Hot deformation behavior of Sc/Nb modified AA2195 Al-Li-Cu alloys

被引:11
|
作者
Singh, Gaurav [1 ]
Nayan, N. [2 ]
Murty, S. V. S. Narayana [2 ]
Yadava, Manasij [3 ]
Bajargan, Govind [2 ]
Mohan, M. [2 ]
机构
[1] 403,LS Bldg,Sanjaynagar, Bangalore 560090, India
[2] Vikram Sarabhai Space Ctr, Mat & Mech Ent, Trivandrum 695022, India
[3] Indian Inst Technol Kanpur, Dept Mat Sci & Engn, Kanpur 208016, India
关键词
Processing maps; Aluminium alloys; Superplasticity; Dynamic recrystallization; Flow curves; Age-hardening; SHAPE-MEMORY ALLOY; PROCESSING MAPS; MECHANICAL-PROPERTIES; MICROSTRUCTURAL EVOLUTION; INSTABILITY CRITERIA; TEMPORAL EVOLUTION; ALUMINUM-ALLOYS; SHEAR BANDS; STRAIN-RATE; MG ALLOY;
D O I
10.1016/j.msea.2022.143169
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The hot workability of third generation AA2195 (Al-Li-Cu-Ag-Mg-Zr) alloy with different Sc (0.15-0.25 wt%) and Nb (0.15-0.25 wt%) additions in the homogenized condition was investigated using processing maps approach. The additions of Sc and Nb were found to be beneficial in refining the as-cast grain size of AA2195 and changing the morphology from less dendritic grain structure to a globular or equiaxed form. Hot compression tests carried out in the temperature, T, range of 300-450 degrees C and strain rate, (epsilon)over dot, of 10(-3) - 10 s(-1) were utilized to generate processing maps at a true strain, epsilon = 0.5. The flow curves of the alloys exhibit a typical dynamic recovery (DRV) characteristics and Arrhenius type constitutive equations successfully predicted flow stress of the alloys. The results obtained from the processing maps and complementary microstructural analysis of the deformed specimens revealed that 0.15 wt% additions of Sc and Nb (separately or in combination) are optimum to improve its workability. However, increasing Sc and Nb contents to 0.25 wt% relatively expanded flow instability regions. With the aid of the processing maps, deformed specimens microstructural analysis, activation energy and Zener-Hollomon parameter, Domain D-3 occurring at higher temperatures and strain rates were identified as the "safe" regimes for hot working of AA2195 with optimum Sc and Nb contents (0.15 wt% added separately or in combination). Limited pancake type grain morphology with higher fractions of dynamically recrystallized (DRX) grains was observed in Domain D-3. The microstructural manifestation in the flow instability regions was flow localization (at higher strain rates), cavities formation at the grain boundaries & precipitates, particles breakage and wedge cracking at the triple junctions at lower strain rates.
引用
收藏
页数:20
相关论文
共 50 条
  • [1] Hot deformation behavior of Sc/Nb modified AA2195 Al–Li–Cu alloys
    Singh, Gaurav
    Nayan, N.
    Narayana Murty, S.V.S.
    Yadava, Manasij
    Bajargan, Govind
    Mohan, M.
    Materials Science and Engineering: A, 2022, 844
  • [2] Hot Compression Deformation Behavior and Microstructure of As-Cast and Homogenized AA2195 Al-Li Alloy
    Zhang, Jin
    Liu, Zemeng
    Shi, Dongfeng
    METALS, 2022, 12 (10)
  • [3] Weld Solidification Cracking Behaviour of AA2195 Al–Cu–Li Alloy
    Muthumanickam Agilan
    Gandham Phanikumar
    Dhenuvakonda Sivakumar
    Transactions of the Indian Institute of Metals, 2018, 71 : 2667 - 2670
  • [4] Weld Solidification Cracking Behaviour of AA2195 Al-Cu-Li Alloy
    Agilan, Muthumanickam
    Phanikumar, Gandham
    Sivakumar, Dhenuvakonda
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2018, 71 (11) : 2667 - 2670
  • [5] Hot deformation behavior and microstructure of strain compression AA2195 alloy under plane
    Yang, Qingbo
    Wang, Xinzhu
    Li, Xu
    Deng, Zanhui
    Jia, Zhihong
    Zhang, Zhiqing
    Huang, Guangjie
    Liu, Qing
    MATERIALS CHARACTERIZATION, 2017, 131 : 500 - 507
  • [6] Effects of pre-deformation on precipitating behavior and grain refinement of AA2195 Al-Li alloy
    Zhang, Xin-Ming
    Liu, Ying-Wei
    Ye, Ling-Ying
    Tang, Jian-Guo
    Zhongnan Daxue Xuebao (Ziran Kexue Ban)/Journal of Central South University (Science and Technology), 2009, 40 (02): : 376 - 382
  • [7] MICROSTRUCTURE AND DEFORMATION-BEHAVIOR OF RAPIDLY SOLIDIFIED AL-LI-CU ALLOYS
    SANKARAN, KK
    PAO, PS
    ONEAL, JE
    JOURNAL OF METALS, 1980, 32 (12): : 67 - 67
  • [8] Influence of different rolling processes on microstructure and strength of the Al–Cu–Li alloy AA2195
    Fan Ye
    Ling Mao
    Jian Rong
    Baoshuai Zhang
    Lijun Wei
    Sihan Wen
    Haojun Jiao
    Sujun Wu
    Progress in Natural Science:Materials International, 2022, 32 (01) : 87 - 95
  • [9] Cracks propagation mechanism of intergranular corrosion in Al-Cu-Li AA2195 alloys governed by constant relative humidity
    Zhao, Jingxin
    Dan, Zhenhua
    Chang, Hui
    Zhou, Lian
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 32 : 165 - 176
  • [10] Influence of different rolling processes on microstructure and strength of the Al-Cu-Li alloy AA2195
    Ye, Fan
    Mao, Ling
    Rong, Jian
    Zhang, Baoshuai
    Wei, Lijun
    Wen, Sihan
    Jiao, Haojun
    Wu, Sujun
    PROGRESS IN NATURAL SCIENCE-MATERIALS INTERNATIONAL, 2022, 32 (01) : 87 - 95