Phase Stability of Low-Density, Multiprincipal Component Alloys Containing Aluminum, Magnesium, and Lithium

被引:207
|
作者
Yang, X. [1 ]
Chen, S. Y. [1 ]
Cotton, J. D. [2 ]
Zhang, Y. [1 ]
机构
[1] Univ Sci & Technol Beijing, High Entropy Theory Ctr, State Key Lab Adv Met & Mat, Beijing 100083, Peoples R China
[2] Boeing Co, Metall Mat Grp, Seattle, WA 98124 USA
关键词
HIGH-ENTROPY ALLOYS; SOLID-SOLUTION PHASE; PROPERTIES OPTIMIZATION; MICROSTRUCTURE; BEHAVIOR; DESIGN;
D O I
10.1007/s11837-014-1059-z
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A series of low-density, multiprincipal component alloys containing high concentrations of Al, Mg, Li, Zn, Cu and/or Sn was designed using a strategy based on high-entropy alloys (HEAs). The alloys were prepared by induction melting under high-purity argon atmosphere, and the resulting microstructures were characterized in the as-cast condition. The resulting microstructures are multiphase and complex and contain significant volume fractions of disordered solutions and intermetallic compounds. By analyzing the atomic size difference, enthalpy of mixing, entropy of mixing, electronegativity difference, and valence electron concentration among the constituent elements, modified phase formation rules are developed for low-density multiprincipal component alloys that are more restrictive than previously established limits based on more frequently studied HEAs comprising mostly transition metals. It is concluded that disordered solid solution phases are generally less stable than competing ordered compounds when formulated from low-density elements including Al, Mg, and Li.
引用
收藏
页码:2009 / 2020
页数:12
相关论文
共 50 条
  • [1] Phase Stability of Low-Density, Multiprincipal Component Alloys Containing Aluminum, Magnesium, and Lithium
    X. Yang
    S. Y. Chen
    J. D. Cotton
    Y. Zhang
    JOM, 2014, 66 : 2009 - 2020
  • [2] Erratum to: Phase Stability of Low-Density, Multiprincipal Component Alloys Containing Aluminum, Magnesium, and Lithium
    X. Yang
    S. Y. Chen
    J. D. Cotton
    Y. Zhang
    JOM, 2015, 67 : 1393 - 1396
  • [3] Phase Stability of Low-Density, Multiprincipal Component Alloys Containing Aluminum, Magnesium, and Lithium (vol 66, pg 2009, 2014)
    Yang, X.
    Chen, S. Y.
    Cotton, J. D.
    Zhang, Y.
    JOM, 2015, 67 (06) : 1393 - 1396
  • [4] Aluminum alloys containing lithium and magnesium
    Fridlyander, I.N.
    Metallovedenie i Termicheskaya Obrabotka Metallov, 2003, (09): : 13 - 16
  • [5] ALUMINUM-LITHIUM ALLOYS - LOW-DENSITY AND HIGH STIFFNESS
    SANDERS, TH
    BALMUTH, ES
    METAL PROGRESS, 1978, 113 (03): : 32 - 37
  • [6] Some new characteristics of the strengthening phase in β-phase magnesium-lithium alloys containing aluminum and beryllium
    Song, GS
    Staiger, M
    Kral, M
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 371 (1-2): : 371 - 376
  • [7] OXIDATION BEHAVIOR OF ALUMINUM-ALLOYS CONTAINING MAGNESIUM AND LITHIUM
    CSANADY, A
    KURTHY, J
    JOURNAL OF MATERIALS SCIENCE, 1981, 16 (10) : 2919 - 2922
  • [8] PRECIPITATION CHARACTERISTICS OF ALUMINUM-LITHIUM ALLOYS CONTAINING MAGNESIUM
    THOMPSON, GE
    NOBLE, B
    JOURNAL OF THE INSTITUTE OF METALS, 1973, 101 (APR): : 111 - 115
  • [9] Aluminum Alloys with Lithium and Magnesium
    I. N. Fridlyander
    Metal Science and Heat Treatment, 2003, 45 : 344 - 347
  • [10] Aluminum alloys with lithium and magnesium
    Fridlyander, IN
    METAL SCIENCE AND HEAT TREATMENT, 2003, 45 (9-10) : 344 - 347