The 455 °C tensile and fatigue behavior of boron-modified Ti-6Al-2Sn-4Zr-2Mo-0.1Si(wt.%)

被引:25
|
作者
Chen, W. [1 ]
Boehlert, C. J. [1 ]
机构
[1] Michigan State Univ, Dept Chem Engn & Mat Sci, E Lansing, MI 48824 USA
关键词
Titanium; Boron; Microstructure; Grain refinement; TiB; CREEP-BEHAVIOR; CRACK GROWTH; MICROSTRUCTURE; TIB; COMPOSITES;
D O I
10.1016/j.ijfatigue.2009.06.002
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
This work investigated the effect of nominal boron additions of 0.1 wt.%, 0.4 wt.%, and 1.0 wt.% on the elevated-temperature (455 degrees C) tensile and fatigue behavior of Ti-6Al-2Sn-4Zr-2Mo-0.1Si(wt.%) (Ti-6242S) castings. Boron additions stabilized the orthorhombic TiB phase where the average TiB-phase volume percents were 0.7, 2.3, and 5.4 for the Ti-6242S-0.1 B(wt.%), Ti-6242S-0.4B(vvt.%), and Ti-6242S-1B(wt.%) alloys, respectively. Larger TiB-phase volume fractions led to larger ultimate tensile strengths. The Ti-6242S-0.1 B alloy exhibited the largest elongation-to-failure (epsilon(f) = 10.3%) while the Ti-6242S-0.4B and Ti-6242S-1B alloys exhibited brittle fracture and epsilon(f) values of approximately 1%. The fatigue S-N behavior was recorded for maximum applied stresses between 300 and 500 MPa (R = 0.1, 5 Hz). The Ti-6242S-0.1B(wt.%) alloy exhibited the longest average fatigue lives, which was suggested to be related to the ductility of this alloy. The Ti-6242S-1B(wt.%) alloy exhibited the lowest average fatigue lives and this was suggested to be related to the low epsilon(f) and poor fatigue crack growth resistance. In situ fatigue crack growth experiments revealed that the TiB phase was the locus for cracking. Each alloy exhibited a-phase cracking and environmentally-assisted surface edge cracking. The fatigue behavior of the as-cast Ti-6242S-xB(wt.%) alloy system was comparable with that of the as-cast Ti-6Al-4V-xB(wt.%) alloy system, although the average fatigue lives of Ti-6242S-0.1 B(wt.%) alloy were significantly greater than those for Ti-6Al-V-0.1B(wt.%). Overall, the Ti-6242S-0.1 B alloy exhibits the best combination of elevated-temperature tensile and tensile-fatigue properties of all the as-cast alpha+beta TiB alloys studied to date. (C) 2009 Elsevier Ltd. All rights reserved.
引用
收藏
页码:799 / 807
页数:9
相关论文
共 50 条
  • [1] Electron beam melting of boron-modified Ti-6Al-2Sn-4Zr-2Mo-0.1Si alloy with superior tensile strength and oxidation resistance at elevated temperatures
    Fujieda, Tadashi
    Cui, Yujie
    Aoyagi, Kenta
    Koizumi, Yuichiro
    Chiba, Akihiko
    [J]. MATERIALIA, 2018, 4 : 367 - 372
  • [2] Microstructure, Tensile Properties, and Fatigue Behavior of Linear Friction-Welded Ti-6Al-2Sn-4Zr-2Mo-0.1Si
    Rajan, Sidharth
    Wanjara, Priti
    Gholipour, Javad
    Kabir, Abu Syed
    [J]. MATERIALS, 2021, 14 (01) : 1 - 21
  • [3] An investigation on fatigue and dwell-fatigue crack growth in Ti-6Al-2Sn-4Zr-2Mo-0.1Si
    Shen, W
    Soboyejo, WO
    Soboyejo, ABO
    [J]. MECHANICS OF MATERIALS, 2004, 36 (1-2) : 117 - 140
  • [4] Effect of Boron on the Elevated-Temperature Tensile and Creep Behavior of Cast Ti-6Al-2Sn-4Zr-2Mo-0.1Si (Weight Percent)
    Chen, W.
    Boehlert, C. J.
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2009, 40A (07): : 1568 - 1578
  • [5] Effect of Boron on the Elevated-Temperature Tensile and Creep Behavior of Cast Ti-6Al-2Sn-4Zr-2Mo-0.1Si (Weight Percent)
    W. Chen
    C.J. Boehlert
    [J]. Metallurgical and Materials Transactions A, 2009, 40 : 1568 - 1578
  • [6] The twisting mechanism of subsurface fatigue cracking in Ti-6Al-2Sn-4Zr-2Mo-0.1Si alloy
    Shanyavskiy, A.
    Banov, M.
    [J]. ENGINEERING FRACTURE MECHANICS, 2010, 77 (11) : 1896 - 1906
  • [7] The effect of processing on the 455°C tensile and fatigue behavior of boron-modified Ti-6Al-4V
    Chen, W.
    Boehlert, C. J.
    Payzant, E. A.
    Howe, J. Y.
    [J]. INTERNATIONAL JOURNAL OF FATIGUE, 2010, 32 (03) : 627 - 638
  • [8] Fatigue Behavior of Linear Friction Welded Ti-6Al-4V and Ti-6Al-2Sn-4Zr-2Mo-0.1Si Dissimilar Welds
    Rajan, Sidharth
    Wanjara, Priti
    Gholipour, Javad
    Kabir, Abu Syed
    [J]. MATERIALS, 2021, 14 (11)
  • [9] Correlation between microstructures and tensile deformation behavior of a PM near α Ti-6Al-2Sn-4Zr-2Mo-0.1Si alloy
    Wu, Xiaogang
    Zhang, Bowen
    Zhang, Youyun
    Niu, Hongzhi
    Zhang, Deliang
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 825
  • [10] Low-temperature superplasticity and coarsening behavior of Ti-6Al-2Sn-4Zr-2Mo-0.1Si
    Park, Chan Hee
    Lee, Byounggab
    Semiatin, S. L.
    Lee, Chong Soo
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (20): : 5203 - 5211