High-temperature thermal stability of Hi-Nicalon™ SiC fiber/SiC matrix composites under long term cyclic heating

被引:14
|
作者
Takeda, M
Imai, Y
Kagawa, Y
Guo, SQ
机构
[1] Nippon Carbon Co Ltd, Res Lab, Kanagawa Ku, Yokohama, Kanagawa 2210031, Japan
[2] Univ Tokyo, Inst Ind Sci, Minato Ku, Tokyo 1068558, Japan
关键词
D O I
10.1016/S0921-5093(00)00820-0
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The high-temperature thermal stability of C-coated standard grade Nicalon(TM) SIC fiber and of C or BN-coated Hi-Nicalon(TM) SiC fiber-reinforced SiC matrix composites under long-term cyclic heat exposure in air has been studied. Woven fabric composites fabricated by the PIP process were cyclic heat-exposed at 1273 and 1673 K for up to 1000 h with one heat exposure cycle of 200 h. The degradation of the composites was evaluated by a three-point flexure test at room temperature. The oxidation of the composite occurred from the matrix phase due to the existence of macro- and micro-pores that exist in the matrix. Degradation of the strength was observed for the C-coated SiC fiber/SiC composites after heat exposure for 200 h at 1273 K. On the contrary, the BN-coated Hi-Nicalon(TM) SiC fiber/SiC composite showed only a slight degradation even after a 1000-h exposure at 1273 K. However, at 1673 K, this composite's strength degraded after an 800-h exposure. (C) 2000 Elsevier Science S.A. All rights reserved.
引用
收藏
页码:312 / 323
页数:12
相关论文
共 50 条
  • [1] Thermal stability of CVI and MI SiC/SiC composites with Hi-Nicalon™-S fibers
    Bhatt, R. T.
    Sola-Lopez, F.
    Halbig, M. C.
    Jaskowiak, M. H.
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2022, 42 (08) : 3383 - 3394
  • [2] High-temperature interlaminar shear strength of Hi-Nicalon™ fiber-reinforced MI-SiC matrix composites with BN/SiC fiber coating
    Lara-Curzio, E
    Singh, M
    [J]. JOURNAL OF MATERIALS SCIENCE LETTERS, 2000, 19 (08) : 657 - 661
  • [3] RECENT DEVELOPMENTS OF THE SIC FIBER NICALON AND ITS COMPOSITES, INCLUDING PROPERTIES OF THE SIC FIBER HI-NICALON FOR ULTRA-HIGH TEMPERATURE
    ISHIKAWA, T
    [J]. COMPOSITES SCIENCE AND TECHNOLOGY, 1994, 51 (02) : 135 - 144
  • [4] Thermal stability of SiO2-coated SiC fiber (Hi-Nicalon) under argon atmosphere
    T. Shimoo
    K. Okamura
    F. Toyoda
    [J]. Journal of Materials Science, 2000, 35 : 3811 - 3816
  • [5] Thermal stability of SiO2-coated SiC fiber (Hi-Nicalon) under argon atmosphere
    Shimoo, T
    Okamura, K
    Toyoda, F
    [J]. JOURNAL OF MATERIALS SCIENCE, 2000, 35 (15) : 3811 - 3816
  • [6] Microstructure and mechanical properties of SiC fiber "Hi-Nicalon Type S" reinforced SiC composites
    Urano, A
    Sakamoto, J
    Takeda, M
    Imai, Y
    Araki, H
    Noda, T
    [J]. 22ND ANNUAL CONFERENCE ON COMPOSITES, ADVANCED CERAMICS, MATERIALS, AND STRUCTURES: A, 1998, 19 (03): : 55 - 63
  • [7] Room temperature tensile behavior and damage accumulation of Hi-Nicalon reinforced SiC matrix composites
    Morscher, GN
    Gyekenyesi, JZ
    [J]. 22ND ANNUAL CONFERENCE ON COMPOSITES, ADVANCED CERAMICS, MATERIALS, AND STRUCTURES: A, 1998, 19 (03): : 241 - 249
  • [8] Thermal stability of low-SiC fiber (Hi-Nicalon) treated in a hot isostatic press
    Shimoo, T
    Tsukada, I
    Seguchi, T
    Okamura, K
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1999, 82 (12) : 3508 - 3512
  • [9] ETS-synthesized Hi-Nicalon fiber-SiC matrix composite
    Yang, W
    Araki, H
    Kohyama, A
    Suzuki, H
    Noda, T
    [J]. CERAMICS INTERNATIONAL, 2005, 31 (01) : 47 - 52
  • [10] The effect of high-temperature annealing on tensile strength and its mechanism of Hi-Nicalon SiC fibres under inert atmosphere
    Yao, R. Q.
    Wang, Y. Y.
    Feng, Z. D.
    [J]. FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2008, 31 (09) : 777 - 787