Synthesis and mechanical behavior of poly (vinyl alcohol) / poly (vinyl acetate) microspheres

被引:3
|
作者
Ambrosio Tellez, Luisa [1 ,2 ,3 ,4 ]
Gisela Veron, Maria [1 ,2 ]
Cardoso Cuneo, Jorge [3 ,4 ,5 ]
Oscar Prado, Miguel [1 ,2 ]
机构
[1] Natl Atom Energy Commiss CNEA, Dept Nucl Mat, Med & Ind Applicat Div, San Carlos De Bariloche, Rio Negro, Argentina
[2] Natl Sci & Tech Res Council CONICET, Buenos Aires, DF, Argentina
[3] Univ Buenos Aires UBA, Med Fac, Buenos Aires, DF, Argentina
[4] Univ Buenos Aires, Nucl Med Oncol Ctr, Inst Oncol Angel H Roffo, Buenos Aires, DF, Argentina
[5] Inst Oncol Angel H Roffo, Dept Gastroenterol Surg, Buenos Aires, DF, Argentina
来源
关键词
Microspheres; structural and thermal studies; mechanical properties; POLY(VINYL ALCOHOL); EMBOLIZATION; DEGRADATION; PARTICLES; BEADS;
D O I
10.1080/25740881.2022.2075273
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
In this work, the effect of an organic solvent (tert-butanol) during the polymerization of vinyl acetate (VAc) on the structural and elastic properties of poly(vinyl alcohol)/poly(vinyl acetate) microspheres fabricated by the suspension polymerization method was investigated. As a result, two types of microspheres were obtained: without tert-butanol (Ms-P) and with tert-butanol (Ms-T), the later was added during the polymerization. For the experimental conditions used in this work, both types of Ms had spherical shape. Also, Ms-P exhibits a size distribution ranging from 10 pm to 1200 mu m with an apparent density value similar to 1.18 +/- 0.03 g/cm(3), a solid structure and a saponification grade alpha similar to 0.8. In turn, Ms-T shows a size distribution between 400 and 1900 mu m, porous structure, a lower density value rho similar to 0.87 +/- 0.03 g/cm(3) and alpha similar to 0.5. The mechanical tests performed on Ms-P and Ms-T in three different conditions (dry, suspended in distilled water and saline solution) showed Young's modulus (E) values of 569 +/- 162 MPa (dried), 8 +/- 9 MPa (distilled water), 11 +/- 9 MPa (saline solution) for Ms-P measured up to 30% of deformation. For Ms-T, 242 +/- 63 MPa (dried), 0.52 +/- 0.08 MPa (distilled water), 0.9 +/- 0.5 MPa (saline solution) values were obtained. Thus, we have found that the E values for Ms-T are more than one order of magnitude lower than for Ms-P. Also, it was observed that keeping Ms in an aqueous medium helps decrease the E value. This work shows that the ability to control the structural and elastic properties in Ms employing addition to an organic solvent gives the possibility of tuning its behavior for possible use in the treatment of embolization and chemoembolization. [GRAPHICS] .
引用
收藏
页码:1676 / 1690
页数:15
相关论文
共 50 条
  • [1] Preparation of poly(vinyl acetate)/clay and poly(vinyl acetate)/poly(vinyl alcohol)/clay microspheres
    Hye Min Jung
    Eun Mi Lee
    Byung Chul Ji
    Sung Ok Sohn
    Han Do Ghim
    Hyunju Cho
    Young A Han
    Jin Hyun Choi
    Jae Deuk Yun
    Jeong Hyun Yeum
    [J]. Fibers and Polymers, 2006, 7 : 229 - 234
  • [2] Preparation of poly(vinyl acetate)/clay and poly(vinyl acetate)/poly(vinyl alcohol)/clay microspheres
    Jung, Hye Min
    Lee, Eun Mi
    Ji, Byung Chul
    Sohn, Sung Ok
    Ghim, Han Do
    Cho, Hyunju
    Han, Young A.
    Choi, An Hyun
    Yun, Jae Deuk
    Yeum, Jeong Hyun
    [J]. FIBERS AND POLYMERS, 2006, 7 (03) : 229 - 234
  • [3] Preparation and characterization of poly(vinyl acetate)/poly(vinyl alcohol)/clay nanocomposite microspheres
    Yeum, Jeong Hyun
    Jung, Hye Min
    Yun, Jae Deuk
    Ji, Byung Chul
    [J]. ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2006, 231
  • [4] Synthesis of poly(vinyl acetate) macromonomers and preparation of poly(vinyl acetate) grafted copolymers and poly(vinyl alcohol) grafted copolymers
    Ohnaga, T
    Sato, T
    [J]. POLYMER, 1996, 37 (16) : 3729 - 3735
  • [5] Synthesis of novel poly(vinyl methyl ether) copolymers by alkylation of poly(vinyl acetate) and poly(vinyl alcohol)
    Markova, D
    Christova, D
    Velichkova, R
    [J]. POLYMER INTERNATIONAL, 2003, 52 (10) : 1600 - 1604
  • [6] NMR SPECTRA OF POLY(VINYL ACETATE) AND POLY(VINYL ALCOHOL)
    RAMEY, KC
    LINI, DC
    [J]. JOURNAL OF POLYMER SCIENCE PART B-POLYMER LETTERS, 1967, 5 (1PB): : 39 - &
  • [7] STUDIES OF ALCOHOLYSIS OF POLY (VINYL ACETATE) TO POLY (VINYL ALCOHOL).
    Bravar, M.
    Rolich, J.
    Ban, N.
    Gnjatovic, V.
    [J]. 1974, (47): : 329 - 334
  • [8] Poly(vinyl acetate)/poly(vinyl alcohol)/montmorillonite nanocomposite microspheres prepared by suspension polymerization and saponification
    Jung, Hye Min
    Lee, Eun Mi
    Ji, Byung Chul
    Deng, Yulin
    Yun, Jae Deuk
    Yeum, Jeong Hyun
    [J]. COLLOID AND POLYMER SCIENCE, 2007, 285 (06) : 705 - 710
  • [9] Poly(vinyl acetate)/poly(vinyl alcohol)/montmorillonite nanocomposite microspheres prepared by suspension polymerization and saponification
    Hye Min Jung
    Eun Mi Lee
    Byung Chul Ji
    Yulin Deng
    Jae Deuk Yun
    Jeong Hyun Yeum
    [J]. Colloid and Polymer Science, 2007, 285 : 705 - 710
  • [10] Synthesis, characterization, and properties of poly(vinyl acetate)- and poly(vinyl alcohol)-grafted chitosan
    Radhakumary, C.
    Nair, Prabha D.
    Mathew, Suresh
    Reghunadhan Nair, C.P.
    [J]. Journal of Applied Polymer Science, 2007, 104 (03): : 1852 - 1859