Nanofibrous poly(vinyl alcohol)/chitosan contained carbonated hydroxyapatite nanoparticles scaffold for bone tissue engineering

被引:99
|
作者
Januariyasa, I. Komang [1 ]
Ana, Ika Dewi [2 ]
Yusuf, Yusril [1 ]
机构
[1] Univ Gadjah Mada, Fac Math & Nat Sci, Dept Phys, Yogyakarta 55281, Indonesia
[2] Univ Gadjah Mada, Dept Dent Biomed Sci, Fac Dent, Yogyakarta 55281, Indonesia
关键词
Bone tissue engineering; Carbonated hydroxyapatite; Nanofibrous scaffold; Electrospinning; Tensile strength; Cell viability; MECHANICAL-PROPERTIES; CALCIUM PHOSPHATES; COMPOSITE SCAFFOLDS; FIBER DIAMETER; ELECTROSPUN; SUBSTITUTION; FABRICATION; CHITOSAN; CELLS; BIOCOMPATIBILITY;
D O I
10.1016/j.msec.2019.110347
中图分类号
TB3 [工程材料学]; R318.08 [生物材料学];
学科分类号
0805 ; 080501 ; 080502 ;
摘要
A scaffold that mimics the physicochemical structure of bone at the nanoscale level is an attractive alternative to conventional bone grafts, but its development remains a main challenge in bone tissue engineering today. This work describes the fabrication of a nanofibrous poly(vinyl alcohol)/chitosan/carbonated hydroxyapatite (PVA/CS/CHAp) scaffold. CHAp nanoparticles were synthesized using a co-precipitation method, and nanofibrous PVA/CS/CHAp scaffolds were fabricated by electrospinning using CHAp concentrations of 0, 5, 10, 15, and 20 wt%. The physicochemical properties of the scaffolds were evaluated by SEM, XRD, FUR, and EDS, and the mechanical properties were determined by tensile strength tests. Swelling behavior, protein adsorption onto the scaffold surfaces, surface biomineralization, and cells viability were also evaluated in vitro. The addition of CHAp to the composite decreased the fiber diameter from similar to 160 nm at 0 wt% to similar to 139 nm at 15 wt% and great agglomerations were evident at 20 wt%. XRD, FUR, and EDS showed effective incorporation of CHAp into the nanofibrous structure. This CHAp incorporation significantly increased the modulus of the scaffold at PVA/CS/CHAp 15 wt%, with an average 103.86 MPa, but tensile strength was not significantly altered. However, the elongation at break was decreased as the CHAp concentration increased. Swelling capacity of scaffold increases due to CHAp addition. Protein adsorption onto the scaffold increased 2.3 fold at 20 wt% when compared to 0 wt %. The PVA/CS/CHAp 15 wt% showed a better bioactivity when compared to PVA/CS/CHAp 0 wt% after immersion of the scaffolds in a simulated body fluid solution for 7 days. Cell viability and cell morphology results reveal that PVA/CS/CHAp able to facilitate osteoblast cells to attach and proliferate. Introducing higher CHAp into the scaffold could increase the cell viability of the scaffold. PVA/CS/CHAp has potential to serve as an alternative scaffold material for bone tissue engineering.
引用
收藏
页数:13
相关论文
共 50 条
  • [1] Fabrication of chitosan/poly(caprolactone) nanofibrous scaffold for bone and skin tissue engineering
    Shalumon, K. T.
    Anulekha, K. H.
    Chennazhi, K. P.
    Tamura, H.
    Nair, S. V.
    Jayakumar, R.
    [J]. INTERNATIONAL JOURNAL OF BIOLOGICAL MACROMOLECULES, 2011, 48 (04) : 571 - 576
  • [2] Chitosan/hydroxyapatite hybrid scaffold for bone tissue engineering
    Brun, V.
    Guillaume, C.
    Alami, S. Mechiche
    Josse, J.
    Jing, J.
    Draux, F.
    Bouthors, S.
