摘要
The lack of suitable joining techniques for dissimilar materials such as metal and ceramic for high-temperature applications and devices is a major hindrance to the utilization of their outstanding properties and lower costs. This paper presents the results of joining between the high-temperature and corrosion resistant iron-chromium-aluminium alloy (Fecralloy) with silicon nitride by use of metallic interlayer. The primary objectives were to produce joints for high-temperature applications (above 500 degreesC) and to observe the effects of processing parameters with regards to joint strength. Joining by use of a thin (12.5 mum) and non-remaining copper foil produced joints with an average maximum shear strength of 67.5 MPa (+/-5) at 1100 degreesC, 30 min dwell time at 9.5 MPa, under vacuum. The processing conditions were found to play a very important role in the joining process and effected joint strength. The results suggest that a thin aluminium nitride, AIN, reaction product layer was present on the silicon nitride interface in the joined samples. This is an indication that reactive wetting was occurring. Iron, chromium, aluminium and copper were found to infiltrate the silicon nitride, whilst silicon and nitrogen diffused into the Fecralloy. Joining was also attempted using a Ti/Cu/Ti multilayer and its variations. Joining was not possible due to the formation of a brittle reaction product layer, highlighting that wetting and joining are not synonymous. (C) 2003 Elsevier B.V. All rights reserved.
引用
收藏
页码:257 / 265
页数:9
相关论文
共 50 条
  • [1] The joining of gamma titanium aluminides via the powder interlayer bonding method
    Davies, P. D.
    Davies, H. M.
    Watkins, I.
    Britton, D. A.
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2020, 109 (7-8): : 2049 - 2054
  • [2] The joining of gamma titanium aluminides via the powder interlayer bonding method
    P. D. Davies
    H. M. Davies
    I. Watkins
    D. A. Britton
    The International Journal of Advanced Manufacturing Technology, 2020, 109 : 2049 - 2054
  • [3] Selection and function of interlayer materials in ceramic/ceramic joining
    Case, ED
    ADVANCES IN JOINING OF CERAMICS, 2003, 138 : 3 - 28
  • [4] Ceramic-to-metal joining via compliant pan
    Geiger, G
    AMERICAN CERAMIC SOCIETY BULLETIN, 1996, 75 (05): : 26 - 26
  • [5] ELECTROMAGNETIC-WAVE TECHNIQUE FOR JOINING CERAMIC TILES TO METAL AND CERAMIC SUBSTRATES
    BUCKLEY, JD
    FOX, RL
    SWAIN, RJ
    AMERICAN CERAMIC SOCIETY BULLETIN, 1981, 60 (03): : 394 - 394
  • [6] METAL CERAMIC JOINING
    ELSSNER, G
    PETZOW, G
    ISIJ INTERNATIONAL, 1990, 30 (12) : 1011 - 1032
  • [7] Joining of ceramic/metal
    Li, Shuhua
    Wang, Jianjiang
    Li, Shutang
    Tezhong Zhuzao Ji Youse Hejin/Special Casting & Nonferrous Alloys, 2000, (02): : 51 - 53
  • [8] CERAMIC-TO-METAL BONDING WITH SPUTTERING AS A METALLIZATION TECHNIQUE
    BRONNES, RL
    HUGHES, RC
    SWEET, RC
    PHILIPS TECHNICAL REVIEW, 1975, 35 (7-8): : 209 - 211
  • [9] BONDING - JOINING TECHNIQUE OF THE FUTURE
    BROCKMANN, W
    MATERIALWISSENSCHAFT UND WERKSTOFFTECHNIK, 1992, 23 (12) : 432 - 436
  • [10] METAL-CERAMIC JOINING
    NOGI, K
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1985, 71 : 1617 - 1617