Densification, Tailored Microstructure, and Mechanical Properties of Selective Laser Melted Ti-6Al-4V Alloy via Annealing Heat Treatment

被引:23
|
作者
Wang, Di [1 ]
Wang, Han [1 ]
Chen, Xiaojun [1 ]
Liu, Yang [2 ]
Lu, Dong [3 ,4 ]
Liu, Xinyu [3 ,4 ]
Han, Changjun [1 ]
机构
[1] South China Univ Technol, Sch Mech & Automot Engn, Guangzhou 510641, Peoples R China
[2] Ningbo Univ, Lab Impact & Safety Engn, Minist Educ, Ningbo 315211, Peoples R China
[3] Pangang Grp Res Inst Co Ltd, State Key Lab Vanadium & Titanium Resources Compr, Panzhihua 617000, Peoples R China
[4] Chengdu Adv Met Mat Ind Technol Res Inst Co Ltd, Sichuan Adv Met Mat Addit Mfg Engn Technol Res Ct, Chengdu 610300, Peoples R China
关键词
additive manufacturing; selective laser melting; laser powder bed fusion; Ti-6Al-4V; heat treatment; annealing; PROCESS PARAMETERS; PROCESSING PARAMETERS; SURFACE QUALITY; EVOLUTION; TENSILE; BEHAVIOR; SLM; OPTIMIZATION; IMPROVEMENT; MARTENSITE;
D O I
10.3390/mi13020331
中图分类号
O65 [分析化学];
学科分类号
070302 ; 081704 ;
摘要
This work investigated the influence of process parameters on the densification, microstructure, and mechanical properties of a Ti-6Al-4V alloy printed by selective laser melting (SLM), followed by annealing heat treatment. In particular, the evolution mechanisms of the microstructure and mechanical properties of the printed alloy with respect to the annealing temperature near the beta phase transition temperature were investigated. The process parameter optimization of SLM can lead to the densification of the printed Ti-6Al-4V alloy with a relative density of 99.51%, accompanied by an ultimate tensile strength of 1204 MPa and elongation of 7.8%. The results show that the microstructure can be tailored by altering the scanning speed and annealing temperature. The SLM-printed Ti-6Al-4V alloy contains epitaxial growth beta columnar grains and internal acicular martensitic alpha ' grains, and the width of the beta columnar grain decreases with an increase in the scanning speed. Comparatively, the printed alloy after annealing in the range of 750-1050 degrees C obtains the microstructure consisting of alpha + beta dual phases. In particular, network and Widmanstatten structures are formed at the annealing temperatures of 850 degrees C and 1050 degrees C, respectively. The maximum elongation of 14% can be achieved at the annealing temperature of 950 degrees C, which was 79% higher than that of as-printed samples. Meanwhile, an ultimate tensile strength larger than 1000 MPa can be maintained, which still meets the application requirements of the forged Ti-6Al-4V alloy.
引用
收藏
页数:15
相关论文
共 50 条
  • [1] Tailorable microstructure and mechanical properties of selective laser melted TiB/Ti-6Al-4V composite by heat treatment
    Zhang, Jinliang
    Song, Bo
    Cai, Chao
    Zhang, Lijun
    Shi, Yusheng
    ADVANCED POWDER MATERIALS, 2022, 1 (02):
  • [2] Effects of heat treatment on microstructure and mechanical properties of selective laser melted Ti-6Al-4V lattice materials
    Jin, Nan
    Yan, Zhenyu
    Wang, Yangwei
    Cheng, Huanwu
    Zhang, Hongmei
    International Journal of Mechanical Sciences, 2021, 190
  • [3] Effects of heat treatment on microstructure and mechanical properties of selective laser melted Ti-6Al-4V lattice materials
    Jin, Nan
    Yan, Zhenyu
    Wang, Yangwei
    Cheng, Huanwu
    Zhang, Hongmei
    INTERNATIONAL JOURNAL OF MECHANICAL SCIENCES, 2021, 190
  • [4] Effect of Annealing Temperature on the Microstructure and Mechanical Properties of Selective Laser Melted Alloy Ti – 6% Al – 4% V
    Yauntao Qu
    Zhiting Luo
    Xin Dong
    Yanan Zhou
    Qi Sun
    Miaomiao Wu
    Ning Li
    Jiazhen Yan
    Biao Zhang
    Rui Li
    Sheng Xu
    Metal Science and Heat Treatment, 2022, 64 : 26 - 33
  • [5] The microstructure transformation of selective laser melted Ti-6Al-4V alloy
    Sun, Jing
    Zhu, Xiaogang
    Qiu, Lianfang
    Wang, Fei
    Yang, Yang
    Guo, Lijie
    MATERIALS TODAY COMMUNICATIONS, 2019, 19 : 277 - 285
  • [6] On the role of different annealing heat treatments on mechanical properties and microstructure of selective laser melted and conventional wrought Ti-6Al-4V
    Khorasani, AmirMahyar
    Gibson, Ian
    Goldberg, Moshe
    Littlefair, Guy
    RAPID PROTOTYPING JOURNAL, 2017, 23 (02) : 295 - 304
  • [7] Microstructural evolution and mechanical properties of selective laser melted Ti-6Al-4V induced by annealing treatment
    Pei, Wang
    Chen Feng-hua
    Eckert, J.
    Pilz, S.
    Scudino, S.
    Prashanth, K. G.
    JOURNAL OF CENTRAL SOUTH UNIVERSITY, 2021, 28 (04) : 1068 - 1077
  • [8] Effect of heat treatment on microstructure evolution and mechanical properties of selective laser melted Ti-6Al-4V and TiB/Ti-6Al-4V composite: A comparative study
    Li, Hailiang
    Jia, Dechang
    Yang, Zhihua
    Liao, Xingqi
    Jin, Haize
    Cai, Delong
    Zhou, Yu
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 801
  • [9] Microstructure and mechanical properties of selective laser melted Ti6Al4V alloy
    Losertova, M.
    Kubes, V.
    27TH JOINT SEMINAR DEVELOPMENT OF MATERIALS SCIENCE IN RESEARCH AND EDUCATION, 2017, 266
  • [10] Effect of Build Orientation on the Microstructure and Mechanical Properties of Selective Laser-Melted Ti-6Al-4V Alloy
    Hartunian, Patrick
    Eshraghi, Mohsen
    JOURNAL OF MANUFACTURING AND MATERIALS PROCESSING, 2018, 2 (04):