    Laurent-Maquin, D.
    Gangloff, S. C.
    Kerdjoudj, H.
    Velard, F.
    [J]. BIO-MEDICAL MATERIALS AND ENGINEERING, 2014, 24 : S63 - S73
  • [3] Nanofibrous poly(ε-caprolactone)/poly(vinyl alcohol)/chitosan hybrid scaffolds for bone tissue engineering using mesenchymal stem cells
    Mohammadi, Y.
    Soleimani, M.
    Fallahi-Sichani, M.
    Gazme, A.
    Haddadi-Asl, V.
    Arefian, E.
    Kiani, J.
    Moradi, R.
    Atashi, A.
    Ahmadbeigi, N.
    [J]. INTERNATIONAL JOURNAL OF ARTIFICIAL ORGANS, 2007, 30 (03): : 204 - 211
  • [4] Poly(vinyl alcohol)-hydroxyapatite biomimetic scaffold for tissue regeneration
    Sinha, Arvind
    Das, Gautam
    Sharma, Binay Kumar
    Roy, Raja Prabahan
    Pramanick, Ashit Kumar
    Nayar, Suprabha
    [J]. MATERIALS SCIENCE & ENGINEERING C-BIOMIMETIC AND SUPRAMOLECULAR SYSTEMS, 2007, 27 (01): : 70 - 74
  • [5] A Comparison of the Effects of Silica and Hydroxyapatite Nanoparticles on Poly(ε-caprolactone)-Poly(ethylene glycol)-Poly(ε-caprolactone)/Chitosan Nanofibrous Scaffolds for Bone Tissue Engineering
    Hokmabad, Vahideh Raeisdasteh
    Davaran, Soodabeh
    Aghazadeh, Marziyeh
    Alizadeh, Effat
    Salehi, Roya
    Ramazani, Ali
    [J]. TISSUE ENGINEERING AND REGENERATIVE MEDICINE, 2018, 15 (06) : 735 - 750
  • [6] A Comparison of the Effects of Silica and Hydroxyapatite Nanoparticles on Poly(ε-caprolactone)-Poly(ethylene glycol)-Poly(ε-caprolactone)/Chitosan Nanofibrous Scaffolds for Bone Tissue Engineering
    Vahideh Raeisdasteh Hokmabad
    Soodabeh Davaran
    Marziyeh Aghazadeh
    Effat Alizadeh
    Roya Salehi
    Ali Ramazani
    [J]. Tissue Engineering and Regenerative Medicine, 2018, 15 : 735 - 750
  • [7] Nanofibrous scaffold from electrospinning biodegradable waterborne polyurethane/poly(vinyl alcohol) for tissue engineering application
    Wu, Yingke
    Lin, Weiwei
    Hao, Hongye
    Li, Jiehua
    Luo, Feng
    Tan, Hong
    [J]. JOURNAL OF BIOMATERIALS SCIENCE-POLYMER EDITION, 2017, 28 (07) : 648 - 663
  • [8] Hydroxyapatite-Chitosan and Gelatin Based Scaffold for Bone Tissue Engineering
    Maji, Kanchan
    Dasgupta, Sudip
    [J]. TRANSACTIONS OF THE INDIAN CERAMIC SOCIETY, 2014, 73 (02) : 110 - 114
  • [9] Reinforcement of hydroxyethyl cellulose / poly (vinyl alcohol) with cellulose nanocrystal as a bone tissue engineering scaffold
    Nor Sarahtul Nadirah Hairol Nizan
    Farah Hanani Zulkifli
    [J]. Journal of Polymer Research, 2020, 27
  • [10] Reinforcement of hydroxyethyl cellulose / poly (vinyl alcohol) with cellulose nanocrystal as a bone tissue engineering scaffold
    Nizan, Nor Sarahtul Nadirah Hairol
    Zulkifli, Farah Hanani
    [J]. JOURNAL OF POLYMER RESEARCH, 2020, 27 (06)