Behavior in the fresh state and in the hardened state of alkali-activated fly ash-based mortars cured at ambient temperature

被引:0
|
作者
Lima, Lucas Pereira [1 ]
Diogenes, Daniel Gomes [1 ,3 ]
Cabral, Eduardo Bezerra [3 ]
Nogueira, Ricardo Emilio F. Q. [2 ]
da Costa, Heloina Nogueira [1 ,2 ]
机构
[1] Univ Fed Ceara, Campus Crateus,BR 226, BR-63700000 Crateus, Ceara, Brazil
[2] Univ Fed Ceara, Programa Posgrad Engn & Ciencia Mat, Av Mister Hall S-N, BR-60455670 Fortaleza, Ceara, Brazil
[3] Univ Fed Ceara, Programa Posgrad Engn Civil Estruturas & Construc, Av Mister Hall S-N, BR-60455670 Fortaleza, Ceara, Brazil
来源
MATERIA-RIO DE JANEIRO | 2022年 / 27卷 / 03期
关键词
alkali activation; waste; construction; MIX DESIGN PROCEDURE; LOW-CALCIUM FLY; GEOPOLYMER CONCRETE; MECHANICAL-PROPERTIES; COMPRESSIVE STRENGTH; PORTLAND-CEMENT; REACTIVITY;
D O I
10.1590/1517-7076-RMAT-2022-0060
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Knowledge and technology in alkali-activated materials has grown in recent years. However, the application in engineering works is still limited, mainly because some precursors require thermal curing for alkaline activation to occur. In this perspective, the objective of this research is to evaluate the behavior in the fresh state and in the hardened state of alkali-activated mortars based on fly ash, cured at ambient temperature. For the production of mortars, an alkaline activator composed of silicate and sodium hydroxide was used, the ratio between activator solution and precursor (s/p) was varied in 0.45, 0.55 and 0.65. Additionally, a conventional mortar was produced for comparison. The products of the alkali-activation reaction were identified by infrared spectroscopy (FTIR) and thermal analysis. In the fresh state, the Flow Table and Squeeze Flow tests were carried out and in the hardened state, tests of compressive strength and tensile strength in bending were carried out. The results indicate the formation of N-A-S-H gel (hydrated sodium aluminum silicate) as the main reaction product. The workability and mechanical strength of alkali-activated mortars were influenced by the amount of alkaline solution and additional water. The results were satisfactory, with tensile strengths between 5.4 MPa and 11.1 MPa and compressive strengths between 11.1 MPa and 33.3 MPa, at 28 days. These values increased as the s/p ratio increased and the additional water decreased. The conventional mortar presented flexural tensile strength of 3.3 MPa and compressive strength of 18.5 MPa. Therefore, alkali-activated mortars based on fly ash have characteristics and properties that enable their application in loco in civil construction.
引用
收藏
页数:12
相关论文
共 50 条
  • [1] Effect of temperature on the fresh and hardened state properties of alkali-activated slag/fly ash mixtures
    Dai, Xiaodi
    Aydin, Serdar
    Yardimci, Mert Yucel
    Sun, Yubo
    De Schutter, Geert
    MATERIALS AND STRUCTURES, 2023, 56 (05)
  • [2] Effect of temperature on the fresh and hardened state properties of alkali-activated slag/fly ash mixtures
    Xiaodi Dai
    Serdar Aydin
    Mert Yücel Yardimci
    Yubo Sun
    Geert De Schutter
    Materials and Structures, 2023, 56
  • [3] Fresh and Hardened Properties of Potassium Hydroxide Activated Metakaolin and Fly Ash-Based Geopolymer Mortars
    Abufarsakh, Ruwa
    Noorvand, Hassan
    Arce, Gabriel
    Hassan, Marwa
    Subedi, Sujata
    TRAN-SET 2022, 2022, : 320 - 329
  • [4] Shrinkage of Alkali-Activated Combined Slag and Fly Ash Concrete Cured at Ambient Temperature
    Rodrigue, Alexandre
    Bissonnette, Benoit
    Duchesne, Josee
    Fournier, Benoit
    ACI MATERIALS JOURNAL, 2022, 119 (03) : 15 - 23
  • [5] Determining physico-chemical parameters for high strength ambient cured fly ash-based alkali-activated cements
    Goswami, Amiya P.
    CERAMICS INTERNATIONAL, 2021, 47 (20) : 29109 - 29119
  • [6] Influence of Concrete Sludge Addition in the Properties of Alkali-Activated and Non-Alkali-Activated Fly Ash-Based Mortars
    Kesikidou, Fotini
    Konopisi, Stavroula
    Anastasiou, Eleftherios K.
    ADVANCES IN CIVIL ENGINEERING, 2021, 2021
  • [7] Frost Resistance of Alkali-Activated Combined Slag and Fly Ash Concrete Cured at Ambient Temperature
    Rodrigue, Alexandre
    Duchesne, Josee
    Fournier, Benoit
    Bissonnette, Benoit
    ACI MATERIALS JOURNAL, 2022, 119 (03) : 3 - 13
  • [8] Utilization of seawater in high calcium fly ash alkali-activated paste cured at ambient temperature
    Wongkvanklom, Athika
    Posi, Patcharapol
    Bangsai, Chaiwat
    Kasemsiri, Pornnapa
    Foytong, Piyawat
    Rukzon, Sumrerng
    Chindaprasirt, Prinya
    ADVANCES IN CONCRETE CONSTRUCTION, 2024, 18 (05) : 369 - 378
  • [9] Fresh and hardened properties of alkali-activated fly ash/slag pastes with superplasticizers
    Jang, J. G.
    Lee, N. K.
    Lee, H. K.
    CONSTRUCTION AND BUILDING MATERIALS, 2014, 50 : 169 - 176
  • [10] Workability and mechanical properties of alkali-activated fly ash-slag concrete cured at ambient temperature
    Fang, Guohao
    Ho, Wing Kei
    Tu, Wenlin
    Zhang, Mingzhong
    CONSTRUCTION AND BUILDING MATERIALS, 2018, 172 : 476 - 487