On Healing Mechanism of Cast Porosities in Cast Ni-Based Superalloy by Hot Isostatic Pressing

被引:6
|
作者
Yuan, Chao [1 ]
Li, Jie [1 ]
Dong, Kai-Xin [1 ]
Guo, Jian-Ting [1 ]
机构
[1] Chinese Acad Sci, Inst Mental Res, Shenyang 110016, Peoples R China
来源
关键词
Cast superalloy; Hot isostatic pressing; Porosity healing; Microstructure evolution; NICKEL-BASED SUPERALLOY; MICROSTRUCTURAL RESTORATION; DELTA PRECIPITATIONS; HIP TEMPERATURE; HEAT-TREATMENTS; EVOLUTION; GAMMA''; ALLOY; OM;
D O I
10.1007/978-3-319-52333-0_24
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
The purpose of this study is to evaluate the effects of hot isostatic pressing (HIP) on the porosity healing and the microstructure evolution of a cast superalloy K452, which is generally applied for fabrication the vanes with the bigger size. The annihilation degree of the porosity, related to the location and shape of the porosity as well as HIP temperature, were studied by high resolution transmission X-ray tomography (HRTXRT) and finite element method (FEM). Results showed that the most of porosities (over 80%) were eliminated by HIP at 1200 degrees C, in which the porosity located in the thin walled parts and with the loose-flat shape was easy to be healed, and the diameter of remnant porosities was decreased to less than 10 lm. Accordingly, A healing mode of the porosity was established. Furthermore, It was found that the slow cooling rate during HIP would obviously lead gamma' precipitates to coarsen, while the rejuvenation heat-treatment (RHT) after HIP could reduce the dendritic segregation degree and readjust the coarsen gamma' precipitates, which finally improved the mechanical properties of the cast superalloy. The HIPed K452 alloy vanes have been successfully used in a civil gas turbine.
引用
收藏
页码:265 / 275
页数:11
相关论文
共 50 条
  • [1] Hot isostatic pressing treatment of cast Ni-base superalloy
    Hu, H
    ACTA METALLURGICA SINICA, 2002, 38 (11) : 1199 - 1202
  • [2] Healing Process of Casting Pores in a Ni-based Superalloy by Hot Isostatic Pressing
    X.G.Zheng
    Y.-N.Shi
    L.H.Lou
    JournalofMaterialsScience&Technology, 2015, 31 (11) : 1151 - 1157
  • [3] Healing Process of Casting Pores in a Ni-based Superalloy by Hot Isostatic Pressing
    Zheng, X. G.
    Shi, Y. -N.
    Lou, L. H.
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2015, 31 (11) : 1151 - 1157
  • [4] Degeneration process and mechanism of primarymc carbides in a cast Ni-based superalloy
    Sun W.
    Qin X.
    Guo J.
    Lou L.
    Zhou L.
    Jinshu Xuebao/Acta Metallurgica Sinica, 2016, 52 (04): : 455 - 462
  • [5] HOT ISOSTATIC PRESSING OF PM AND CAST COMPONENTS
    STEPHENSON, DJ
    DOWNING, M
    MATERIALS AT HIGH TEMPERATURES, 1991, 9 (02) : 59 - 68
  • [6] The effect of hot isostatic pressing on cast aluminum
    Lei, CSC
    Frazier, WE
    Lee, EW
    JOM-JOURNAL OF THE MINERALS METALS & MATERIALS SOCIETY, 1997, 49 (11): : 38 - 39
  • [7] The effect of hot isostatic pressing on cast aluminum
    C. S. C. Lei
    W. E. Frazier
    E. W. Lee
    JOM, 1997, 49 : 38 - 39
  • [8] Microstructural Evolution of Creep-Induced Cavities and Casting Porosities for a Damaged Ni-based Superalloy Under Various Hot Isostatic Pressing Conditions
    Wang, Xiao-Meng
    Zhou, Yu
    Zhao, Zi-Hua
    Zhang, Zheng
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2015, 28 (05) : 628 - 633
  • [9] Microstructural Evolution of Creep-Induced Cavities and Casting Porosities for a Damaged Ni-based Superalloy Under Various Hot Isostatic Pressing Conditions
    Xiao-Meng Wang
    Yu Zhou
    Zi-Hua Zhao
    Zheng Zhang
    ActaMetallurgicaSinica(EnglishLetters), 2015, 28 (05) : 628 - 633
  • [10] Microstructural Evolution of Creep-Induced Cavities and Casting Porosities for a Damaged Ni-based Superalloy Under Various Hot Isostatic Pressing Conditions
    Xiao-Meng Wang
    Yu Zhou
    Zi-Hua Zhao
    Zheng Zhang
    Acta Metallurgica Sinica (English Letters), 2015, 28 : 628 - 633