Synthesis and sintering of TiB2 nanoparticles

被引:45
|
作者
Rabiezadeh, A. [1 ]
Hadian, A. M. [2 ]
Ataie, A. [2 ]
机构
[1] Islamic Azad Univ, Shiraz Branch, Dept Mat Engn, Coll Chem & Mat Engn, Shiraz, Iran
[2] Univ Tehran, Coll Engn, Sch Met & Mat Engn, Tehran, Iran
关键词
Sol-gel processes; Sintering; Electron microscopy; TiB2; TITANIUM DIBORIDE; MECHANICAL-PROPERTIES; SILICON-NITRIDE; TEMPERATURE; ROUTE; DENSIFICATION; REDUCTION;
D O I
10.1016/j.ceramint.2014.07.102
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Titanium diboride nanoparticles were prepared from TTIP and boron oxide using a sol-gel method followed by mechano-chemical reduction in the presence of aluminum. Optimum weight ratio of B2O3:TTIP:2-propanol was 1:3:60. The XRD results revealed that mechano-chemical reduction of the zerogel by aluminum had led to the formation of TiB2 and Al2O3 phases after 15 hours of milling. The XRD results confirmed complete removal of Al2O3 via leaching the milled sample in 10 M NaOH at 150 degrees C. SEM and TEM studies showed that the mean particle size of the synthesized TiB2 is less than 30 nm. The densification experiments were carried out using hot pressing and pressureless sintering. The binderless densification of monolithic TiB2 up to 92% theoretical density was achieved by hot pressing at 1700 degrees C for 2 h in vacuum. The hot pressed TiB2 exhibits high Vickers hardness (25.9 GPa) and relative high fracture toughness (5.7 MPa.m(1/2)). In the pressureless sintering route, a maximum density of 82.3% NI, is achieved after sintering at 1900 degrees C for 2 h in vacuum. (C) 2014 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
引用
收藏
页码:15775 / 15782
页数:8
相关论文
共 50 条
  • [1] Sintering of TiB2 with Polycarbosilane
    Lee, Kwang Jung
    Kang, Shin Hyuk
    Kim, Deug Joong
    JOURNAL OF THE KOREAN CERAMIC SOCIETY, 2005, 42 (08) : 588 - 592
  • [2] Synthesis and sintering of TiB2 and TiB2-TiC composite under high pressure
    Bhaumik, SK
    Divakar, C
    Singh, AK
    Upadhyaya, GS
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2000, 279 (1-2): : 275 - 281
  • [3] Wet chemistry and combustion synthesis of nanoparticles of TiB2
    Axelbaum, R.L.
    Bates, S.E.
    Buhro, W.E.
    Frey, C.
    Kelton, K.F.
    Lawton, S.A.
    Rosen, L.J.
    Sastry, S.M.
    Nanostructured Materials, 1993, 2 (02):
  • [4] Influence of milling mechanism on synthesis of TiB2 and TiB/TiB2 composites
    Wexler, D
    Fenwick, A
    Calka, A
    METASTABLE, MECHANICALLY ALLOYED AND NANOCRYSTALLINE MATERIALS, 2003, : 199 - 204
  • [5] PROCESSING AND SINTERING OF SUBMICROMETER TIB2 POWDERS
    FINCH, CB
    BAIK, S
    BLEIER, A
    BECHER, PF
    AMERICAN CERAMIC SOCIETY BULLETIN, 1984, 63 (08): : 991 - 991
  • [6] Preparation and sintering of ultrafine TiB2 powders
    Ma, Li
    Yu, Jincheng
    Guo, Xue
    Xie, Bingying
    Gong, Hongyu
    Zhang, Yujun
    Zhai, Yanxia
    Wu, Xiuzheng
    CERAMICS INTERNATIONAL, 2018, 44 (04) : 4491 - 4495
  • [7] Pulsed electric current, in situ synthesis and sintering of textured TiB2 ceramics
    Ran, Songlin
    Zhang, Li
    Van der Biest, Omer
    Vleugels, Jef
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2010, 30 (04) : 1043 - 1047
  • [8] Rapid synthesis of TiB2/Fe composite in situ by spark plasma sintering
    Binghong Li
    Ying Liu
    Hui Cao
    Lin He
    Jun Li
    Journal of Materials Science, 2009, 44 : 3909 - 3912
  • [9] Rapid synthesis of TiB2/Fe composite in situ by spark plasma sintering
    Li, Binghong
    Liu, Ying
    Cao, Hui
    He, Lin
    Li, Jun
    JOURNAL OF MATERIALS SCIENCE, 2009, 44 (14) : 3909 - 3912
  • [10] Facile synthesis of 10 nm surface clean TiB2 nanoparticles
    Javadi, Abdolreza
    Pan, Shuaihang
    Cao, Chezheng
    Yao, Gongcheng
    Li, Xiaochun
    MATERIALS LETTERS, 2018, 229 : 107 - 110