Microscale investigations of the metal-dusting corrosion mechanism on mild steel

被引:3
|
作者
Schmid, B [1 ]
Walmsley, JC
Grong, O
Odegård, R
机构
[1] STATOIL, Oil & Gas Refining, Res Ctr, N-7005 Trondheim, Norway
[2] Norwegian Univ Sci & Technol, Dept Mat Technol & Electrochem, N-7491 Trondheim, Norway
[3] SINTEF, Mat Technol, N-7465 Trondheim, Norway
关键词
D O I
10.1007/s11661-003-0335-2
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The internal and external products from metal-dusting corrosion of a mild steel specimen have been investigated, with the intention of further exploring the corrosion reaction mechanism. Scanning electron microscopy (SEM) and transmission electron microscopy (TEM) have been employed. A section of a steel tube, which had been subjected to heavily corrosive attack under controlled conditions, was studied. Electron-transparent TEM samples from this specimen were observed in the cross-sectional and plan-view orientations of the corrosion interface. Deposit on the corroded surface contained amorphous carbon, graphitic crystalline carbon, and decomposition products. Supersaturated cementite is an intermediate reaction product and was present at the surface of the exposed alloy. Surface cementite was seen to decompose locally into the graphite, where graphite basal planes were oriented perpendicular to the cementite surface. Iron was transported through the graphite, and the mild steel disintegrated by continuous formation and disintegration of the surface cementite. The observations are discussed with reference to the prevailing model mechanism for metal-dusting corrosion.
引用
收藏
页码:345 / 354
页数:10
相关论文
共 50 条
  • [1] Microscale investigations of the metal-dusting corrosion mechanism on mild steel
    Bernd Schmid
    Rolf Ødegård
    John Charles Walmsley
    Øystein Grong
    Metallurgical and Materials Transactions A, 2003, 34 : 345 - 354
  • [2] Initiation of Metal-Dusting Pits and a Method to Mitigate Metal-Dusting Corrosion
    Z. Zeng
    K. Natesan
    Oxidation of Metals, 2006, 66 : 1 - 20
  • [3] Initiation of metal-dusting pits and a method to mitigate metal-dusting corrosion
    Zeng, Z.
    Natesan, K.
    OXIDATION OF METALS, 2006, 66 (1-2): : 1 - 20
  • [4] Metal-dusting corrosion of low-chromium steels
    Chun, CM
    Ramanarayanan, TA
    OXIDATION OF METALS, 2004, 62 (1-2): : 71 - 92
  • [5] METAL-DUSTING CORROSION IN COAL-GASIFICATION ENVIRONMENTS
    PERKINS, RA
    COONS, WC
    RADD, FJ
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1976, 123 (08) : C253 - C253
  • [6] CASE OF METAL-DUSTING
    CENTO, L
    METALLURGIA ITALIANA, 1973, 65 (06): : 343 - 348
  • [7] Metal-Dusting Corrosion of Low-Chromium Steels
    C. M. Chun
    T. A. Ramanarayanan
    Oxidation of Metals, 2004, 62 : 71 - 92
  • [8] Relationship of carbon crystallization to the metal-dusting mechanism of nickel
    Zeng, Z
    Natesan, K
    CHEMISTRY OF MATERIALS, 2003, 15 (04) : 872 - 878
  • [9] Corrosion resistance of a high-silicon alloy in metal-dusting environments
    Chun, C. M.
    Ramanarayanan, T. A.
    OXIDATION OF METALS, 2007, 67 (3-4): : 215 - 234
  • [10] Corrosion Resistance of a High-Silicon Alloy in Metal-Dusting Environments
    C. M. Chun
    T. A. Ramanarayanan
    Oxidation of Metals, 2007, 67 : 215 - 234