Influence of cold rolling reduction on the grain boundary character distribution and secondary recrystallization in nitrided Fe 3% Si alloy

被引:12
|
作者
Harase, J [1 ]
Shimizu, R [1 ]
机构
[1] Pohang Univ Sci & Technol, Grad Sch Iron & Steel Technol, Pohang 790784, Kyunbug, South Korea
关键词
grain-oriented silicon steel; primary recrystallization; secondary recrystallization; coincidence boundary; grain boundary; magnetic induction;
D O I
10.1016/S0304-8853(00)00074-3
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The intensities of grain boundaries with misorientation angles between 20 degrees and 45 degrees (I-HE), and coincidence boundaries (I-C) in relation to Goss orientation were examined in the Fe-3%Si alloy processed with different levels of cold-rolling reduction. No relationship was found between the sharpness of Goss secondary recrystallization and the I-HE values; however, some correlation was found between Goss secondary recrystalization and the I-C values. (C) 2000 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:89 / 91
页数:3
相关论文
共 50 条
  • [1] Effects of cold rolling reduction on secondary recrystallization of Fe-3%Si alloy
    Shimazu, T
    Arai, S
    Sakai, T
    Tsubakino, H
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2002, 88 (03): : 49 - 56
  • [2] Influence of annealing temperature before cold rolling and Cu content on the secondary recrystallization in nitrided Fe-3% si alloy
    Harase, J
    Shimizu, R
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2003, 254 : 343 - 345
  • [3] Secondary recrystallization of the nitrided Fe-3%Si alloy
    Woo, JS
    Han, CH
    Hong, BD
    Harase, J
    ISIJ INTERNATIONAL, 1998, 38 (10) : 1114 - 1120
  • [4] Effect of cold rolling reduction on secondary recrystallization of 3%Si-FE
    Arai, S
    Ushigami, Y
    Takahashi, N
    GRAIN GROWTH IN POLYCRYSTALLINE MATERIALS II, PTS 1 AND 2, 1996, 204- : 617 - 622
  • [5] Effects of electrostatic field on recrystallization texture and grain boundary character distribution in a Fe-3%Si alloy
    Sha, YH
    Gao, XY
    Dai, CL
    Xu, JZ
    Zhao, X
    Zuo, L
    TEXTURES OF MATERIALS, PTS 1 AND 2, 2002, 408-4 : 1329 - 1334
  • [6] EFFECT OF COLD-ROLLING REDUCTION ON THE SECONDARY RECRYSTALLIZATION IN 3-PERCENT SI-FE ALLOY
    HARASE, J
    SHIMIZU, R
    TAKAHASHI, N
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1990, 54 (04) : 381 - 387
  • [7] INSTABILITY OF SECONDARY RECRYSTALLIZATION CAUSED BY EXCESSIVE COLD-ROLLING REDUCTION IN FE-3-PERCENT-SI ALLOY
    YOSHITOMI, Y
    MASUI, H
    HARASE, J
    TAKAHASHI, N
    MATERIALS TRANSACTIONS JIM, 1995, 36 (10): : 1234 - 1243
  • [8] INSTABILITY OF SECONDARY RECRYSTALLIZATION CAUSED BY EXCESSIVE COLD-ROLLING REDUCTION IN FE-3-PERCENT SI ALLOY
    YOSHITOMI, Y
    MASUI, H
    HARASE, J
    TAKAHASHI, N
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1994, 58 (08) : 882 - 891
  • [9] Effect of rolling reduction on antiphase domains, grain boundary character distribution and plastic deformation of Fe-6.5 wt%Si alloy
    Cai, Guojun
    Li, Changsheng
    Cai, Ban
    Wang, Qiwen
    MATERIALS LETTERS, 2019, 238 : 249 - 253
  • [10] The onset temperature of secondary recrystallization and the sharpness of Goss secondary recrystallization texture in the nitrided Fe-3%Si alloy
    Woo, JS
    Han, CH
    Hong, BD
    Harase, J
    ACTA MATERIALIA, 1998, 46 (14) : 4905 - 4909