Shear Bond Strength of Lithium Disilicate to Resin Cement After Treatment with Hydrofluoric Acid and a Self-etching Ceramic Primer

被引:0
|
作者
Pinto Klippel, Gesinete Goncalves [1 ]
de Melo-Silva, Claudio Luis [2 ]
Favieri de Melo-Silva, Tereza Cristina [2 ]
Elias, Carlos Nelson [3 ]
de Biasi, Ronaldo Sergio [3 ]
dos Santos, Claudinei [4 ]
机构
[1] Univ Fed Fluminense UFF, Escola Engn Ind Met Volta Redonda EEIMVR, Av Trabalhadores 420, BR-27255125 Volta Redonda, RJ, Brazil
[2] Ctr Univ Volta Redonda UniFOA, Ave Paulo Erlei Alves Abrantes 1325, Volta Redonda, RJ, Brazil
[3] Inst Mil Engn IME, Dept Ciencia Mat, Pr Gen Tiburcio 80, BR-22290270 Rio De Janeiro, RJ, Brazil
[4] Univ Estado Rio de Janeiro UERJ, Fac Tecnol Resende FAT, Rodovia Presidente Dutra,Km 298, BR-27537000 Resende, RJ, Brazil
关键词
Lithium disilicate; Li2Si2O5; shear bond strength; hydrofluoric acid; self-etching ceramic primer; DENTAL APPLICATIONS; UNIVERSAL ADHESIVE; SURFACE-TREATMENT; RELIABILITY; EVOLUTION; PROTOCOLS; BEHAVIOR;
D O I
10.1590/1980-5373-MR-2021-0079
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The aim of this work was to analyze the properties and shear bond strength (SBS) of lithium disilicate to resin cement before and after etching the glass-ceramic surfaces. Lithium-metasilicate samples were heat treated and characterized by Scanning Electron Microscopy, X-ray diffraction and roughness measurement. For the analysis of the shear bonding strength (SBS) of lithium disilicate to dental resin cement, three groups (n = 12) of Li2Si2O5 were prepared: 1 degrees)without treatment (NT); 2 degrees)surface etching with hydrofluoric acid(HF), followed by silane agent and adhesive treatment; 3 degrees) surface treatment with a self-etching ceramic primer (SECP). After the heat-treatment, the samples had Li2Si2O5 crystalline phase dispersed in a residual amorphous phase. Roughness of the NT and SECP samples was smaller that of the HF samples. Samples without surface treatment (NT) had the lowest SBS (5.5MPa). HF(24.2MPa) and SECP(24.8MPa) samples has similar SBS. Weibull statistics showed that HF-samples are more reliable than NT and SECP. The SBS was significantly increased by either HF etching and SECP surface treatment. While the chemical characteristics of the surface submitted to SECP treatment are considered to be responsible for the SBS increase, the main adhesion mechanism after HF etching is the increase in surface roughness.
引用
收藏
页数:11
相关论文
共 50 条
  • [1] The effect of hydrofluoric acid and resin cement formulation on the bond strength to lithium disilicate ceramic
    Sundfeld, Daniel
    Muniz Palialol, Alan Rodrigo
    Fugolin, Ana Paula Piovesan
    Bovi Ambrosano, Glaucia Maria
    Correr-Sobrinho, Lourenco
    Marcondes Martins, Luis Roberto
    Pfeifer, Carmem Silvia
    BRAZILIAN ORAL RESEARCH, 2018, 32
  • [2] Durability of Resin Bonding to Lithium Disilicate and Zirconia Ceramic using a Self-etching Primer
    Wille, Sebastian
    Lehmann, Frank
    Kern, Matthias
    JOURNAL OF ADHESIVE DENTISTRY, 2017, 19 (06): : 491 - 496
  • [3] Effect of self etching ceramic primer and universal adhesive on bond strength of lithium disilicate ceramic
    Alrahlah, Ali
    Awad, Mohamed M.
    Vohra, Fahim
    Al-Mudahi, Abdulellah
    Al Jeaidi, Zaid A.
    Elsharawy, Mohamed
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2017, 31 (23) : 2611 - 2619
  • [4] Effect of Hydrofluoric Acid Concentration and Etching Time on Bond Strength to Lithium Disilicate Glass Ceramic
    Puppin-Rontani, J.
    Sundfeld, D.
    Costa, A. R.
    Correr, A. B.
    Puppin-Rontani, R. M.
    Borges, G. A.
    Sinhoreti, M. A. C.
    Correr-Sobrinho, L.
    OPERATIVE DENTISTRY, 2017, 42 (06) : 606 - 615
  • [5] Etching efficacy and bonding performance of resin to lithium disilicate ceramic using self-etching primer with different reaction times
    Alshihri, Abdulmonem
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2019, 33 (11) : 1215 - 1225
  • [6] Thermocycling effects on shear bond strength of a self-etching primer
    Elekdag-Turk, Selma
    Turk, Tamer
    Isci, Devrim
    Ozkalayci, Nurhat
    ANGLE ORTHODONTIST, 2008, 78 (02) : 351 - 356
  • [7] The effect of several dentin desensitizers on shear bond strength of adhesive resin luting cement using self-etching primer
    Huh, Jung-Bo
    Kim, Jee-Hwan
    Chung, Moon-Kyu
    Lee, Ho-Yong
    Choi, Yong-Geun
    Shim, June-Sung
    JOURNAL OF DENTISTRY, 2008, 36 (12) : 1025 - 1032
  • [8] Surface Treatment Effect on Shear Bond Strength between Lithium Disilicate Glass-Ceramic and Resin Cement
    Simasetha, Siripan
    Klaisiri, Awiruth
    Sriamporn, Tool
    Sappayatosok, Kraisorn
    Thamrongananskul, Niyom
    EUROPEAN JOURNAL OF DENTISTRY, 2022, 16 (02) : 373 - 380
  • [9] Self-etching ceramic primer versus hydrofluoric acid etching: Etching efficacy and bonding performance
    El-Damanhoury, Hatem M.
    Gaintantzopoulou, Maria D.
    JOURNAL OF PROSTHODONTIC RESEARCH, 2018, 62 (01) : 75 - 83
  • [10] Does a Self-etching Ceramic Primer Improve Bonding to Lithium Disilicate Ceramics? Bond Strengths and FESEM Analyses
    Lopes, G. C.
    Perdigao, J.
    Baptista, D.
    Ballarin, A.
    OPERATIVE DENTISTRY, 2019, 44 (02) : 210 - 218