Effect of high zirconium content on hydrogenation properties and anti-poisoning ability of air-exposed TiFe alloy

被引:22
|
作者
Lv, Peng [1 ,2 ]
Liu, Zhichen [2 ]
机构
[1] East China Univ Technol, Sch Biol Chem & Mat Sci, 418 Guanglan Rd, Nanchang 330013, Jiangxi, Peoples R China
[2] East China Univ Technol, Sch Innovat & Entrepreneurship Educ, 418 Guanglan Rd, Nanchang 330013, Jiangxi, Peoples R China
基金
中国国家自然科学基金;
关键词
TiFe alloy; First hydrogenation; Rate limiting step; Crystal structure; Morphology; Anti-poisoning ability; SOLID-STATE REACTIONS; HIGH-PRESSURE TORSION; STORAGE PROPERTIES; MECHANICAL ACTIVATION; FETI; PERFORMANCE; HYDROLYSIS; ABSORPTION; STABILITY; EVOLUTION;
D O I
10.1016/j.jrnrt.7019.09.077
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In order to improve the anti-poisoning ability of air-exposed TiFe alloy, the TiFe + x wt.% Zr (x=8, 12 and 16) alloys were synthesized by arc melting and subsequently exposed in air for different time. The results show that all samples handled in air can absorb the hydrogen directly without any incubation time. In addition, their first hydrogenation kinetics increases with the proportion of zirconium. And for the samples exposed in air for 35 h, all samples also can absorb the hydrogen without any heating and mechanical treatment, but x = 8 sample needs a long incubation time. Further study, it can be found that each alloy exposed in air for 35 h includes three phases: a TiFe main phase with very small amount of zirconium, a hcp secondary phase with high proportion of zirconium and very small titanium phase. Also, more hcp secondary phases are beneficial for the improvement of the first hydrogenation kinetics but also lead to higher loss of capacity after first absorption and desorption. Above results suggest that introducing high zirconium content can improve the anti-poisoning ability of TiFe alloy effectively. This may be because that the bright phase (hcp phase) probably cant be oxidized as easily as the dark phase (TiFe phase). (C) 2019 The Authors. Published by Elsevier B.V.
引用
收藏
页码:5972 / 5983
页数:12
相关论文
共 9 条
  • [1] Influence of Ball Milling, Cold Rolling and Doping (Zr + 2Cr) on Microstructure, First Hydrogenation Properties and Anti-poisoning Ability of TiFe Alloy
    Peng Lv
    Zhichen Liu
    Abhishek Kumar Patel
    Xingsheng Zhou
    Jacques Huot
    Metals and Materials International, 2021, 27 : 1346 - 1357
  • [2] Correction to: Influence of Ball Milling, Cold Rolling and Doping (Zr + 2Cr) on Microstructure, First Hydrogenation Properties and Anti-poisoning Ability of TiFe Alloy
    Peng Lv
    Zhichen Liu
    Abhishek Kumar Patel
    Xingsheng Zhou
    Jacques Huot
    Metals and Materials International, 2021, 27 : 1358 - 1358
  • [3] Effect of Fe substitution by Mn and Cr on first hydrogenation kinetics of air-exposed TiFe-based hydrogen storage alloy
    Park, Ki Beom
    Ko, Won-Seok
    Fadonougbo, Julien O.
    Na, Tae-Wook
    Im, Hyeon-Tae
    Park, Jae-Young
    Kang, Jang-Won
    Kang, Hyun-Su
    Park, Chang-Soo
    Park, Hyung-Ki
    MATERIALS CHARACTERIZATION, 2021, 178
  • [4] Influence of Ball Milling, Cold Rolling and Doping (Zr + 2Cr) on Microstructure, First Hydrogenation Properties and Anti-poisoning Ability of TiFe Alloy (vol 13, pg 127, 2020)
    Lv, Peng
    Liu, Zhichen
    Patel, Abhishek Kumar
    Zhou, Xingsheng
    Huot, Jacques
    METALS AND MATERIALS INTERNATIONAL, 2021, 27 (05) : 1358 - 1358
  • [5] Pd17Se15 alloy on Se spheres with a high anti-poisoning ability for alcohol fuel electrooxidation
    Qiao, Wei
    Zha, Meng
    Yang, Yun
    Hu, Guangzhi
    Feng, Ligang
    CHEMICAL COMMUNICATIONS, 2022, 58 (76) : 10651 - 10654
  • [6] Effect of rate on the deformation properties of metastable β in a high Sn content zirconium alloy
    Cochrane, C.
    Skippon, T.
    Daymond, M. R.
    INTERNATIONAL JOURNAL OF PLASTICITY, 2019, 119 : 102 - 122
  • [7] Correction to: Influence of Ball Milling, Cold Rolling and Doping (Zr + 2Cr) on Microstructure, First Hydrogenation Properties and Anti-poisoning Ability of TiFe Alloy (Metals and Materials International, (2021), 27, 5, (1346-1357), 10.1007/s12540-019-00501-1)
    Lv, Peng
    Liu, Zhichen
    Patel, Abhishek Kumar
    Zhou, Xingsheng
    Huot, Jacques
    Metals and Materials International, 2021, 27 (05):
  • [8] Superior anti-impurity gas poisoning ability and hydrogen storage properties of Ti-Cr alloy by introducing zirconium as additive
    Lv, Peng
    Zhong, Changlin
    Huang, Dongfang
    Zhou, Xingsheng
    Liu, Zhichen
    Zhao, Ruixue
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2022, 47 (43) : 18772 - 18785
  • [9] Effect of Si addition on crystallization behavior, thermal ability and magnetic properties in high Fe content Fe-Si-B-P-Cu-C alloy
    Xu, Jia
    Yang, Yuanzheng
    Li, Wen
    Xie, Zhiwei
    Chen, Xianchao
    MATERIALS RESEARCH BULLETIN, 2018, 97 : 452 - 456