Ageing kinetics and strength of airborne-particle abraded 3Y-TZP ceramics

被引:39
|
作者
Cotic, Jasna [1 ]
Jevnikar, Peter [1 ]
Kocjan, Andraz [2 ]
机构
[1] Univ Ljubljana, Fac Med, Dept Prosthodont, Hrvatski Trg 6, SI-1000 Ljubljana, Slovenia
[2] Jozef Stefan Inst, Dept Nanostruct Mat, Jamova 39, SI-1000 Ljubljana, Slovenia
关键词
Zirconia; Airborne-particle abrasion; Low-temperature degradation; Phase transformation; Flexural strength; LOW-TEMPERATURE DEGRADATION; Y-TZP CERAMICS; STABILIZED TETRAGONAL ZIRCONIA; HYDROTHERMAL DEGRADATION; DENTAL APPLICATIONS; PHASE-TRANSFORMATION; DAMAGE;
D O I
10.1016/j.dental.2017.04.014
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objective. The combined effects of alumina airborne-particle abrasion and prolonged in vitro ageing on the flexural strength of 3Y-TZP ceramic have been studied. The aim was to identify the different effects on the surface and subsurface regions that govern the performance of this popular bioceramic known for its susceptibility to low-temperature degradation (LTD). Methods.<bold> </bold>As-sintered or airborne-particle abraded 3Y-TZP discs were subjected to ageing at 134 degrees C for up to 480 h. Biaxial flexural strength was measured and the relative amount of monoclinic phase determined using X-ray diffraction. The transformed zone depth (TZD) was observed on cross-sections with scanning electron microscopy coupled with a focused ion beam. Segmented linear regression was used to analyze the flexural strength and TZD as functions of the ageing time. Results. A two-step linear ageing kinetics was detected in airborne-particle abraded specimens, reflecting the different microstructures through which the LTD proceeds into the bulk. A 10 mu m thick altered zone under the abraded surface was involved in both the surface strengthening and the increased ageing resistance. When the zone was annihilated by the LTD, the strength of the ceramic specimens and the speed of LTD returned to the values measured before abrasion. Even at prolonged ageing times, the strength of abraded groups was not lower than that of as-sintered groups. Significance. Both the ageing kinetics and the flexural strength were prominently affected by airborne-particle abrasion, which altered the subsurface microstructure and phase composition. Airborne-particle abrasion was not harmful to the 3Y-TZP ceramics stability. (C) 2017 The Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:847 / 856
页数:10
相关论文
共 50 条
  • [1] Complexity of the relationships between the sintering-temperature-dependent grain size, airborne-particle abrasion, ageing and strength of 3Y-TZP ceramics
    Cotic, Jasna
    Jevnikar, Peter
    Kocjan, Andraz
    Kosmac, Tomaz
    DENTAL MATERIALS, 2016, 32 (04) : 510 - 518
  • [2] The Influence of Alumina Airborne-Particle Abrasion on the Properties of Zirconia-Based Dental Ceramics (3Y-TZP)
    Lagodzinska, Paulina
    Dejak, Beata
    Konieczny, Bartlomiej
    COATINGS, 2023, 13 (10)
  • [3] Microstructural Characteristics of 3Y-TZP Ceramics and Their Effects on the Flexural Strength
    Alves, Manuel Fellipe Rodrigues Pais
    de Campos, Leonardo Queiroz Bueno
    Simba, Bruno Galvao
    da Silva, Cosme Roberto Moreira
    Strecker, Kurt
    dos Santos, Claudinei
    CERAMICS-SWITZERLAND, 2022, 5 (04): : 798 - 813
  • [4] Processing and structural characterisation of 3Y-TZP ceramics resistant to hydrothermal ageing
    Rodriquez-Pulido, A
    Ross, IM
    Rainforth, WM
    EURO CERAMICS VII, PT 1-3, 2002, 206-2 : 1053 - 1056
  • [5] Relationship between grain size and strength for 3Y-TZP ceramics
    Zheng, YS
    Yan, DS
    Gao, L
    Lu, ZL
    ECF 11 - MECHANISMS AND MECHANICS OF DAMAGE AND FAILURE, VOLS I-III, 1996, : 765 - 770
  • [6] Ageing effects on the nanoindentation response of sub-micrometric 3Y-TZP ceramics
    Stefano Guicciardi
    Takayoshi Shimozono
    Giuseppe Pezzotti
    Journal of Materials Science, 2007, 42 : 718 - 722
  • [7] Ageing effects on the nanoindentation response of sub-micrometric 3Y-TZP ceramics
    Guicciardi, Stefano
    Shimozono, Takayoshi
    Pezzotti, Giuseppe
    JOURNAL OF MATERIALS SCIENCE, 2007, 42 (02) : 718 - 722
  • [8] Effect of ageing on scratch resistance of 3Y-TZP
    Hvizdos, P.
    Chintapalli, R.
    Valle, J.
    Anglada, M.
    KOVOVE MATERIALY-METALLIC MATERIALS, 2009, 47 (05): : 333 - 339
  • [9] Novel process for the production of 3Y-TZP ceramics: comparison between ageing in artificial saliva and accelerated ageing
    Aragon-Duarte, M. C.
    Bocanegra Bernal, M.
    Reyes-Rojas, A.
    Esparza-Ponce, H. E.
    MATERIALS RESEARCH EXPRESS, 2020, 7 (06)
  • [10] Strength limits in mesoscaled 3Y-TZP ceramics for micro-surgical instruments
    Antolino, N.
    Muhlstein, C.
    Hayes, G.
    Adair, J.
    Bermejo, R.
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2019, 91 : 99 - 108