Effect of different firing atmospheres on debonding strength of dental porcelain fused to commercially pure titanium

被引:0
|
作者
Wang, Jen-Chyan [1 ,2 ,5 ]
Fu, Po-Sung [1 ,3 ]
Lai, Pei-Ling [2 ]
Liu, Chen-Shih [1 ]
Chen, Wen-Cheng [4 ,5 ]
Hung, Chun-Cheng [1 ,2 ,5 ]
机构
[1] Kaohsiung Med Univ, Sch Dent, Coll Dent Med, 100,Shih Chuan 1st Rd, Kaohsiung 80756, Taiwan
[2] Kaohsiung Med Univ Hosp, Div Prosthodont, Dept Dent, Kaohsiung, Taiwan
[3] Kaohsiung Municipal Tatung Hosp, Dept Dent, Kaohsiung, Taiwan
[4] Feng Chia Univ, Adv Med Devices & Composites Lab, Dept Fiber & Composite Mat, Coll Engn, Taichung, Taiwan
[5] Kaohsiung Med Univ, Dent Med Devices & Mat Res Ctr, Coll Dent Med, Kaohsiung, Taiwan
来源
KAOHSIUNG JOURNAL OF MEDICAL SCIENCES | 2020年 / 36卷 / 03期
关键词
bending; bonding strength; commercially pure titanium (cp Ti); noble gases; porcelain fused to metal (PFM); LOW-FUSING PORCELAIN; ALPHA-CASE FORMATION; MECHANICAL-PROPERTIES; BOND STRENGTH; ALLOY; OXIDATION; COATINGS; POROSITY; CAST; SIO2;
D O I
10.1002/kjm2.12157
中图分类号
R-3 [医学研究方法]; R3 [基础医学];
学科分类号
1001 ;
摘要
An in vitro investigation was performed to evaluate the bonding characteristics of porcelain fused to metal (PFM)/commercially pure titanium (cp Ti, grade II) in three firing atmospheres of under vacuum and using two noble gases argon (Ar) and helium (He). Three groups of porcelain veneers firing under vacuum, Ar, and He were prepared to evaluate the bonding of porcelain fused to the cold-rolled cp Ti. The bond strength of PFM durability by a three-point bending test, phases, microhardness of cp Ti after firing processes, and fractures were measured and evaluated. Results show the microhardness of cp Ti in group of porcelain firing under He atmosphere was significantly lower than that of the two other groups, which were in vacuum and Ar (P < .05). X-ray diffraction showed the He group produced in relatively small amounts of TiO2 and TiO oxides than other groups but featured relatively high quantity of airhole defects in the porcelain body leading to the lowest bond strength. The Ar group presented the highest bond strength of comparing with the groups under vacuum and using He (P < .05). Although the firing processes in He could efficiently prevent the diffusion of oxygen into Ti, the porcelain-cp Ti bond strength using Ar protective atmosphere presented the advantage to achieve clinical requirement because porcelain firing under He revealed prominent voids and defects within the body of porcelain.
引用
收藏
页码:212 / 219
页数:8
相关论文
共 50 条
  • [1] BONDING OF LOW-FUSING DENTAL PORCELAIN TO COMMERCIALLY PURE TITANIUM
    KONONEN, M
    KIVILAHTI, J
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1994, 28 (09): : 1027 - 1035
  • [2] Effect of silica coating on the bond strength of milled pure titanium to dental porcelain
    Ye, Jiantao
    Ye, Xiuhua
    Chang, Shaohai
    Liu, Lang
    Zhang, Yiping
    Lin, Shiyao
    EUROPEAN JOURNAL OF ORAL SCIENCES, 2016, 124 (05) : 498 - 503
  • [3] BOND STRENGTH INVESTIGATION OF DENTAL PORCELAIN FUSED TO TITANIUM METAL
    GUTIERREZ, JM
    BLACKMAN, RB
    DERIJK, WG
    JOURNAL OF DENTAL RESEARCH, 1995, 74 : 237 - 237
  • [4] Effect of surface treatment on bond strength of low-fusing porcelain to commercially pure titanium
    Al Hussaini, I
    Al Wazzan, KA
    JOURNAL OF PROSTHETIC DENTISTRY, 2005, 94 (04): : 350 - 356
  • [5] Effects of nitrogen implantation on the bonding strength of porcelain fused to pure titanium
    Xie, Weili
    Zhong, Zhaowei
    Li, Changcheng
    Wen, Guangwu
    PROGRESSES IN FRACTURE AND STRENGTH OF MATERIALS AND STRUCTURES, 1-4, 2007, 353-358 : 2261 - +
  • [6] Strength of porcelain fused to titanium beam
    White, SN
    Ho, L
    Caputo, AA
    Goo, E
    JOURNAL OF PROSTHETIC DENTISTRY, 1996, 75 (06): : 640 - 648
  • [7] The effect of thermal cycling on the bond strength of low-fusing porcelain to commercially pure titanium and titanium-aluminium-vanadium alloy
    Troia, MG
    Henriques, GEP
    Nóbilo, MAA
    Mesquita, MF
    DENTAL MATERIALS, 2003, 19 (08) : 790 - 796
  • [8] EFFECT OF A MAGNETRON-SPUTTERED ZRSIN/ZRO2 FILM ON THE BOND STRENGTH OF COMMERCIALLY PURE TITANIUM TO PORCELAIN
    Wang, Guowei
    Wang, Xiaojing
    Zhao, Yimin
    Guo, Tianwen
    JOURNAL OF PROSTHETIC DENTISTRY, 2013, 109 (05): : 313 - 318
  • [9] Effects of different bond agents on commercially pure Ti-porcelain bond strength
    Zhang, Zhuoran
    Tan, Fei
    Ba, Yama
    Zhang, Yumei
    MATERIALS LETTERS, 2013, 109 : 214 - 216
  • [10] Stress-relieving and porcelain firing cycle influence on marginal fit of commercially pure titanium and titanium-aluminum-vanadium copings
    Fonseca, JC
    Henriques, GEP
    Sobrinho, LC
    de Góes, MF
    DENTAL MATERIALS, 2003, 19 (07) : 686 - 691