Dry sliding wear behavior of low carbon dual phase powder metallurgy steels

被引:25
|
作者
Tekeli, S. [1 ]
Gural, A.
Ozyurek, D.
机构
[1] Gazi Univ, Tech Educ Fac, Div Mat, TR-06500 Ankara, Turkey
[2] Zonguldak Karaelmas Univ, Karabuk Tech Educ Fac, Casting Div, TR-078100 Karabuk, Turkey
来源
MATERIALS & DESIGN | 2007年 / 28卷 / 05期
关键词
D O I
10.1016/j.matdes.2006.03.013
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Dry sliding wear behavior of Fe + 0.3% graphite powder metallurgy processed (PM) steels was investigated at constant sliding speed, load and distance. For this purpose, atomized iron powder was mixed with 0.3% graphite powder and sintered at 1200 degrees C for 30 min under Argon gas atmosphere. The sintered PM specimens were intercritically annealed at different temperatures (728 and 760 degrees C) and then water-quenched. After sintering, a typical ferrite + pearlite microstructure was obtained. In the microstructure of the intercritically annealed PM specimens, a ferrite + martensite microstructure was produced. After wear tests, it was seen that the wear rate of the intercritically annealed specimens was very low in comparison to as-sintered specimen. The specimen intercritically annealed at 728 degrees C showed the lowest wear rate, despite its lower martensite volume fraction. (c) 2006 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1685 / 1688
页数:4
相关论文
共 50 条
  • [1] Influence of martensite particle size on dry sliding wear behaviour of low carbon dual phase powder metallurgy steels
    Gural, A.
    KOVOVE MATERIALY-METALLIC MATERIALS, 2010, 48 (01): : 25 - 31
  • [2] Dry Sliding Wear Behavior of Powder Metallurgy Aluminium Matrix Composite
    Ganesh, R.
    Subbiah, Ram
    Chandrasekaran, K.
    MATERIALS TODAY-PROCEEDINGS, 2015, 2 (4-5) : 1441 - 1449
  • [3] The role of heat treatment on wear behavior of powder metallurgy low alloy steels
    Khorsand, H
    Habibi, SM
    Yoozbashizadea, H
    Janghorban, K
    Reihani, SMS
    Seraji, HR
    Ashtari, M
    MATERIALS & DESIGN, 2002, 23 (07): : 667 - 670
  • [4] The role of heat treatment on wear behavior of powder metallurgy low alloy steels
    Khorsand, H
    Habibi, M
    Ashtari, M
    Yoozbashizadeh, H
    POWDER METALLURGY IN AUTOMOTIVE APPLICATIONS-II, 2002, : 197 - 201
  • [5] Dry Sliding Wear Behavior of Sintered Copper-Diamond Composite Fabricated by Powder Metallurgy
    Zheng, RunGuo
    Zhan, ZaiJi
    Peng, XiaoTing
    Wang, WenKui
    MANUFACTURING ENGINEERING AND AUTOMATION I, PTS 1-3, 2011, 139-141 : 335 - 339
  • [6] Investigation of Dry Sliding Wear Behavior of Pack Boriding Fe-Based Powder Metallurgy
    Fang, Huimin
    Xu, Feng
    Zhang, Guangsheng
    INTEGRATED FERROELECTRICS, 2020, 208 (01) : 67 - 82
  • [7] Dry sliding oxidative wear in plain carbon dual phase steel
    Abouei, V.
    Saghafian, H.
    Kheirandish, Sh
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2007, 14 (04) : 43 - 48
  • [8] Dry sliding friction and wear in plain carbon dual phase steel
    Tyagi, R
    Nath, SK
    Ray, S
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2001, 32 (02): : 359 - 367
  • [9] Dry Sliding Oxidative Wear in Plain Carbon Dual Phase Steel
    V. Abouei
    H. Saghafian
    Sh. Kheirandish
    Journal of Iron and Steel Research International, 2007, 14 : 43 - 48
  • [10] Dry Sliding Oxidative Wear in Plain Carbon Dual Phase Steel
    V Abouei
    H Saghafian
    Sh Kheirandish
    Journal of Iron and Steel Research(International), 2007, (04) : 43 - 48