Sulfide stress cracking susceptibility of the heat-affected zone of an 9% Ni steel welded joint

被引:9
|
作者
Passos, Augusto Verissimo [1 ]
Cipriano Farias, Francisco Werley [1 ]
Pereira Moraes e Oliveira, Victor Hugo [1 ]
Goncalves Rios, Mara Cardoso [1 ]
Payao Filho, Joao da Cruz [1 ]
机构
[1] Fed Univ Rio de Janeiro UFRJ, Program Met & Mat Engn, BR-21941972 Rio De Janeiro, RJ, Brazil
关键词
Welding simulation; Heat-affected zone; Sour environment; Environment-assisted cracking; Slow strain rate testing; FRACTURE CHARACTERISTICS; MECHANICAL-PROPERTIES; RETAINED AUSTENITE; HYDROGEN; BEHAVIOR; TRANSFORMATION; METHODOLOGY; CORROSION;
D O I
10.1016/j.conbuildmat.2021.122573
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
A 9% Ni steel (ASTM A333 Gr. 8) was selected for the first time for use in CO2 injection units (CO2-IUs) in the Brazilian pre-salt; however, because of the presence of H2S, it is susceptible to sulfide stress cracking (SSC), especially in welded joints. In this regard, the susceptibility to SSC of the subzones of the heat-affected zone (HAZ) of a 9% Ni steel (BM) welded pipe joint was evaluated. The thermal cycles of the HAZ were simulated numerically and physically. HAZ subzones were evaluated through optical micro-scopy, scanning electron microscopy, X-ray diffraction, Vickers microhardness, and slow strain rate testing. The BM and subcritical HAZ showed similar microstructures (fine ferrite and carbide/retained austenite (gamma(ret)) aggregates) and behaviors in aggressive environment, with plastic elongation ratios (REs) of 0.15 and 0.17, respectively. The intercritical HAZ (ICHAZ; fine ferrite and martensite) had the highest microhardness and gamma(ret) content, with a decrease in RE (0.04); fine-grain HAZ (FGHAZ; martensite and bainite) showed the smallest RE (0.01) and brittle fracture. The coarse-grain HAZ (CGHAZ; coarse martensite and coalesced bainite) showed the lowest plastic region and brittle fracture, with RE of 0.05 and the highest time-to-failure ratio. The high microhardness of the ICHAZ, FGHAZ, and CGHAZ (>250 HV, NACE 0175 / ISO 15156) made them more susceptible to SSC than the BM. These results lead to the conclusion that both the 9% Ni steel and its welded joints are prone to SSC, and the use of this steel in CO2-IUs presents an operational failure risk. (C) 2021 Elsevier Ltd. All rights reserved.
引用
收藏
页数:16
相关论文
共 50 条
  • [1] Sulfide stress cracking susceptibility of the heat-affected zone of an 9% Ni steel welded joint
    Veríssimo Passos, Augusto
    Farias, Francisco Werley Cipriano
    Moraes e Oliveira, Victor Hugo Pereira
    Rios, Mara Cardoso Gonçalves
    Payão Filho, João da Cruz
    Veríssimo Passos, Augusto (augusto.verissimo@poli.ufrj.br), 1600, Elsevier Ltd (282):
  • [2] HEAT-AFFECTED ZONE CRACKING IN WELDED TRANSMISSION POLES
    HERRSCHAFT, DC
    WATSON, PD
    MATERIALS EVALUATION, 1975, 33 (06) : 121 - 127
  • [3] Microstructural characterization of the physical simulated and welded heat-affected zone of 9% Ni steel pipe
    Rios, Mara Cardoso Goncalves
    Payao Filho, Joao da Cruz
    Farias, Francisco Werley Cipriano
    Passos, Augusto Verissimo
    Moraes e Oliveira, Victor Hugo Pereira
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2022, 17 : 3033 - 3046
  • [4] Case Study: Pitting and Stress Corrosion Cracking in Heat-Affected Zone of Welded Underground 304 Stainless Steel Pipe
    Tawancy, H. M.
    Al-Hadhrami, Luai M.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2012, 21 (08) : 1757 - 1762
  • [5] Case Study: Pitting and Stress Corrosion Cracking in Heat-Affected Zone of Welded Underground 304 Stainless Steel Pipe
    H. M. Tawancy
    Luai. M. Al-Hadhrami
    Journal of Materials Engineering and Performance, 2012, 21 : 1757 - 1762
  • [6] Microstructural Characterization of the Simulated Heat-Affected Zone of 9 Pct Ni Steel
    Rios, Mara Cardoso Goncalves
    Payao Filho, Joao da Cruz
    Farias, Francisco Werley Cipriano
    Oliveira, Victor Hugo Pereira Moraes e
    Passos, Augusto Verissimo
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2021, 52 (11): : 5016 - 5031
  • [7] Microstructural Characterization of the Simulated Heat-Affected Zone of 9 Pct Ni Steel
    Mara Cardoso Gonçalves Rios
    João da Cruz Payão Filho
    Francisco Werley Cipriano Farias
    Victor Hugo Pereira Moraes e Oliveira
    Augusto Veríssimo Passos
    Metallurgical and Materials Transactions A, 2021, 52 : 5016 - 5031
  • [8] STRESS CORROSION CRACKING AND ITS MECHANISM OF 16Mn STEEL AND HEAT-AFFECTED ZONE IN ALKALINE SULFIDE SOLUTIONS
    Hao Wenkui
    Liu Zhiyong
    Li Xiaogang
    Du Cuiwei
    ACTA METALLURGICA SINICA, 2013, 49 (07) : 881 - 889
  • [9] HEAT TREATMENT OF WELDED JOINT OF TUBES WITH LOCAL HEATING OF JOINT AND HEAT-AFFECTED ZONE
    BOGATOV, NA
    SHALGIN, AF
    TSVETAEV, RA
    TARASOV, VV
    STAL IN ENGLISH-USSR, 1968, (10): : 878 - +
  • [10] Heat-affected zone cracking susceptibility in high nitrogen-containing austenitic stainless steel
    Woo, I
    Horinouchi, T
    Kikuchi, Y
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2001, 87 (07): : 486 - 493