Evaluation of cold crack susceptibility on HSLA steel welded joints

被引:3
|
作者
Silverio-Freire, RC [1 ]
Moura-Maciel, T
da Silva, PG
机构
[1] Univ Fed Rio Grande do Norte, Ctr Exact Sci & Earth, Program Doctorate Sci & Engn Mat, BR-59072970 Natal, RN, Brazil
[2] Univ Fed Paraiba, Ctr Sci & Technol, Dept Mech Engn, BR-58109970 Campina Grande, Paraiba, Brazil
关键词
cold cracking; HSLA steels; microstructure; Tekken tests;
D O I
10.3989/revmetalm.2003.v39.i2.318
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The present study addresses an evaluation of the effect of several welding parameters on cold cracking formation in welded joints of High Strength and Low Alloy steels, as well as the resulting microstructures and hardness values. The main parameters studied include the variation of the preheating temperature, drying time of the electrode, chemical composition and thickness of the base metal. The presence of cold cracking in the joints was analyzed from Tekken tests using steel plates made of SAR 80 T, 100 T and 120 T with of various thickness. The plates were welded by Shielded Metal Arc Welding either with or without pre-heating. Different preheating temperatures were studied, i.e., 375, 455 and 525 K. AWS E 12018 G and 11018 G electrodes were used under different conditions, i.e., not dried or dried up to 2, 3 and 4 h at 515 K. The results indicated the presence of cracks in the welded metals with the combination of hardness values above 230 HV and the formation of high contents of acicular ferrite (above 93 %) in the welds without preheating. Higher crack susceptibility was also observed in the thick welded metal plates.
引用
收藏
页码:83 / 89
页数:7
相关论文
共 50 条
  • [1] Investigations on the impact toughness of HSLA steel arc welded joints
    Pamnani, Rishi
    Jayakumar, T.
    Vasudevan, M.
    Sakthivel, T.
    JOURNAL OF MANUFACTURING PROCESSES, 2016, 21 : 75 - 86
  • [2] CRACK INITIATION AND PROPAGATION RESISTANCE OF HSLA STEEL WELDED JOINT CONSTITUENTS
    Jovanovic, M.
    Camagic, I
    Sedmak, S. A.
    Zivkovic, P.
    Sedmak, A.
    STRUCTURAL INTEGRITY AND LIFE-INTEGRITET I VEK KONSTRUKCIJA, 2020, 20 (01): : 11 - 14
  • [3] DETERMINATION OF FATIGUE CRACK GROWTH PARAMETERS IN WELDED JOINT OF HSLA STEEL
    Milovic, Ljubica
    Vuherer, Tomaz
    Radakovic, Zoran
    Petrovski, Blagoj
    Jankovic, Miodrag
    Zrilic, Milorad
    Danicic, Darko
    STRUCTURAL INTEGRITY AND LIFE-INTEGRITET I VEK KONSTRUKCIJA, 2011, 11 (03): : 183 - 187
  • [4] Effect of temperature on the crack resistance of steel and of welded joints
    Troshchenko, V.T.
    Pokrovskii, V.V.
    Yarusevich, V.L.
    Yasnii, P.V.
    Timofeev, B.T.
    Varovin, A.Ya.
    Zakharchenko, V.V.
    Strength of materials, 1988, : 143 - 149
  • [5] Evaluation of fatigue crack growth in welded joints
    NRIM Research Activities, 1994,
  • [6] Research on microstructure and performance of welded joints of HSLA steel under vibration conditioning
    School of Materials Science and Engineering, Shenyang University of Technology, Shenyang
    110870, China
    不详
    110159, China
    Hanjie Xuebao, 1 (105-108):
  • [7] EXPERIMENTAL STUDY ON MAG WELDED E350 HSLA STEEL JOINTS
    Moorthy, S. Bradeesh
    Malayalamurthy, R.
    Amirthagadeswaran, K. S.
    MATERIALI IN TEHNOLOGIJE, 2024, 58 (02): : 209 - 215
  • [8] FE SIMULATION OF COLD CRACKING SUSCEPTIBILITY IN X70 STRUCTURAL STEEL WELDED JOINTS
    Olden, Vigdis
    Akselsen, Odd Magne
    OMAE2011: PROCEEDINGS OF THE ASME 30TH INTERNATIONAL CONFERENCE ON OCEAN, OFFSHORE AND ARCTIC ENGINEERING, VOL 3: MATERIALS TECHNOLOGY, 2011, : 445 - +
  • [9] Cooling Rate Control on Cold Cracking in Welded Thick HSLA Steel Plate
    Winarto
    Anis, Muhammad
    Taufiqullah
    MATERIALS MODELING, SIMULATION, AND CHARACTERIZATION, 2011, 689 : 269 - 275
  • [10] Fatigue crack initiation and subsequent crack growth in fillet welded steel joints
    Mikulski, Zbigniew
    Lassen, Tom
    INTERNATIONAL JOURNAL OF FATIGUE, 2019, 120 : 303 - 318