reclaimed from waste printed circuit boards (PCBs) are used to replace wood flour in the production of wood plastic composite (WPC). To evaluate property durability against weather exposure, the effects of accelerated aging process on the properties of WPC are investigated. The results show that filling of nonmetals in WPC improves the flexural strength and tensile strength, and reduces screw withdrawal strength. Before hollow WPC with 15% nonmetals (H-15-WPC) underwent aging process, H-15-WPC had a flexural strength of 25.8 MPa, a tensile strength of 9.8 MPa, a charpy impact strength of 3.4 kJ/m(2), and face/edge screw withdrawal strength of 121/115 N/mm. It is found that flexural strength of H-15-WPC decreases linearly with the increase of accelerated aging cycles, and the effects of aging test on tensile and impact strength of H-15-WPC are minor. For solid WPC,the accelerated aging test decreases screw withdrawal strength slightly. All the results indicate that nonmetals of waste PCBs can be reused as an alternative for wood flour in WPC products rather than resorting to their landfill or combustion.
引用
收藏
页码:463 / 468
页数:6
相关论文
共 50 条
  • [1] Performance and thermal behavior of wood plastic composite produced by nonmetals of pulverized waste printed circuit boards
    Guo, Jie
    Tang, Yinen
    Xu, Zhenming
    [J]. JOURNAL OF HAZARDOUS MATERIALS, 2010, 179 (1-3) : 203 - 207
  • [2] Asphalt Modified with Nonmetals Separated from Pulverized Waste Printed Circuit Boards
    Guo, Jiuyong
    Guo, Jie
    Wang, Shifeng
    Xu, Zhenming
    [J]. ENVIRONMENTAL SCIENCE & TECHNOLOGY, 2009, 43 (02) : 503 - 508
  • [3] A plate produced by nonmetallic materials of pulverized waste printed circuit boards
    Guo, Jie
    Cao, Bin
    Guo, Jiuyong
    Xu, Zhenming
    [J]. ENVIRONMENTAL SCIENCE & TECHNOLOGY, 2008, 42 (14) : 5267 - 5271
  • [4] New solutions for reusing nonmetals reclaimed from waste printed circuit boards
    Mou, P
    Xiang, D
    Pan, XY
    Wa, LD
    Gao, JG
    Duan, GH
    [J]. 2005 IEEE INTERNATIONAL SYMPOSIUM ON ELECTRONICS & THE ENVIRONMENT, CONFERENCE RECORD, 2005, : 205 - 209
  • [5] Completely separating metals and nonmetals from waste printed circuit boards by slurry electrolysis
    Yang, Deze
    Chu, Yingying
    Wang, Jianbo
    Chen, Mengjun
    Shu, Jiancheng
    Xiu, Furong
    Xu, Zhonghui
    Sun, Shuhui
    Chen, Shu
    [J]. SEPARATION AND PURIFICATION TECHNOLOGY, 2018, 205 : 302 - 307
  • [6] Recovery of Metals and Nonmetals from Waste Printed Circuit Boards (PCBs) by Physical Recycling Techniques
    Kaya, Muammer
    [J]. ENERGY TECHNOLOGY 2017: CARBON DIOXIDE MANAGEMENT AND OTHER TECHNOLOGIES, 2017, : 433 - 451
  • [7] The reuse of nonmetals recycled from waste printed circuit boards as reinforcing fillers in the polypropylene composites
    Zheng, Yanhong
    Shen, Zhigang
    Cai, Chujiang
    Ma, Shulin
    Xing, Yushan
    [J]. JOURNAL OF HAZARDOUS MATERIALS, 2009, 163 (2-3) : 600 - 606
  • [8] Production of sustainable wood-plastic composites from the nonmetals in waste printed circuit boards: Excellent physical performance achieved by solid-state shear milling
    Yang, Shuangqiao
    Jiang, Jun
    Duan, Wenfeng
    Bai, Shibing
    Wang, Qi
    [J]. COMPOSITES SCIENCE AND TECHNOLOGY, 2020, 200
  • [9] Influence of nonmetals recycled from waste printed circuit boards on flexural properties and fracture behavior of polypropylene composites
    Zheng, Yanhong
    Shen, Zhigang
    Cai, Chujiang
    Ma, Shulin
    Xing, Yushan
    [J]. MATERIALS & DESIGN, 2009, 30 (04) : 958 - 963
  • [10] Application of glass-nonmetals of waste printed circuit boards to produce phenolic moulding compound
    Guo, Jie
    Rao, Qunli
    Xu, Zhenming
    [J]. JOURNAL OF HAZARDOUS MATERIALS, 2008, 153 (1-2) : 728 - 734