Flatness based inductive reheating of A356 billets into the semi-solid state

被引:2
|
作者
Schonbohm, A. [1 ]
Gasper, R. [1 ]
Abel, D. [1 ]
机构
[1] Univ Aachen, Inst Automat Control, D-52056 Aachen, Germany
关键词
flatness; open-loop control; induction heating; aluminum; semi-solid; A356;
D O I
10.4028/www.scientific.net/SSP.116-117.766
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
An important step in the processing of semi-solid metals is the inductive re-heating of the feedstock material. The heating should lead to an uniform billet temperature in order to obtain good forming results. The billet is supposed to be heated to the target temperature as fast as possible and at the same time it must be guaranteed, that the outer area of the billet does not melt prematurely. Conventionally the open-loop trajectories consist of simple power over time diagrams and are generated by extensive experiments. By using an open-loop control scheme it is possible to chose a desired trajectory for the middle axis temperature of the billet which respects the given constraint on the heating process. By taking advantage of the flatness property of the system, an open loop trajectory for the coil current can be calculated which ensures the desired behavior of the axis temperature. The shape of the trajectory is determined by the shape of the desired trajectory and the temperature dependent material properties, which have to be known with the needed accuracy. The losses of the converter and induction coil are estimated online so that the induced power is known. The trajectory ensures that the billet is heated to a temperature just below the solidus temperature without overheating of the billet's surface and with a very homogeneous temperature distribution. The Experiments have been conducted using A356 aluminum alloy.
引用
收藏
页码:766 / 770
页数:5
相关论文
共 50 条
  • [1] Reheating process for the semi-solid A356 alloy
    Tsinghua University, Beijing, China
    Tezhong Zhuzao Ji Youse Hejin, 2006, 12 (781-783):
  • [2] Microstructural evolution of semi-solid A356 alloy during reheating
    Hu, Yong
    Zhao, Longzhi
    Liu, Dejia
    Tang, Yanchuan
    Jiang, Hui
    INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2018, 109 (10) : 951 - 956
  • [3] A study of the optimum reheating process for A356 alloy in semi-solid forging
    Park J.H.
    Choi J.C.
    Kim Y.H.
    Yoon J.M.
    The International Journal of Advanced Manufacturing Technology, 2002, 20 (4) : 277 - 283
  • [4] A study of the optimum reheating process for A356 alloy in semi-solid forging
    Kim, YH
    Choi, JC
    Yoon, JA
    Park, JH
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2002, 20 (04): : 277 - 283
  • [5] Recrystallization behavior of ECAPed A356 alloy at semi-solid reheating temperature
    Moradi, M.
    Nili-Ahmadabadi, M.
    Poorganji, B.
    Heidarian, B.
    Parsa, M. H.
    Furuhara, T.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (16-17): : 4113 - 4121
  • [6] Study on Thixotropic Property of A356 Alloy in Semi-Solid State
    Simlandi, Sudip
    Barman, Nilkanta
    Chattopadhyay, Himadri
    SEMI-SOLID PROCESSING OF ALLOYS AND COMPOSITES XII, 2013, 192-193 : 335 - 340
  • [7] Semi-solid microstructure evolution during reheating of aluminum A356 alloy deformed severely by ECAP
    Ashouri, S.
    Nili-Ahmadabadi, M.
    Moradi, M.
    Iranpour, M.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2008, 466 (1-2) : 67 - 72
  • [8] Semi-solid microstructure evolution during reheating of aluminum A356 alloy deformed severely by ECAP
    Ashouri, S.
    Nili-Ahmadabadi, M.
    Moradi, M.
    Iranpour, M.
    Journal of Alloys and Compounds, 2008, 466 (1-2): : 67 - 72
  • [9] Behavior of A356 Alloy in semi-solid state produced by mechanical stirring
    Nourouzi, Salman
    Kolahdooz, Amin
    Botkan, Mohammad
    ADVANCES IN METALLURGICAL AND MINING ENGINEERING, 2012, 402 : 331 - 336
  • [10] Rheological behavior of semi-solid A356 aluminum alloy at steady state
    Zhang, YJ
    Mao, WM
    Zhao, ZD
    Liu, Z
    ACTA METALLURGICA SINICA, 2006, 42 (02) : 163 - 166