Composition and mechanical properties of hard ceramic coating containing α-Al2O3 produced by microarc oxidation on Ti-6Al-4V alloy

被引:94
|
作者
Sun, XT [1 ]
Jiang, ZH [1 ]
Xin, SG [1 ]
Yao, ZP [1 ]
机构
[1] Harbin Inst Technol, Dept Appl Chem, Harbin 150001, Peoples R China
基金
中国国家自然科学基金;
关键词
microarc oxidation; phase composition; titanium alloy; coating;
D O I
10.1016/j.tsf.2004.06.096
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Ceramic coatings with 1100-1600 HK50 (g) hardness were deposited on Ti-6Al-4V alloy substrates using a microarc oxidation (MAO) technique, based on a dielectric barrier discharge created during anodic oxidation in an aqueous electrolyte. The influences of electrolyte concentration, deposition time and the cathodic to anodic current ratio Ic/Ia on phase composition and mechanical properties of the coatings have been studied using X-ray diffraction (XRD), scanning electron microscopy (SEM) and electron probe microanalysis methods (EPMA), as well as microhardness measurement, direct pull-off and impact tests. The results show alpha-Al2O3 phase, which greatly improved the hardness of the coatings, can be obtained at high concentration of NaAlO2 and its relative content increases with decreasing Ic/Ia ratio. The direct pull-off test and impact test results indicate that the films have the excellent adhesion with the substrate. (C) 2004 Elsevier B.V. All rights reserved.
引用
收藏
页码:194 / 199
页数:6
相关论文
共 50 条
  • [1] Microstructure of ceramic coating formed by microarc oxidation in silicate solution on Ti-6Al-4V alloy
    Xue, Wenbin
    Deng, Zhiwei
    Chen, Ruyi
    Zhang, Tonghe
    Gongye Jianzhu/Industrial Construction, 2000, 30 (02): : 5 - 7
  • [2] Structure and properties characterization of ceramic coatings produced on Ti-6Al-4V alloy by microarc oxidation in aluminate solution
    Xue, WB
    Wang, C
    Chen, RY
    Deng, ZW
    MATERIALS LETTERS, 2002, 52 (06) : 435 - 441
  • [3] Tribological Behavior of Microarc Oxidation Ceramic Coating on Ti6Al4V Alloy Surfaces
    Chen Fei
    Zhou Hai
    Xia Yangjian
    RARE METAL MATERIALS AND ENGINEERING, 2008, 37 : 70 - 73
  • [4] Effects of acidic electrolyte on microarc oxidation of Ti-6Al-4V alloy
    School of Materials Science and Engineering, Hefei University of Technology, Hefei 230009, China
    Cailiao Rechuli Xuebao, 2009, 1 (135-139):
  • [5] Microstructure and elevated temperature tribological behavior of TiO2/Al2O3 composite ceramic coating formed by microarc oxidation of Ti6Al4V alloy
    Wang, Shuaixing
    Zhao, Qing
    Liu, Daoxin
    Du, Nan
    SURFACE & COATINGS TECHNOLOGY, 2015, 272 : 343 - 349
  • [6] MECHANICAL PROPERTIES AND HIGH TEMPERATURE OXIDATION BEHAVIOR OF Ti-Al COATING REINFORCED BY NITRIDES ON Ti-6Al-4V ALLOY
    Dai, Jingjie
    Yu, Huijun
    Zhu, Jiyun
    Weng, Fei
    Chen, Chuanzhong
    SURFACE REVIEW AND LETTERS, 2016, 23 (05)
  • [7] Microstructure and properties of Al2O3/CuSnTi+B/Ti-6Al-4V alloy joint
    He, P. (hithepeng@hit.edu.cn), 1600, Chinese Ceramic Society (40):
  • [8] Influence of electrolytes on the microstructure of microarc oxidation coatings on Ti-6Al-4V alloy
    Xue, WB
    Wang, C
    Deng, ZW
    Chen, RY
    Zhang, TH
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2002, 18 (01) : 37 - 39
  • [9] Growth kinetics and mechanism of microarc oxidation coating on Ti-6Al-4V alloy in phosphate/silicate electrolyte
    Zhai, Dajun
    Qiu, Tao
    Shen, Jun
    Feng, Keqin
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2022, 29 (11) : 1991 - 1999