Effects of heat treatment and counterface on the wear behaviour of Cr21 cast iron

被引:3
|
作者
Guo, Z-H [1 ,2 ,3 ,4 ]
Xiao, F-R [3 ,4 ]
Lu, S-L [1 ,2 ]
Liu, R-L [1 ,2 ]
Liao, B. [3 ,4 ]
机构
[1] Hebei Univ Sci & Technol, Hebei Key Lab Mat Near Net Forming Technol, Shijiazhuang 050000, Hebei, Peoples R China
[2] Hebei Univ Sci & Technol, Coll Mat Sci & Engn, Shijiazhuang 050000, Hebei, Peoples R China
[3] Yanshan Univ, Key Lab Metastable Mat Sci & Technol, Qinhuangdao 066004, Peoples R China
[4] Yanshan Univ, Coll Mat Sci & Engn, Qinhuangdao 066004, Peoples R China
关键词
Sliding; Wear; Heat treatment; Hardness; Pin-on-disc test; Counterface; Adhesive wear; Oxidation; ABRASION RESISTANCE; WHITE IRONS; CHROMIUM; MICROSTRUCTURE; HARDNESS;
D O I
10.1080/03019233.2016.1259870
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The unlubricated sliding wear test of high chromium white cast irons (HCCIs) was conducted using a pin-on-disc configuration under different heat treatments and different hardnesses of the counterface. With the increase of counterface hardness (20 HRC-47 HRC-54 HRC), the mass loss of the sample first increases then decreases. When the counterface hardness is 20 HRC, adhesion wear mainly takes place between the high chromium cast iron and the surface of 1045 steel. When the hardness is 47 or 54 HRC, first HCCI' matrix wear takes place, then carbide bump flakes under alternating stress. The mass loss of the counterface decreases with the increase of hardness for the same sample. The mass loss of quenching, once tempering and twice tempering sample decreases gradually for the same counterface hardness, but fluctuation of the samples' surface increased. The disc material is always softer than the pin material and results in a severe wear regime operation.
引用
收藏
页码:257 / 263
页数:7
相关论文
共 50 条
  • [1] Heat treatment effect on microstructure, hardness and wear resistance of Cr26 white cast iron
    Shaoping Zhou
    Yehui Shen
    Hao Zhang
    Dequan Chen
    Chinese Journal of Mechanical Engineering, 2015, 28 : 140 - 147
  • [2] Heat Treatment Effect on Microstructure, Hardness and Wear Resistance of Cr26 White Cast Iron
    ZHOU Shaoping
    SHEN Yehui
    ZHANG Hao
    CHEN Dequan
    Chinese Journal of Mechanical Engineering, 2015, (01) : 140 - 147
  • [3] Heat Treatment Effect on Microstructure, Hardness and Wear Resistance of Cr26 White Cast Iron
    Zhou Shaoping
    Shen Yehui
    Zhang Hao
    Chen Dequan
    CHINESE JOURNAL OF MECHANICAL ENGINEERING, 2015, 28 (01) : 140 - 147
  • [4] Heat Treatment Effect on Microstructure, Hardness and Wear Resistance of Cr26 White Cast Iron
    ZHOU Shaoping
    SHEN Yehui
    ZHANG Hao
    CHEN Dequan
    Chinese Journal of Mechanical Engineering, 2015, 28 (01) : 140 - 147
  • [5] EFFECT OF HEAT TREATMENT ON WEAR OF MANGANESE CAST IRON.
    Stanchev, D.I.
    1600, (14): : 11 - 12
  • [6] A comparative study on wear behaviour of Cr/Mo surface modified grey cast iron
    Zulhishamuddin, A. R.
    Aqida, S. N.
    Rashidi, M. Mohd
    OPTICS AND LASER TECHNOLOGY, 2018, 104 : 164 - 169
  • [7] Wear behaviour of hardfacing deposits on cast iron
    Chatterjee, S
    Pal, TK
    WEAR, 2003, 255 : 417 - 425
  • [8] Influence of Heat Treatment on Erosive Wear Resistance of High Cr Cast Irons
    Ngo, Huynh Kinh Luan
    Yamamoto, Kaoru
    Okuyama, Tetsuya
    Nakayama, Masaru
    Mizuno, Kuniaki
    Koizumi, Koreaki
    INTERNATIONAL JOURNAL OF METALCASTING, 2024,
  • [9] The effect of titanium on the wear behaviour of a 16%Cr white cast iron under pure sliding
    Bedolla-Jacuinde, A.
    Coffea, R.
    Mejia, I.
    Quezada, J. G.
    Rainforth, W. M.
    WEAR, 2007, 263 : 808 - 820
  • [10] Heat treatment in high Cr white cast iron Nb alloy
    A. F. Farah
    O. R. Crnkovic
    L. C. F. Canale
    Journal of Materials Engineering and Performance, 2001, 10 : 42 - 45