MOF-derived iron as an active energy storage material for intermediate-temperature solid oxide iron-air redox batteries

被引:19
|
作者
Zhang, Cuijuan [1 ,2 ]
Huang, Kevin [1 ]
机构
[1] Univ South Carolina, Dept Mech Engn, Columbia, SC 29208 USA
[2] Tianjin Univ, Sch Chem Engn & Technol, Tianjin 300350, Peoples R China
关键词
PERFORMANCE; DURABILITY;
D O I
10.1039/c7cc06131e
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
here demonstrate that the iron derived from an iron-based metal-organic framework (MOF), with exposed high-density Fe-atom planes, exhibits improved reduction activity, enabling good rechargeability of solid oxide iron-air redox batteries at 500 degrees C. The discharge mass specific energies are 226.5 W h kg(-1)-Fe and 214.8Wh kg(-1)-Fe at C/4 and C/3, respectively, at a constant Fe-utilization of 20%.
引用
收藏
页码:10564 / 10567
页数:4
相关论文
共 41 条
  • [1] Energy efficiency of an intermediate-temperature solid oxide iron-air redox battery
    Jin, Xinfang
    Zhao, Xuan
    Tong, Jingjing
    Yasmeen, Farzana
    White, Ralph E.
    Huang, Kevin
    JOURNAL OF ENERGY STORAGE, 2015, 3 : 1 - 9
  • [2] An Intermediate-Temperature Solid Oxide Iron-Air Redox Battery Operated on O2--Chemistry and Loaded with Pd-Catalyzed Iron-Based Energy Storage Material
    Zhang, Cuijuan
    Huang, Kevin
    ACS ENERGY LETTERS, 2016, 1 (06): : 1206 - 1211
  • [3] Energy storage characteristics of a new rechargeable solid oxide iron-air battery
    Zhao, Xuan
    Xu, Nansheng
    Li, Xue
    Gong, Yunhui
    Huang, Kevin
    RSC ADVANCES, 2012, 2 (27): : 10163 - 10166
  • [4] Solid Oxide Iron-Air Rechargeable Battery - A New Energy Storage Mechanism
    Zhao, X.
    Xu, N.
    Li, X.
    Gong, Y.
    Huang, K.
    BATTERIES AND ENERGY TECHNOLOGY (GENERAL SESSION) - 222ND ECS MEETING/PRIME 2012: IN HONOR OF JAMES MCBREEN, 2013, 50 (45): : 115 - 123
  • [5] A novel intermediate-temperature all ceramic iron-air redox battery: the effect of current density and cycle duration
    Zhao, Xuan
    Li, Xue
    Gong, Yunhui
    Xu, Nansheng
    Huang, Kevin
    RSC ADVANCES, 2014, 4 (43): : 22621 - 22624
  • [6] Demonstration of 10+hour energy storage with φ1′′ laboratory size solid oxide iron-air batteries
    Tang, Qiming
    Zhang, Yongliang
    Xu, Nansheng
    Lei, Xueling
    Huang, Kevin
    ENERGY & ENVIRONMENTAL SCIENCE, 2022, 15 (11) : 4659 - 4671
  • [7] Proton-mediated energy storage in intermediate-temperature solid-oxide metal-air batteries
    Xu, Nansheng
    Zhang, Cuijuan
    Huang, Kevin
    JOURNAL OF MATERIALS CHEMISTRY A, 2018, 6 (42) : 20659 - 20662
  • [8] Integration of CaO/CaCO3-CaCl2 thermochemical energy storage system with solid oxide iron-air redox battery
    Mirmoghtadaei, Golshan
    Mehrpooya, Mehdi
    Mahmoudi, Mahdi
    Ganjali, Mohammad Reza
    ENERGY CONVERSION AND MANAGEMENT, 2023, 290
  • [9] Heat Balance in a Planar Solid Oxide Iron-Air Redox Battery: A Computational Analysis
    Jin, Xinfang
    Zhao, Xuan
    White, Ralph E.
    Huang, Kevin
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2015, 162 (08) : F821 - F833
  • [10] All-Solid-State Iron-Air Batteries: A Promising High-Temperature Battery Technology for Large-Scale Energy Storage
    Wang, Hao
    Sun, Bingqian
    Peng, Cheng
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2024, 171 (07)