Role of silica fume on hydration and strength development of ultra-high performance concrete

被引:39
|
作者
Xi, Juyu [1 ,2 ]
Liu, Jianzhong [1 ]
Yang, Kai [2 ]
Zhang, Shihao [2 ]
Han, Fangyu [1 ]
Sha, Jianfang [1 ]
Zheng, Xin [3 ]
机构
[1] Jiangsu Res Inst Bldg Sci Co Ltd, State Key Lab High Performance Civil Engn Mat, Nanjing 210008, Peoples R China
[2] Chongqing Univ, Sch Mat Sci & Engn, Chongqing 400044, Peoples R China
[3] Jiangsu Keyonghe Testing & Accrediting Ctr Constru, Nanjing 211199, Peoples R China
基金
中国国家自然科学基金; 国家重点研发计划;
关键词
Ultra-high performance concrete; Silica fume; Filler effect; Pozzolanic reaction; Cement hydration; Strength development; AUTOGENOUS SHRINKAGE; TRICALCIUM SILICATE; AMORPHOUS SILICA; CEMENT PASTE; LOW WATER; MICROSTRUCTURE; MECHANISMS; NUCLEATION; KINETICS; UHPC;
D O I
10.1016/j.conbuildmat.2022.127600
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Silica fume (SF) is the most commonly used ingredient in ultra-high performance concrete (UHPC) due to its inherited properties, which can effectively improve the rheology and mechanical performance. However, in-vestigations with regard to its filler effect and pozzolanic reaction on UHPC are limited. To assess the contri-bution from SF, a chemically inert filler of titanium dioxide (TD), with a comparable particle size distribution and specific surface area (per unit volume), was selected as a reference ingredient to eliminate the influence of packing effect. Results showed the addition of SF will accerate the early hydation of UHPC and it is controlled by the combined effect of seeding effect and preferential adsorption. Moreover, the SF's surface characteristic controlling the concentration of adsorption sites provided for hydration product is the key factor influencing the early hydration rather than surface specific area. Furthermore, the enhancement of compressive strength of UHPC after 3 days is attributed to the pozzolanic reaction of SF and its promoting effect on cement hydration degree. The total contribution is less than 20%, and it will enhances with the decrease of W/C ratio.
引用
收藏
页数:11
相关论文
共 50 条
  • [1] EFFECT OF REPLACEMENT OF SILICA FUME WITH CALCINED CLAY ON THE HYDRATION AND MICROSTRUCTURAL DEVELOPMENT OF ULTRA-HIGH PERFORMANCE CONCRETE
    Huang, Wei
    Kazemi-Kamya, Hadi
    Sun, Wei
    Scrivener, Karen
    1ST INTERNATIONAL CONFERENCE ON UHPC MATERIALS AND STRUCTURES, 2016, 105 : 403 - 408
  • [2] Glass fiber reinforced ultra-high strength concrete with silica fume
    Natarajan, Sathyakumar
    Murugesan, Arun
    Dhanapal, Jagatheeswaran
    Narayanan, Arunachalam
    GRADEVINAR, 2022, 74 (10): : 849 - 856
  • [3] Uncovering the role of micro silica in hydration of ultra-high performance concrete (UHPC)
    Lee, Nam Kon
    Koh, K. T.
    Kim, Min Ook
    Ryu, G. S.
    CEMENT AND CONCRETE RESEARCH, 2018, 104 : 68 - 79
  • [4] Influence of amorphous silica on the hydration in ultra-high performance concrete
    Oertel, Tina
    Helbig, Uta
    Hutter, Frank
    Kletti, Holger
    Sextl, Gerhard
    CEMENT AND CONCRETE RESEARCH, 2014, 58 : 121 - 130
  • [5] Effects of Silica Fume Purity on Behavior of Ultra-High Performance Concrete
    Carey, Ashley S.
    Howard, Isaac L.
    Shannon, Jay
    ADVANCES IN CIVIL ENGINEERING MATERIALS, 2022, 11 (01): : 354 - 371
  • [6] Influence of silica fume and thermal curing on long-term hydration, microstructure and compressive strength of ultra-high performance concrete (UHPC)
    Xu, Disheng
    Tang, Jinhui
    Hu, Xiang
    Zhou, Yichuan
    Yu, Cheng
    Han, Fangyu
    Liu, Jiaping
    CONSTRUCTION AND BUILDING MATERIALS, 2023, 395
  • [7] The influence of the amount of silica fume on the mechanical property of ultra-high performance concrete
    Park, Jung-Jun
    Ryu, Gum-Sung
    Kang, Su-Tae
    Kim, Sung-Wook
    ADVANCES IN FRACTURE AND DAMAGE MECHANICS VII, 2008, 385-387 : 701 - 704
  • [8] Amorphous silica in ultra-high performance concrete: First hour of hydration
    Oertel, Tina
    Hutter, Frank
    Helbig, Uta
    Sextl, Gerhard
    CEMENT AND CONCRETE RESEARCH, 2014, 58 : 131 - 142
  • [9] MICROSTRUCTURAL DEVELOPMENT DURING HYDRATION IN ULTRA-HIGH PERFORMANCE CONCRETE
    Pfeifer, Claudia
    Moeser, Bernd
    Stark, Jochen
    CEMENT WAPNO BETON, 2010, 15 (03): : 123 - +
  • [10] Hydration, phase and microstructure development of Ultra-High Performance Concrete
    Pfeifer, Claudia
    Moeser, Bernd
    Stark, Jochen
    ZKG INTERNATIONAL, 2010, 63 (10): : 71 - 79