Development of a thin ceramic-graphene nanolaminate coating for corrosion protection of stainless steel

被引:95
|
作者
Mondal, Jayanta [1 ]
Marques, Andreia [2 ,3 ]
Aarik, Lauri [1 ]
Kozlova, Jekaterina [1 ]
Simoes, Alda [2 ,3 ]
Sammelselg, Vaeino [1 ,4 ]
机构
[1] Univ Tartu, Inst Phys, Ravila 14c, EE-50411 Tartu, Estonia
[2] Univ Lisbon, Inst Super Tecn, CQE, Av Rovisco Pais, P-1049001 Lisbon, Portugal
[3] Univ Lisbon, Inst Super Tecn, Dept Chem Engn, Av Rovisco Pais, P-1049001 Lisbon, Portugal
[4] Univ Tartu, Inst Chem, Ravila 14a, EE-50411 Tartu, Estonia
关键词
Stainless steel; EIS; SEM; Amorphous structures; Oxide coatings; Passive films; ATOMIC LAYER DEPOSITION; ELECTROCHEMICAL IMPEDANCE SPECTROSCOPY; OPTICAL-PROPERTIES; PASSIVE FILM; TIO2; FILMS; AISI; 316L; BEHAVIOR; OXIDE; RESISTANCE; OXIDATION;
D O I
10.1016/j.corsci.2016.01.013
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A nanometric (thickness <= 200 nm) composite hybrid coating consisting of alternating laminate layers of aluminium and titanium oxides deposited by atomic layer deposition (ALD) onto a thin graphene layer of reduced graphene oxide (rGO) nanoplatelets applied on AISI 304 stainless steel, was developed and its electrochemical properties were studied. The rGO by itself has not revealed significant effects in terms of protection, whereas the laminate reinforced the passivity by decreasing the passive current. The best performance was obtained by the complete system, in which the rGO film acts as a primer for the anchoring of the ceramic layer, as a barrier for corrosive ions, and as a shield for local electrical fields if these are generated by starting local corrosion, thus, decreases the tendency to metastable pitting. (C) 2016 Elsevier Ltd. All rights reserved.
引用
收藏
页码:161 / 169
页数:9
相关论文
共 50 条
  • [1] Development and Evaluation of a Thin Cerium Oxide-Gelatin Nanolaminate Coating for Corrosion Protection of AISI 316L Stainless Steel
    Hayajneh, Mohammed T.
    Almomani, Mohammed
    Al-Daraghmeh, Mohammad
    MANUFACTURING TECHNOLOGY, 2021, 21 (03): : 330 - 339
  • [2] Corrosion protection of stainless steel in molten carbonate by a ceramic coating
    Au, SF
    Keijzer, M
    Hemmes, K
    van derPut, PJJM
    de Wit, JHW
    Schoonman, J
    ELECTROCHEMICAL METHODS IN CORROSION RESEARCH VI, PTS 1 AND 2, 1998, 289-2 : 699 - 706
  • [3] Zirconia-alumina nanolaminate for perforated pitting corrosion protection of stainless steel
    Gaertner, WF
    Hoppe, EE
    Omari, MA
    Sorbello, RS
    Aita, CR
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A, 2004, 22 (02): : 272 - 280
  • [4] Corrosion protection of stainless steel by electropolymerised pani coating
    Sathiyanarayanan, S.
    Devi, S.
    Venkatachari, G.
    PROGRESS IN ORGANIC COATINGS, 2006, 56 (2-3) : 114 - 119
  • [5] Corrosion protection of Cr-Cu alloy coating on stainless steel
    Vatani, Razieh
    Zamani-Meymian, Mohammad-Reza
    Ghaffarinejad, Ali
    Khalilzadeh, Shaghayegh
    SURFACE & COATINGS TECHNOLOGY, 2023, 474
  • [6] Effect of ceramic particles on corrosion resistance of thermal sprayed stainless steel coating
    Quan, Tang
    Suo-de, Zhang
    Min, Xu
    Jian-qiang, Wang
    CAILIAO GONGCHENG-JOURNAL OF MATERIALS ENGINEERING, 2021, 49 (11): : 125 - 135
  • [7] Pitting corrosion protection of stainless steel by sputter deposited hafnia, alumina, and hafnia-alumina nanolaminate films
    Almomani, M. A.
    Aita, C. R.
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A, 2009, 27 (03): : 449 - 455
  • [8] Improved Corrosion Protection of Stainless Steel by Two Dimensional BN Nanomaterial Coating
    Duran, Berrin
    Pat, Suat
    ECS JOURNAL OF SOLID STATE SCIENCE AND TECHNOLOGY, 2022, 11 (06)
  • [9] Alumina nanostructured coating for corrosion protection of 316L stainless steel
    Doodman, P.
    Faghihi-Sani, M. A.
    Barati, N.
    Afshar, A.
    INTERNATIONAL JOURNAL OF NANO DIMENSION, 2014, 5 (01) : 27 - 33
  • [10] Investigation of Tribological Behavior of Ceramic-Graphene Composite Coating Produced by Plasma Electrolytic Oxidation
    Vatan, H. Nasiri
    Adabi, M.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2018, 71 (07) : 1643 - 1652