Corrosion and Tensile Behaviors of Ti-4Al-2V-1Mo-1Fe and Ti-6Al-4V Titanium Alloys

被引:34
|
作者
Qiao, Yanxin [1 ]
Xu, Daokui [2 ]
Wang, Shuo [1 ,2 ,3 ]
Ma, Yingjie [2 ]
Chen, Jian [1 ]
Wang, Yuxin [1 ]
Zhou, Huiling [1 ]
机构
[1] Jiangsu Univ Sci & Technol, Sch Mat Sci & Engn, Zhenjiang 212003, Jiangsu, Peoples R China
[2] Chinese Acad Sci, Inst Met Res, Shenyang 110016, Liaoning, Peoples R China
[3] Northeastern Univ, Sch Mat Sci & Engn, Shenyang 110004, Liaoning, Peoples R China
基金
中国国家自然科学基金;
关键词
titanium alloy; corrosion; passive film; mechanical behavior; ELECTROCHEMICAL-BEHAVIOR; MECHANICAL-PROPERTIES; PASSIVATION KINETICS; STAINLESS ALLOYS; PURE TITANIUM; TIO2; FILMS; DISSOLUTION; MOLYBDENUM; ELEMENTS; IONS;
D O I
10.3390/met9111213
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
X-ray diffraction (XRD), scanning electron microscope (SEM), immersion, electrochemical, and tensile tests were employed to analyze the phase constitution, microstructure, corrosion behaviors, and tensile properties of a Ti-6Al-4V alloy and a newly-developed low cost titanium alloy Ti-4Al-2V-1Mo-1Fe. The results showed that both the Ti-6Al-4V and Ti-4Al-2V-1Mo-1Fe alloys were composed of alpha and beta phases. The volume fractions of beta phase for these two alloys were 7.4% and 47.3%, respectively. The mass losses after 180-day immersion tests in 3.5 wt.% NaCl solution of these alloys were negligible. The corrosion resistance of the Ti-4Al-2V-1Mo-1Fe alloy was higher than that of the Ti-6Al-4V alloy. The tensile tests showed that the Ti-4Al-2V-1Mo-1Fe alloy presented a slightly higher strength but a lower ductility compared to the Ti-6Al-4V alloy.
引用
收藏
页数:11
相关论文
共 50 条
  • [1] Corrosion Behavior of Ti-6Al-4V Alloys
    Nava-Dino, C. G.
    Lopez-Melendez, C.
    Bautista-Margulis, R. G.
    Neri-Flores, M. A.
    Chacon-Nava, J. G.
    de la Torre, S. D.
    Gonzalez-Rodriguez, J. G.
    Martinez-Villafane, A.
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2012, 7 (03): : 2389 - 2402
  • [2] Comparison of electrochemical behaviors of Ti-5Al-2Sn-4Zr-4Mo-2Cr-1Fe and Ti-6Al-4V titanium alloys in NaNO3 solution
    Liu, Jia
    Duan, Shuanglu
    Yue, Xiaokang
    Qu, Ningsong
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2024, 31 (04) : 750 - 763
  • [3] STRUCTURE AND PITTING CORROSION OF Ti-6Al-4V ALLOY AND Ti-6Al-4V WELDS
    Ferdinandov, Nikolay Vasilev
    Gospodinov, Danail Dimitrov
    Ilieva, Mariana Dimitrova
    Radev, Rossen Hristov
    PROCEEDINGS OF THE 7TH INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND SYSTEMS, 2018, : 325 - 330
  • [4] Influence of Environment on Constant Load and Fatigue Crack Propagation of Titanium Alloys Ti-6Al-4V and Ti-8Al-1Mo-1V.
    Doeker, Hubert
    Forschungsbericht - Deutsche Forschungs- und Versuchsanstalt fuer Luft- und Raumfahrt, 1980, (80-8):
  • [5] Powder interlayer bonding of titanium alloys: Ti-6Al-2Sn-4Zr-6Mo and Ti-6Al-4V
    P. Davies
    A. Johal
    H. Davies
    S. Marchisio
    The International Journal of Advanced Manufacturing Technology, 2019, 103 : 441 - 452
  • [6] Powder interlayer bonding of titanium alloys: Ti-6Al-2Sn-4Zr-6Mo and Ti-6Al-4V
    Davies, P.
    Johal, A.
    Davies, H.
    Marchisio, S.
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2019, 103 (1-4): : 441 - 452
  • [7] Dynamic Shear Deformation and Failure of Ti-6Al-4V and Ti-5Al-5Mo-5V-1Cr-1Fe Alloys
    Ran, Chun
    Chen, Pengwan
    MATERIALS, 2018, 11 (01)
  • [8] Effect of hydrogen charging on microstructural evolution and corrosion behavior of Ti-4Al-2V-1Mo-1Fe alloy
    Yanxin Qiao
    Daokui Xu
    Shuo Wang
    Yingjie Ma
    Jian Chen
    Yuxin Wang
    Huiling Zhou
    Journal of Materials Science & Technology, 2021, 60 (01) : 168 - 176
  • [9] Effect of hydrogen charging on microstructural evolution and corrosion behavior of Ti-4Al-2V-1Mo-1Fe alloy
    Qiao, Yanxin
    Xu, Daokui
    Wang, Shuo
    Ma, Yingjie
    Chen, Jian
    Wang, Yuxin
    Zhou, Huiling
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 60 : 168 - 176
  • [10] Study of corrosion of combinations of titanium/Ti-6Al-4V implants and dental alloys
    Yamazoe, Masatoshi
    DENTAL MATERIALS JOURNAL, 2010, 29 (05) : 542 - 553